Abstract:
Since both the yield stress and bleeding originate from the network of interacting cement particles, their correlation seems to be possible. The purpose of this paper is to investigate the existence of this correlation by varying solid volume fraction of cement paste. The static yield stress measurements were carried out using a traditional rheological test, and bleeding was determined by turbidimetry measurements. It appears that the correlation between yield stress and bleeding depends strongly on the solid volume fraction.
Related References:
1. Gaimster R, Dixon N. Self-compacting concrete. In: Advanced Concrete Technology. ; 2003. doi: 10.1016/B978-075065686-3/50295-0
2. Powers TC, Dahl LA. The Bleeding of Portland Cement Paste, Mortar and Concrete, Treated as a Special Case of Sedimentation,. Chicago: Portland Cement Association Bulletin. No.2; 1939.
3. Josserand L, Coussy O, de Larrard F. Bleeding of concrete as an ageing consolidation process. Cem Concr Res. 2006. doi: 10.1016/j.cemconres.2004.10.006
4. Perrot A, Lecompte T, Khelifi H, Brumaud C, Hot J, Roussel N. Yield stress and bleeding of fresh cement pastes. Cem Concr Res. 2012;42(7):937-944. doi: 10.1016/j.cemconres.2012.03.015
5. Kovler K, Roussel N. Properties of fresh and hardened concrete. Cem Concr Res. 2011. doi: 10.1016/j.cemconres.2011.03.009
6. Peng Y, Lauten RA, Reknes K, Jacobsen S. Bleeding and sedimentation of cement paste measured by hydrostatic pressure and Turbiscan. Cem Concr Compos. 2017;76:25-38. doi: 10.1016/j.cemconcomp.2016.11.013
7. Toorman EA. Sedimentation and self-weight consolidation: general unifying theory. Géotechnique. 2009. doi: 10.1680/geot.1996.46.1.103
8. DAVIES L, DOLLIMORE D, SHARP JH. SEDIMENTATION OF SUSPENSIONS : IMPLICATIONS OF THEORIES OF HINDERED SETTLING. Powder Technol. 1976. doi: 10.1016/0032-5910(75)87015-X
9. Barnes H a. The yield stress — a review or ‘ panta roi ’— everything flows ? J Non-Newtonian Fluid Mech. 1999;81(May 1998):133-178. doi: 10.1016/S0377-0257(98)00094-9
10. Barnes HA, Walters K. The yield stress myth? Rheol Acta. 1985. doi: 10.1007/BF01333960
11. Roussel N, Lemaître A, Flatt RJ, Coussot P. Steady state flow of cement suspensions: A micromechanical state of the art. Cem Concr Res. 2010;40(1):77-84. doi: 10.1016/j.cemconres.2009.08.026
12. Liddell P V, Boger D V. Yield stress measurements with the vane. Time. 1996;0257(95):235-261.
13. Kapur PC, Scales PJ, Boger D V., Healy TW. Yield Stress of Suspensions Loaded with Size Distributed Particles. AIChE J. 1997. doi: 10.1002/aic.690430506
14. Ben aicha M, Burtschell Y, Alaoui AH, El Harrouni K, Jalbaud O. Correlation between Bleeding and Rheological Characteristics of Self-Compacting Concrete. J Mater Civ Eng. 2017. doi: 10.1061/(ASCE)MT.1943-5533.0001871
15. Aït-Kadi A, Marchal P, Choplin L, Chrissemant AS, Bousmina M. Quantitative analysis of mixer-type rheometers using the couette analogy. Can J Chem Eng. 2002. doi: 10.1002/cjce.5450800618
16. Autier C, Azéma N, Boustingorry P. Using settling behaviour to study mesostructural organization of cement pastes and superplasticizer efficiency. Colloids Surfaces A Physicochem Eng Asp. 2014;450(1):36-45. doi: 10.1016/j.colsurfa.2014.02.050
17. Tramaux A, Azéma N, El Bitouri Y, et al. Synthesis of phosphonated comb-like copolymers and evaluation of their dispersion efficiency on CaCO3suspensions part II: Effect of macromolecular structure and ionic strength. Powder Technol. 2018;334. doi: 10.1016/j.powtec.2018.04.020
18. Flatt RJ, Bowen P. Yodel: A yield stress model for suspensions. J Am Ceram Soc. 2006;89(4):1244-1256. doi: 10.1111/j.1551-2916.2005.00888.x
19. Zhou Z, Solomon MJ, Scales PJ, Boger D V. The yield stress of concentrated flocculated suspensions of size distributed particles. J Rheol (N Y N Y). 2002. doi: 10.1122/1.551029
20. Mehdipour I, Khayat KH. Understanding the role of particle packing characteristics in rheo-physical properties of cementitious suspensions: A literature review. Constr Build
Mater. 2018. doi: 10.1016/j.conbuildmat.2017.11.147
21. Eckert WF, Masliyah JH, Gray MR, Fedorak PM. Prediction of Sedimentation and Consolidation of Fine Tails. AIChE J. 1996. doi: 10.1002/aic.690420409
22. Mahaut F, Mokéddem S, Chateau X, Roussel N, Ovarlez G. Effect of coarse particle volume fraction on the yield stress and thixotropy of cementitious materials. Cem Concr Res. 2008;38(11):1276-1285. doi: 10.1016/j.cemconres.2008.06.001
23. Tan TS, Wee TH, Tan SA, Tam CT, Lee SL. A consolidation model for bleeding of cement paste. Adv Cem Res. 1987. doi: 10.1680/adcr.1987.1.1.18
24. Perrot A, Rangeard D, Picandet V, Mélinge Y. Hydro-mechanical properties of fresh cement pastes containing polycarboxylate superplasticizer. Cem Concr Res. 2013. doi: 10.1016/j.cemconres.2013.06.015