Effect of a Lignosulfonate Plasticizer on the Hydration of a Belite-Ye’elimite-Ferrite Cement Paste

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of a Lignosulfonate Plasticizer on the Hydration of a Belite-Ye’elimite-Ferrite Cement Paste

Author(s): Angélique Barneoud-Chapelier, Youssef El Bitouri, Nathalie Azéma, Gwenn Le Saout

Publication: Symposium Paper

Volume: 349

Issue:

Appears on pages(s): 40-51

Keywords: Adsorption, belite ye’elimite ferrite (BYF) cement, lignosulfonate, yield stress

DOI: 10.14359/51732737

Date: 4/22/2021

Abstract:
Belite-Ye’elimite-Ferrite (BYF) cements have been recently developed in order to substitute ordinary Portland cement (OPC), as they release up to 30 % less CO2 and their performances tend to be similar. This work aims to give a first insight and understanding on the influence of a lignosulfonate plasticizer (LS) on the hydration and the properties of a BYF cement paste. For this purpose, hydration of neat cement paste (w/c=0.4) was followed by isothermal calorimetry associated with in situ XRD for the first 4 hours. In addition, plasticizer adsorption was investigated using TOC measurements. Rheological and compressive strength tests were also performed. The results showed that LS changes the hydration kinetics, modifying both induction period (that becomes shorter for low dosage and longer for higher dosage) and rate of ettringite precipitation. For all dosages used, LS decreases the heat of hydration and the compressive strength in the first day. Also, its impact on particle surfaces improves their dispersion and causes a diminution of the shear stress of cement paste, allowing better workability.

Related References:

1. Olivier, J. G. J. (PBL)., Janssens-Maenhout, G. (EC-J., Muntean, M. (EC-J., et al. “Trends in Global CO2 Emissions: 2016 Report,” PBL Netherlands Environmental Assessment Agency

& European Commission’s Joint Research Centre (JRC), 2016, p. 86.

2. Gartner, E., and Sui, T. “Alternative cement clinkers,” Cement and Concrete Research, 2017.

3. Sharp, J. H., Lawrencef, C. D., and Yang, R. “Calcium sulfoaluminate cements — lowenergy cements , special cements or what?,” Advances in Cement Research, V. 11, No. 1,

1999, pp. 3–13.

4. Quillin, K., Dunster, A., Tipple, C., et al. “Project AETHER Testing the durability of a lower-CO2 alternative to Portland cement.” 34th Annual Cement & Concrete Science

Conference. 2014.

5. Cuesta, A., Álvarez-Pinazo, G., Sanfélix, S. G., et al. “Hydration mechanisms of two polymorphs of synthetic ye’elimite,” Cement and Concrete Research, V. 63, 2014, pp. 127–

36.

6. Álvarez-Pinazo, G., Cuesta, A., García-Maté, M., et al. “In-situ early-age hydration study of sulfobelite cements by synchrotron powder diffraction,” Cement and Concrete Research, V.

56, 2014, pp. 12–9.

7. Morin, V., Walenta, G., Gartner, E., et al. “Hydration of a Belite-Calcium Sulfoaluminate-Ferrite cement : Aether TM.” 13th International Congress on the Chemistry of Cement. 2011.

pp. 1–7.

8. Li, G. S., Walenta, G., and Gartner, E. M. “Formation and Hydration of Low-CO 2 Cements Based on Belite, Calcium Sulfoaluminate and Calcium Aluminoferrite,” 12th International

Congress on the Chemistry of Cement., No. November 2015, 2007.

9. Wang, J. “Hydration mechanism of cements based on low-CO2 clinkers containing belite, ye’elimite and calcium alumino-ferrite.” Université Lille 1, 2010.

10. Álvarez-Pinazo, G., Santacruz, I., Aranda, M. A. G., et al. “Hydration of belite–ye’elimite–ferrite cements with different calcium sulfate sources,” Advances in Cement Research, V. 28, No. 8, 2016, pp. 529–43.

11. Álvarez-Pinazo, G., Santacruz, I., León-Reina, L., et al. “Hydration Reactions and Mechanical Strength Developments of Iron-Rich Sulfobelite Eco-cements,” Industrial &

Engineering Chemistry Research, V. 52, No. 47, 2013, pp. 16606–14.

12. Fukuhara, M., Goto, S., Asaga, K., et al. “Mechanisms and kinetics of C4AF hydration with gypsum,” Cement and Concrete Research, V. 11, No. 3, 1981, pp. 407–14.

13. Möschner, G., Lothenbach, B., Winnefeld, F., et al. “Solid solution between Al-ettringite and Fe-ettringite,” Cement and Concrete Research, V. 39, No. 6, 2009, pp. 482–9.

14. Meller, N., Hall, C., Jupe, A. C., et al. “The paste hydration of brownmillerite with and without gypsum : a time resolved synchrotron diffraction study at 30 , 70 , 100 and 150 u C,” 2004.

15. Zajac, M., Skocek, J., Bullerjahn, F., et al. “Effect of retarders on the early hydration of calcium-sulpho-aluminate (CSA) type cements,” Cement and Concrete Research, V. 84,

2016, pp. 62–75.

16. Ma, B., Ma, M., Shen, X., et al. “Compatibility between a polycarboxylate superplasticizer and the belite-rich sulfoaluminate cement: Setting time and the hydration properties,”

Construction and Building Materials, V. 51, 2014, pp. 47–54.

17. He, Z., Shen, A., Guo, Y., et al. “Cement-based materials modified with superabsorbent polymers: A review,” Construction and Building Materials, V. 225, 2019, pp. 569–90.

18. Marchon, D., and Flatt, R. J. “Impact of chemical admixtures on cement hydration.” In: Aïtcin, P.-C., Flatt, R. J., eds. Science and Technology of Concrete Admixtures. Elsevier,

2016. pp. 279–304.

19. Gargulak, J. D., and Lebo, S. E. “Commercial use of lignin-based materials,” ACS Symposium Series, V. 742, No. Figure 1, 1999, pp. 304–20.

20. Arel, H. Ş., and Aydin, E. “Effects of Ca-, Mg-, K-, and Na-lignosulfonates on the behavior of fresh concrete,” Construction and Building Materials, V. 157, 2017, pp. 1084–91.

21. Colombo, A., Geiker, M., Justnes, H., et al. “The effect of calcium lignosulfonate on ettringite formation in cement paste,” Cement and Concrete Research, V. 107, No. January,

2018, pp. 188–205.

22. Bishop, M., and Barron, A. R. “Cement hydration inhibition with sucrose, tartaric acid, and lignosulfonate: Analytical and spectroscopic study,” Industrial and Engineering Chemistry

Research, V. 45, No. 21, 2006, pp. 7042–9.

23. Danner, T., Justnes, H., Geiker, M., et al. “Phase changes during the early hydration of Portland cement with Ca-lignosulfonates,” Cement and Concrete Research, V. 69, 2015, pp.

50–60.

24. Paulini, P. “Reaction mechanisms of concrete admixtures,” Cement and Concrete Research, V. 20, No. 6, 1990, pp. 910–8.

25. Kauppi, A., Andersson, K. M., and Bergström, L. “Probing the effect of superplasticizer adsorption on the surface forces using the colloidal probe AFM technique,” Cement and

Concrete Research, V. 35, No. 1, 2005, pp. 133–40.

26. Marchon, D., Juilland, P., Gallucci, E., et al. “Molecular and submolecular scale effects of comb-copolymers on tri-calcium silicate reactivity: Toward molecular design,” Journal of

the American Ceramic Society, V. 100, No. 3, 2017, pp. 817–41.

27. Plank, J., and Hirsch, C. “Impact of zeta potential of early cement hydration phases on superplasticizer adsorption,” Cement and Concrete Research, V. 37, No. 4, 2007, pp. 537–

42.

28. Zingg, A., Winnefeld, F., Holzer, L., et al. “Adsorption of polyelectrolytes and its influence on the rheology, zeta potential, and microstructure of various cement and hydrate phases,” Journal of Colloid and Interface Science, V. 323, No. 2, 2008, pp. 301–12.

29. Bishop, M., and Barron, A. R. “Cement Hydration Inhibition with Sucrose, Tartaric Acid, and Lignosulfate: Analytical and Spectoscopic Study,” Industrial Eng. Chem. Res., V. 45,

No. 21, 2006, pp. 7042–9.