Title: Changes in ACI 318 Code Provisions for Earthquake-Resistant Structures, Part 1

Author(s): S.K. Ghosh and Andrew W. Taylor

Publication: Concrete International

Volume: 43

Issue: 3

Appears on pages(s): 45-49

Keywords: keywords: joint, reinforcement, beam, column

DOI: 10.14359/51732620

Date: 3/1/2021

Abstract:
Only three sections in Chapter 18—Earthquake-Resistant Structures of ACI 318-19 remain unchanged in comparison to ACI 318-14. This is the first of two articles that outline these changes, covering changes in sections governing structural systems, mechanical splices, and the design of moment frames.

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 623 pp.

2. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.