Title:
Comparison of Several Methodologies Used for Designing Tabletop Foundations
Author(s):
Mukti Lal Das
Publication:
Symposium Paper
Volume:
348
Issue:
Appears on pages(s):
35-46
Keywords:
Rule-of-thumb, Eigenvalues, Rayleigh frequencies, Turbine force amplitude
DOI:
10.14359/51732678
Date:
3/1/2021
Abstract:
The availability of high-speed computers at a reasonable price resulted in various sophisticated analysis
and design methodologies for the elevated flexible pedestal (Tabletop) foundations replacing the rule-of-thumb
processes based on static equivalent principle which used to produce either unsafe or overly conservative structures.
A thorough study is undertaken with four typical models usually selected for static and dynamic analyses
in the structural/mechanical engineering practice. It is found that all the models provide comparable results. However,
each one has its own advantages and disadvantages. These will be highlighted in the Summary and Concluding
Remarks of this paper.
Related References:
1. Arya, S. C., O’Neill, M. W., and Pincus, G., 1984. “Design of Structures and Foundations for Vibrating Machines,” Gulf Publishing Company, 113-186.
2. American Concrete Institute, 2018. “Report on Foundations for Dynamic Equipment,” ACI Committee ACI 351.3R-18, 42-56.
3. Biggs, J. M., 1964. “Introduction to Structural Dynamics,” McGraw-Hill Book Company, 85-149.
4. Bhatia, K. G., 2008. “Foundations for Industrial Machines,” D-CAD Publishers, New Delhi, (6-1) – (10-78).
5. Das, Braja M., 1990. “Principles of Foundation Engineering,” PWS-KENT Publishing Company, 211-248.
6. STAAD/STAAD.Pro, Bentley Systems, Inc., 685 Stockton Dr., Exton, PA 19341, USA.
7. “Proceedings of the First International Conference, Application of Artificial Intelligence in Engineering Problems,” Southampton University, UK, Springer Verlag, Berlin, 1986.