Flexural Behavior of Reinforced Concrete Beams Strengthened with Near-Surface-Mounted Prestressing ScrewThreaded Steel Bars Using Digital Image Correlation Method

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexural Behavior of Reinforced Concrete Beams Strengthened with Near-Surface-Mounted Prestressing ScrewThreaded Steel Bars Using Digital Image Correlation Method

Author(s): Jiao Huang, Guohua Xing, Zhaoqun Chang, and Boquan Liu

Publication: Structural Journal

Volume: 118

Issue: 5

Appears on pages(s): 263-274

Keywords: crack analysis; digital image correlation (DIC) technique; flexural behavior; near-surface mounted (NSM); prestressed beam; prestressing screw-threaded steel bar (PSB)

DOI: 10.14359/51732834

Date: 9/1/2021

Abstract:
In this paper, the flexural behavior of four reinforced concrete (RC) beam specimens strengthened with near-surface-mounted (NSM) prestressing screw-threaded steel bars (PSBs) were investigated with four-point bending experiments, where the failure mode, load-deflection relationships, ductility, and cracking behavior were examined as key properties. The digital image correlation (DIC) technique was used to perform full-field measurement and provide information on the deformation and failure process of concrete members. The test results indicated that the beams strengthened with NSM PSBs exhibited improved load-bearing capacity and enhanced ductility performance. It was also observed that prestressing the strengthening bar and increasing the NSM reinforcement ratio can significantly enhance the strengthening effect on the beams while controlling the development and propagation of cracks; however, the deformability of the specimen would reduce accordingly. In addition, the emerging optical technique proved to be effective in measuring the full-field deformation and monitoring the cracking evolution of concrete structures.

Related References:

1. Macdonald, M. D., and Calder, A. J. J., “Bonded Steel Plating for Strengthening Concrete Structures,” International Journal of Adhesion and Adhesives, V. 2, No. 2, 1982, pp. 119-127. doi: 10.1016/0143-7496(82)90125-7

2. Jones, R.; Swamy, R. N.; and Charif, A., “Plate Separation and Anchorage of Reinforced Concrete Beams Strengthened by Epoxy-Bonded Steel Plates,” Structural Engineering, V. 66, No. 5, 1988, pp. 85-94.

3. Sharpe, R., and Ugrte, E., “Seismic Strengthening of PALO ALTO Civic Centre,” Proceedings, Ninth World Conference on Earthquake Engineering, Tokyo, Japan, 1988, pp. 445-450.

4. Adhikary, B. B.; Mutsuyoshi, H.; and Sano, M., “Shear Strengthening of Reinforced Concrete Beams Using Steel Plates Bonded on Beam Web: Experiments and Analysis,” Construction and Building Materials, V. 14, No. 5, 2000, pp. 237-244. doi: 10.1016/S0950-0618(00)00023-4

5. Barnes, R. A.; Baglin, P. S.; Mays, G. C.; and Subedi, N. K., “External Steel Plate Systems for the Shear Strengthening of Reinforced Concrete Beams,” Engineering Structures, V. 23, No. 9, 2001, pp. 1162-1176. doi: 10.1016/S0141-0296(00)00124-3

6. Büyükkaragöz, A., and Arslan, A., “The Effect of Steel Plates with Shear Studs for Weak Column-Strong Beam Connections in the Reinforced Concrete Structures under Earthquake Effect,” Strain, V. 47, No. 2, 2011, p. 19.

7. Cumhur, A.; Altundal, A.; Aykac, S.; and Aykac, B., “Strengthening of Hollow Brick Infill Walls with Expanded Steel Plates,” Earthquakes and Structures, V. 11, No. 5, 2016, pp. 887-904. doi: 10.12989/eas.2016.11.5.887

8. Altin, S.; Anil, Ö.; and Kara, M. E., “Improving Shear Capacity of Existing RC Beams Using External Bonding of Steel Plates,” Engineering Structures, V. 27, No. 5, 2005, pp. 781-791. doi: 10.1016/j.engstruct.2004.12.012

9. Su, R. K. L.; Lam, W. Y.; and Pam, H. J., “Behaviour of Embedded Steel Plate in Composite Coupling Beams,” Journal of Constructional Steel Research, V. 64, No. 10, 2008, pp. 1112-1128. doi: 10.1016/j.jcsr.2007.09.013

10. Ashrafuddin, M.; Baluch, M. H.; Sharif, A.; Al-Sulaimani, G. J.; Azad, A. K.; and Khan, A. R., “Peeling and Diagonal Tension Failures in Steel Plated R/C Beams,” Construction and Building Materials, V. 13, No. 8, 1999, pp. 459-467. doi: 10.1016/S0950-0618(99)00044-6

11. Cairns, J., and Rafeeqi, F. A., “Strengthening Reinforced Concrete Beams with External Unbonded Bars: Experimental Investigation,” Proceedings of the Institution of Civil Engineers. Structures and Buildings, V. 156, No. 1, 2003, pp. 27-37. doi: 10.1680/stbu.2003.156.1.27

12. Zhao, W.; Yu, Y.; and Xie, Q., “Nonuniform Interface Failure of Steel-Concrete Composite Structures Bonded Using Epoxy Resin Mortar,” Engineering Structures, V. 184, Apr. 2019, pp. 447-458. doi: 10.1016/j.engstruct.2019.01.109

13. Kothandaraman, S., and Vasudevan, G., “Flexural Retrofitting of RC Beams Using External Bars at Soffit Level—An Experimental Study,” Construction and Building Materials, V. 24, No. 11, 2010, pp. 2208-2216. doi: 10.1016/j.conbuildmat.2010.04.036

14. Badawi, M., and Soudki, K., “Flexural Strengthening of RC Beams with Prestressed NSM CFRP Rods: Experimental and Analytical Investigation,” Construction and Building Materials, V. 23, No. 10, 2009, pp. 3292-3300. doi: 10.1016/j.conbuildmat.2009.03.005

15. El-Hacha, R., and Gaafar, M., “Flexural Strengthening of Reinforced Concrete Beams Using Prestressed, Near-Surface-Mounted CFRP Bars,” PCI Journal, V. 56, No. 4, 2011, pp. 134-151. doi: 10.15554/pcij.09012011.134.151

16. Hosen, M. A.; Jumaat, M. Z.; Islam, A. B. M. S.; Salam, M. A.; and Mo, K. H., “Side-NSM Composite Technique for Flexural Strengthening of RC Beams,” Computers and Concrete, V. 20, No. 4, 2017, pp. 439-448.

17. El-Hacha, R., and Rizkalla, S., “Near-Surface-Mounted Fiber-Reinforced Polymer Reinforcements for Flexural Strengthening of Concrete Structures,” ACI Structural Journal, V. 101, No. 5, Sept.-Oct. 2004, pp. 717-726.

18. Xing, G. H.; Chang, Z. Q.; and Bai, Z. Q., “Flexural Behaviour of RC Beams Strengthened with Near-Surface-Mounted BFRP Bars,” Magazine of Concrete Research, V. 70, No. 11, 2018, pp. 570-582. doi: 10.1680/jmacr.17.00227

19. Xing, G. H.; Chang, Z. Q.; and Ozbulut, O. E., “Behavior and Failure Modes of Reinforced Concrete Beams Strengthened with NSM GFRP or Aluminum Alloy Bars,” Structural Concrete, V. 19, No. 4, 2018, pp. 1023-1035. doi: 10.1002/suco.201700099

20. Sabau, C.; Popescu, C.; Sas, G.; Schmidt, J. W.; Blanksvärd, T.; and Täljsten, B., “Strengthening of RC Beams Using Bottom and Side NSM Reinforcement,” Composites. Part B, Engineering, V. 149, Sept, 2018, pp. 82-91. doi: 10.1016/j.compositesb.2018.05.011

21. Zhong, X.; Zhang, T.; Zhao, C.; Shu, X.; Shen, M.; and Chen, Y. F., “New Non-Destructive Dynamic Tensile Testing of Prestressing Fine-Rolled Screw-Threaded Steel Bars,” Engineering Structures, V. 182, Mar. 2019, pp. 153-163. doi: 10.1016/j.engstruct.2018.12.065

22. ISO 6934-5, “Steel for the Prestressing of Concrete—Part 5: Hot-Rolled Steel Bars with or without Subsequent Processing,” International Organization for Standardization, Geneva, Switzerland, 1991.

23. GB/T 20065-2016, “Screw-Thread Steel Bars for the Prestressing of Concrete,” Standardization Administration of China, Beijing, China, 2016.

24. Khoo, S. W.; Karuppanan, S.; and Tan, C. S., “A Review of Surface Deformation and Strain Measurement Using Two-Dimensional Digital Image Correlation,” Metrology and Measurement Systems, V. 23, No. 3, 2016, pp. 461-480. doi: 10.1515/mms-2016-0028

25. Zhou, H.; Attard, T. L.; Wang, Y.; Wang, J. A.; and Ren, F., “Rehabilitation of Notch Damaged Steel Beams Using a Carbon Fiber Reinforced Hybrid Polymeric-Matrix Composite,” Composite Structures, V. 106, Dec. 2013, pp. 690-702. doi: 10.1016/j.compstruct.2013.07.001

26. Destrebecq, J. F.; Toussaint, E.; and Ferrier, E., “Analysis of Cracks and Deformations in a Full Scale Reinforced Concrete Beam Using a Digital Image Correlation Technique,” Experimental Mechanics, V. 51, No. 6, 2011, pp. 879-890. doi: 10.1007/s11340-010-9384-9

27. Nonis, C.; Niezrecki, C.; Yu, T.-Y.; Ahmed, S.; Su, C. F.; and Schmidt, T., “Structural Health Monitoring of Bridges Using Digital Image Correlation,” Health Monitoring of Structural and Biological Systems, Proceedings of SPIE, V. 8695, T. Kundu, ed., SPIE, 2013.

28. Hui, C.; Zhu, Y. Z.; Cao, W. L.; and Wang, Y. Q., “Seismic Experiment and Analysis of Rectangular Bottom Strengthened Steel-Concrete Composite Columns,” Steel and Composite Structures, V. 20, No. 3, 2016, pp. 599-621. doi: 10.12989/scs.2016.20.3.599

29. Dai, Y. T.; Wang, H. T.; Ge, T. Y.; Wu, G.; Wan, J. X.; Cao, A. Y.; Yang, F. J.; and He, X.-Y., “Stereo-Digital Image Correlation in the Behavior Investigation of CFRP-Steel Composite Members,” Steel and Composite Structures, V. 23, No. 6, 2017, pp. 727-736.

30. Pagani, A.; Zappino, E.; de-Miguel, A. G.; Martilla, V.; and Carrera, E., “Full Field Strain Measurements of Composite Wing by Digital Image Correlation,” Advances in Aircraft and Spacecraft Science, V. 61, No. 1, 2019, pp. 69-86.

31. ACI Committee 440, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-08),” American Concrete Institute, Farmington Hills, MI, 2015.

32. ISO 6892-1, “Metallic Materials—Tensile Testing—Part 1: Method of Test at Room Temperature,” International Organization for Standardization, Geneva, Switzerland, 2016.

33. Blaber, J.; Adair, B.; and Antoniou, A., “Ncorr: Open-Source 2D Digital Image Correlation MATLAB Software,” Experimental Mechanics, V. 55, No. 6, 2015, pp. 1105-1122. doi: 10.1007/s11340-015-0009-1

34. Ab Ghani, A. F.; Ali, M. B.; Dhar Malingam, S.; and Mahmud, J., “Digital Image Correlation (DIC) Technique in Measuring Strain Using Opensource Platform Ncorr,” Journal of Advanced Research in Applied Mechanics, V. 26, 2016, pp. 10-21.

35. Liu, B. Q.; Huang, J.; and Xing, G. H., “Crack Behavior of Concrete Beam in Flexure Strengthened with NSM Prestressing Screw-Thread Steel Bars,” Materials and Structures, V. 53, No. 4, 2020, p. 80. doi: 10.1617/s11527-020-01521-9

36. Rezazadeh, M.; Costa, I.; and Barros, J., “Influence of Prestress Level on NSM CFRP Laminates for the Flexural Strengthening of RC Beams,” Composite Structures, V. 116, Sept.-Oct. 2014, pp. 489-500.

37. Mahal, M.; Blanksvärd, T.; Täljsten, B.; and Sas, G., “Using Digital Image Correlation to Evaluate Fatigue Behavior of Strengthened Reinforced Concrete Beams,” Engineering Structures, V. 105, Dec. 2015, pp. 277-288. doi: 10.1016/j.engstruct.2015.10.017

38. Daghash, S. M., and Ozbulut, O. E., “Flexural Performance Evaluation of NSM Basalt FRP-Strengthened Concrete Beams Using Digital Image Correlation System,” Composite Structures, V. 176, Sept. 2017, pp. 748-756. doi: 10.1016/j.compstruct.2017.06.021


ALSO AVAILABLE IN: