Synergetic Effect of Combined Converter Steel Slag and Metakaolin Hydration

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Synergetic Effect of Combined Converter Steel Slag and Metakaolin Hydration

Author(s): Winnie Franco Santos, Katrin Schollbach, Sieger van der Laan, and H.J.H.Brouwers

Publication: Symposium Paper

Volume: 349

Issue:

Appears on pages(s): 466-478

Keywords: converter steel slag; metakaolin, mineralogy, reactivity

DOI: 10.14359/51732765

Date: 4/22/2021

Abstract:
Converter steel slag exhibits very low hydration activity compared to ordinary portland cement. To increase its reactivity, a mixture with metakaolin (Al2O3·2SiO2) was designed to increase the binding capacity. Metakaolin was used for its purity and high pozzolanic reactivity, owing to its high alumina and silica content. Two systems were prepared, metakaolin and portlandite as a reference, and the second system was composed of converter slag and metakaolin. Reactivity was assessed by measuring the heat release of the hydration reactions by isothermal calorimetry. Calorimetry results show the cumulative heat of converter slag increases when metakaolin is added. Furthermore, new hydration products were identified. Large area phase mapping based on SEM/EDX spectral imaging was done to investigate the reactions between the components.