Assessing Rheology of Self-Consolidating Paste Systems— A New Approach

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Assessing Rheology of Self-Consolidating Paste Systems— A New Approach

Author(s): Usman Mahmood Raja, Thomas A. Bier, and Syed Ali Rizwan

Publication: Materials Journal

Volume: 118

Issue: 4

Appears on pages(s): 79-90

Keywords: Bingham and Herschel–Bulkley equations; repeatability; rheology; viscosity; yield stress

DOI: 10.14359/51732793

Date: 7/1/2021

Abstract:
The rheology of a self-consolidating cementitious system (SCCS) is often characterized by its yield stress and viscosity. These parameters are traditionally determined through a rheometer. However, there is some variability in results obtained, which raises the question of reproducibility. The current paper proposes a simpler mechanistic approach for their determination. An optical setup, attached with a flow apparatus, is designed to map the behavior of a flowing cement paste in real time using digital image processing (DIP) techniques. To evaluate rheological parameters, a superposition principle was used with two possible cases based on whether or not the paste’s shear stresses exceed its yield strength. With the parameters obtained, Bingham’s linear and Herschel–Bulkley’s equations were modeled. The computed results showed a plausible agreement with rheometric measurements and provided a quantitative tool for assessing the rheology and stability of cementitious systems. The repeatability of results is also significantly improved.

Related References:

1. Naik, T. R.; Kumar, R.; Ramme, B. W.; and Canpolat, F., “Development of High-Strength, Economical Self-Consolidating Concrete,” Construction and Building Materials, V. 30, 2012, pp. 463-469. doi: 10.1016/j.conbuildmat.2011.12.025

2. Kovler, K., and Roussel, N., “Properties of Fresh and Hardened Concrete,” Cement and Concrete Research, V. 41, No. 7, 2011, pp. 775-792. doi: 10.1016/j.cemconres.2011.03.009

3. Hanehara, S., and Yamada, K., “Rheology and Early Age Properties of Cement Systems,” Cement and Concrete Research, V. 38, No. 2, 2008, pp. 175-195. doi: 10.1016/j.cemconres.2007.09.006

4. Von Schowalter, W. R., Mechanics of Non‐Newtonian Fluids, Pergamon Press, Oxford, UK, 1978.

5. Schwartzentruber, L. A.; Le Roy, R.; and Cordin, J., “Rheological Behaviour of Fresh Cement Pastes Formulated from a Self Compacting Concrete (SCC),” Cement and Concrete Research, V. 36, No. 7, 2006, pp. 1203-1213. doi: 10.1016/j.cemconres.2004.10.036

6. Bird, R. B.; Dai, G.; and Yarusso, B. J., “The Rheology and Flow of Viscoplastic Materials,” Reviews in Chemical Engineering, V. 1, No. 1, 1983, pp. 1-70. doi: 10.1515/revce-1983-0102

7. Cross, M. M., “Rheology of Non-Newtonian Fluids: A New Flow Equation for Pseudoplastic Systems,” Journal of Colloid Science, V. 20, No. 5, 1965, pp. 417-437. doi: 10.1016/0095-8522(65)90022-X

8. Atzeni, C.; Massidda, L.; and Sanna, U., “Comparison between Rheological Models for Portland Cement Pastes,” Cement and Concrete Research, V. 15, No. 3, 1985, pp. 511-519. doi: 10.1016/0008-8846(85)90125-5

9. Khayat, K. H.; Assaad, J.; and Daczko, J., “Comparison of Field-Oriented Test Methods to Assess Dynamic Stability of Self-Consolidating Concrete,” ACI Materials Journal, V. 101, No. 2, Mar.-Apr. 2004, pp. 168-176.

10. Thrane, L.; Pade, C.; and Svensson, T., Estimation of Bingham Rheological Parameters of SCC from Slump Flow Measurement, RILEM Publications SARL, Paris, France, 2007, pp. 353-358.

11. Remond, S., and Pizette, P., “A DEM Hard-Core Soft-Shell Model for the Simulation of Concrete Flow,” Cement and Concrete Research, V. 58, 2014, pp. 169-178. doi: 10.1016/j.cemconres.2014.01.022

12. Saak, A. W.; Jennings, H. M.; and Shah, S. P., “A Generalized Approach for the Determination of Yield Stress by Slump and Slump Flow,” Cement and Concrete Research, V. 34, No. 3, 2004, pp. 363-371. doi: 10.1016/j.cemconres.2003.08.005

13. Roussel, N., “Correlation between Yield Stress and Slump: Comparison between Numerical Simulations and Concrete Rheometers Results,” Materials and Structures, V. 39, No. 4, 2007, pp. 501-509. doi: 10.1617/s11527-005-9035-2

14. Benaicha, M.; Jalbaud, O.; Alaoui, A. H.; and Burtschell, Y., “Correlation between Viscosity and V-Funnel Flow Time,” International Journal of Advanced Technology & Engineering Research, V. 3, No. 1, 2013, pp. 103-108.

15. Rizwan, S. A., “High-Performance Mortars and Concrete Using Secondary Raw Materials,” PhD thesis, TU Freiberg, Germany, 161 pp.

16. Ferraris, C. F., and DeLarrard, F., “Testing and Modeling of Fresh Concrete Rheology,” NIST Interagency/Internal Report (NISTIR) 6094, National Institute of Standards and Technology, Gaithersburg, MD, 1998.

17. Bouvet, A.; Ghorbel, E.; and Bennacer, R., “The Mini-Conical Slump Flow Test: Analysis and Numerical Study,” Cement and Concrete Research, V. 40, No. 10, 2010, pp. 1517-1523. doi: 10.1016/j.cemconres.2010.06.005

18. Roussel, N.; Stefani, C.; and Leroy, R., “From Mini-Cone Test to Abrams Cone Test: Measurement of Cement-Based Materials Yield Stress Using Slump Tests,” Cement and Concrete Research, V. 35, No. 5, 2005, pp. 817-822. doi: 10.1016/j.cemconres.2004.07.032

19. Nielsen, I., and Wallevik, O., “Rheological Evaluation of Some Empirical Test Methods–Preliminary Results,” International RILEM Symposium on Self-Compacting Concrete, RILEM Publications SARL, Paris, France, 2003, pp. 55-68.

20. de Larrard, F., and Sedran, T., “Optimization of Ultra-High-Performance Concrete by the Use of a Packing Model,” Cement and Concrete Research, V. 24, No. 6, 1994, pp. 997-1009. doi: 10.1016/0008-8846(94)90022-1

21. Chang, P.-K., “An Approach to Optimizing Mix Design for Properties of High-Performance Concrete,” Cement and Concrete Research, V. 34, No. 4, 2004, pp. 623-629. doi: 10.1016/j.cemconres.2003.10.010

22. Wallevik, O. H., and Wallevik, J. E., “Rheology as a Tool in Concrete Science: The Use of Rheographs and Workability Boxes,” Cement and Concrete Research, V. 41, No. 12, 2011, pp. 1279-1288. doi: 10.1016/j.cemconres.2011.01.009

23. Yeh, I.-C., “Design of High-Performance Concrete Mixture Using Neural Networks and Nonlinear Programming,” Journal of Computing in Civil Engineering, ASCE, V. 13, No. 1, 1999, pp. 36-42. doi: 10.1061/(ASCE)0887-3801(1999)13:1(36)

24. Thrane, L. N.; Pade, C.; and Nielsen, C. V., “Determination of Rheology of Self-Consolidating Concrete Using the 4C-Rheometer and How to Make Use of the Results,” Journal of ASTM International, V. 7, No. 1, 2009, pp. 1-10.

25. Hočevar, A.; Kavčič, F.; and Bokan-Bosiljkov, V., “Rheological Parameters of Fresh Concrete–Comparison of Rheometers,” Gradevinar, V. 65, No. 2, 2013, pp. 99-109. doi: 10.14256/JCE.851.2012

26. Carette, G., and Malhotra, V., “In Situ Tests: Variability and Strength Prediction of Concrete at Early Ages,” In Situ/Nondestructive Testing of Concrete, SP-82, American Concrete Institute, Farmington Hills, MI, 1984, pp. 111-142.

27. Roussel, N.; Geiker, M. R.; Dufour, F.; Thrane, L. N.; and Szabo, P., “Computational Modeling of Concrete Flow: General Overview,” Cement and Concrete Research, V. 37, No. 9, 2007, pp. 1298-1307. doi: 10.1016/j.cemconres.2007.06.007

28. Banfill, P. F. G., Rheology of Fresh Cement and Concrete: Proceedings of an International Conference, Liverpool, 1990, CRC Press, Boca Raton, FL, 2014.

29. Haralick, R. M.; Sternberg, S. R.; and Zhuang, X., “Image Analysis Using Mathematical Morphology,” IEEE Transactions on Pattern Analysis and Machine Intelligence, V. PAMI-9, No. 4, 1987, pp. 532-550. doi: 10.1109/TPAMI.1987.4767941

30. Mathworks, “Measure Properties of Image Regions - MATLAB regionprops,” 2021, https://www.mathworks.com/help/images/ref/regionprops.html. (last accessed June 28, 2021)

31. Schneider, A., and Bruckner, H., “Impact of Some Parameters on Rheological Properties of Cement Paste in Combination with PCE-Based Plasticizers,” 2013.

32. Hill, R., The Mathematical Theory of Plasticity, Oxford University Press, Oxford, UK, 1998.

33. Lucas, B. D., and Kanade, T., “An Iterative Image Registration Technique with an Application to Stereo Vision,” IJCAI’81: Proceedings of the 7th International Joint Conference on Artificial Intelligence, 1981, pp. 674-679.

34. Gooch, J. W., “Momentum Flux,” Encyclopedic Dictionary of Polymers, Springer, 2011, p. 472.

35. Mewis, J., and Wagner, N. J., Colloidal Suspension Rheology, Cambridge University Press, Cambridge, UK, 2012.

36. Fox, R. W.; McDonald, A. T.; and Pritchard, P. J., Introduction to Fluid Mechanics, sixth edition, John Wiley & Sons, Inc., Hoboken, NJ, 2003.

37. Mansour, S. M.; Abadlia, M. T.; Bekkour, K.; and Messaoudene, I., “Improvement of Rheological Behaviour of Cement Pastes by Incorporating Metakaolin,” European Journal of Scientific Research, V. 42, 2010, pp. 442-452.

38. Shaughnessy, R. III, and Clark, P. E., “The Rheological Behavior of Fresh Cement Pastes,” Cement and Concrete Research, V. 18, No. 3, 1988, pp. 327-341. doi: 10.1016/0008-8846(88)90067-1

39. Kasińska, M.; Kempiński, J.; and Świerzko, R., “The Consistency of Cement Pastes and their Rheological Parameters,” Acta Scientiarum Polonorum. Formatio Circumiectus, V. 15, No. 3, 2016, pp. 71-81. doi: 10.15576/ASP.FC/2016.15.3.71

40. Van Der Vurst, F.; Grünewald, S.; and De Schutter, G., “The Impact of VMA on the Rheology, Thixotropy and Robustness of Self-Compacting Mortars,” Calcined Clays for Sustainable Concrete, Springer, 2015, pp. 159-167.

41. Cyr, M.; Legrand, C.; and Mouret, M., “Study of the Shear Thickening Effect of Superplasticizers on the Rheological Behaviour of Cement Pastes Containing or Not Mineral Additives,” Cement and Concrete Research, V. 30, No. 9, 2000, pp. 1477-1483. doi: 10.1016/S0008-8846(00)00330-6


ALSO AVAILABLE IN:

Electronic Materials Journal