Abstract:
The inclusion of rubber in concrete mixtures improved the impact resistance but negatively affected the strength and fresh properties of self-consolidating concrete (SCC). The objective of this investigation was to optimize the balance between the improved impact resistance and the reductions in the strength and fresh properties of rubberized SCC mixtures. This investigation evaluated and assessed the type/size and percentage of rubber needed to
develop successful SCC mixtures with maximized impact strength and minimized reductions in strength. The studied
variables were the type/size of rubber used (crumb rubber (CR) and two sizes of powder rubbers), percentage of rubber
(0%, 15%, 25%, 30%, 35%, and 40%), type of concrete (SCC and vibrated concrete), and the use of fibers in the mixture. Because of the fresh properties restrictions of SCC, it was only possible to develop rubberized SCC with up to 25%, 30%, and 35% CR, powder rubber 40/80, and powder rubber 140, respectively. With the absence of fresh properties restrictions of SCC, it was possible to develop vibrated rubberized concrete with up to 40% of any type of
rubber. Using higher percentages of rubber in vibrated rubberized concrete dropped the compressive strength to less than 25 MPa (3.63 ksi). The results also indicated that despite the slight improvement in the fresh properties and strength of mixtures with powder rubbers compared to mixtures with CR, mixtures with CR showed significantly higher improvements in the impact resistance.
Related References:
1. Ismail, M. K., De Grazia, M. T., and Hassan, A. A. A., 2015, “Mechanical properties of self-consolidating rubberized concrete with different supplementary cementing materials”, Proceedings of International Conference on Transportation and Civil Engineering (ICTCE'15), London, UK.
2. Gupta, T., Sharma, R. K., and Chaudhary, S., 2015, “Impact resistance of concrete containing waste rubber fiber and silica fume”, International Journal of Impact Engineering, 83, 76–87.
3. Al-Tayeb, M. M., Abu Bakar, B. H., Akil, H. M., and Ismail, H., 2012, “Effect of partial replacements of sand and cement by waste rubber on the fracture characteristics of concrete”, Polymer-Plastics Technology and Engineering, 51(6), 583–589.
4. Najim, K. B., and Hall, M. R., 2010, “A Review of the fresh/hardened properties and applications for plain-(PRC) and self-compacting rubberised concrete (SCRC)”, Construction and Building Materials, 24(11), 2043–2051.
5. Su, H., Yang, J., Ling, T. C., Ghataora, G. S., and Dirar, S., 2015, “Properties of concrete prepared with waste tyre rubber particles of uniform and varying sizes”, Journal of Cleaner Production, 91, 288–296.
6. Najim, K. B., and Hall, M., 2012, “Mechanical and dynamic properties of self-compacting crumb rubber modified concrete”, Construction and Building Materials, 27(1), 521–530.
7. Ismail, M. K., and Hassan, A. A. A., 2016, “Use of metakaolin on enhancing the mechanical properties of selfconsolidating concrete containing high percentages of crumb rubber”, Journal of Cleaner Production, 125, 282–295.
8. Ismail, M. K., and Hassan, A. A. A., 2016, “Impact resistance and acoustic absorption capacity of selfconsolidating rubberized concrete”, ACI Materials Journal, 113(6), 725-736.
9. Ismail, M. K., and Hassan, A. A. A., 2015, “Influence of mixture composition and type of cementitious materials on enhancing the fresh properties and stability of self-consolidating rubberized concrete”, Journal of Materials in Civil Engineering (ASCE), 28(1), 04015075.
10. Ganjian, E., Khorami, M, and Maghsoudi, A.A., 2009, “Scrap-tyre-rubber replacement for aggregate and filler in concrete”, Construction and Building Materials, 23(5), 1828–1836.
11. Zheng, L., Sharon Huo, X., and Yuan, Y., 2008, “Experimental investigation on dynamic properties of rubberized concrete”, Construction and Building Materials, 22(5), 939–947.
12. Taha, M. M., El-Dieb, A. S., Abd El-Wahab, M. A., and Abdel-Hameed, M. E., 2008, “Mechanical, fracture, and microstructural investigations of rubber concrete”, Journal of Materials in Civil Engineering, 20(10), 640–649.
13. Topçu, I. B., 1995, “The properties of rubberized concretes,” Cement and Concrete Research, 25(2), 304–310.
14. Gheni, A. A., and ElGawady, M. A., 2019, “Recycled additive to improve freeze-thaw durability of high fly ash content mortar,” ACI Special Publications, 334, 166–184
15. Li, G., Stubblefield, M., Garrick, G., Eggers, J., Abadie, C., and Huang, B., 2002, “Development of waste tire modified concrete”, Cement and Concrete Research, 34(12), 2283–2289.
16. Ismail, M. K., and Hassan, A. A. A., 2017, “Use of steel fibers to optimize self-consolidating concrete mixtures containing crumb rubber”, ACI Materials Journal, 114(4), 581-594.
17. Khatib, Z. K., and Bayomy, F. M., 1999, “Rubberized portland cement concrete”, Journal of Materials in Civil Engineering, 11(3), 206–213.
18. Khaloo, A. R., Dehestani, M., and Rahmatabadi, P., 2008, “Mechanical properties of concrete containing a high volume of tire-rubber particles”, Waste Management, 28(12), 2472–2482.
19. Ismail, M. K., Sherir, M. A., Siad, H., Hassan, A. A. A., and Lachemi, M., 2018, “Properties of self-consolidating engineered cementitious composite modified with rubber”, Journal of Materials in Civil Engineering (ASCE), 30(4), 04018031.
20. Song, P. S., and Hwang, S. 2004, “Mechanical properties of high-strength steel fiber–reinforced concrete”, Construction and Building Materials, 18(9), 669–673.
21. Khaloo, A., Raisi, E. M., Hosseini, P., and Tahsiri, H., 2014, “Mechanical performance of self–compacting concrete reinforced with steel fibers”, Construction and Building Materials, 51, 179–186.
22. Nia, A. A., Hedayatian, M., Nili, M., and Sabet, V.A., “An experimental and numerical study on how steel and polypropylene fibers affect the impact resistance in fiber-reinforced concrete”, International Journal of Impact Engineering, 46, 62–73.
23. Jun Li, J., Gang Niu, J., Jun Wan, C., Jin, B., and Liu Yin, Y., “Investigation on mechanical properties and microstructure of high performance polypropylene fiber reinforced lightweight aggregate concrete”, Construction and Building Materials, 118, 27–35.
24. Lee, J. H., Yoo, D. Y., and Yoon, Y. S., 2016, “Mechanical behaviour of concrete with amorphous metallic and steel fibres”, Magazine of Concrete Research, 68(24), 1253–1264.
25. Ganesan, N., Raj, B., and Shashikala, A. P., 2013, “Behavior of self-consolidating rubberized concrete beamcolumn joints”, ACI Materials Journal, 110(6), 697-704.
26. AbdelAleem, B. H., Ismail, M. K., and Hassan, A. A. A., 2018, “Effect of synthetic fibers on shear capacity of reinforced rubberized concrete beams”, ACI Materials Journal, 115(2), 279–288.
27. AbdelAleem, B. H., Ismail, M. K., and Hassan, A. A. A., 2018, “The combined effect of crumb rubber and synthetic fibers on impact resistance of self-consolidating concrete”, Construction and Building Materials, 162, 816–829.
28. Sallam, H. E. M., Sherbini, A. S., Seleem, M. H., and Balaha, M. M., 2008, “Impact resistance of rubberized concrete”, Engineering Research Journal, 31(3), 265–271.
29. Ismail, M. K., and Hassan, A. A. A., 2016, “Impact resistance and mechanical properties of self-consolidating rubberized concrete reinforced with steel fibers”, Journal of Materials in Civil Engineering (ASCE), 29(1), 04016193.
30. ACI, 1999, “Measurement of properties of fiber reinforced concrete,” ACI 544.2 R-89, West Conshohocken, PA.
31. EFNARC, 2005, “The European Guidelines for self-compacting concrete specification, production and use”, European Federation for Specialist Construction Chemicals and Concrete Systems, English ed. Norfolk, UK.
32. Atis, C. D., and Karahan, O., 2009, "Properties of steel fiber reinforced fly ash concrete”, Construction and Building Materials, 23(1), 392-399.
33. Olivito, R. S., and Zuccarello, F. A., 2010, “An experimental study on the tensile strength of steel fiber reinforced concrete”, Composite Part B, 41(3), 246-255.