Seismic Performance of Reinforced Concrete Frame Joints after Exposure to Fire

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Performance of Reinforced Concrete Frame Joints after Exposure to Fire

Author(s): Y. Wang, V. K. R. Kodur, C. Fu, C. Liu, H. Zhou, and M. Z. Naser

Publication: Structural Journal

Volume: 118

Issue: 3

Appears on pages(s): 3-14

Keywords: cyclic loading tests; ductility; post-heating response; reinforced concrete framed joints; residual capacity; seismic performance

DOI: 10.14359/51731586

Date: 5/1/2021

Abstract:
An experimental study was carried out to investigate the seismic performance of fire-exposed reinforced concrete (RC) frame joints. This experimental program consisted of testing four full-scale joints used in RC frames. The first joint was tested under ambient conditions to serve as a benchmark case and to study room temperature response of concrete joints. The other three full-scale joints were exposed to different fire exposure scenarios and then tested, after cooling down to room temperature, by subjecting the joints to different levels of combined axial loading and cyclic lateral displacement history to simulate seismic loading conditions. Test results indicate that RC frame joints do not experience significant damage when exposed to 60 minutes of fire because most temperature-induced degradation in concrete and steel gets fully recovered upon cooling. However, joints in RC frames exposed to 90 minutes of fire undergo substantial damage due to significant temperature-induced property degradation in concrete and steel.

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete and Commentary (ACI 318M-05),” American Concrete Institute, Farmington Hills, MI, 2005, 438 pp.

2. Kodur, V. K. R.; Yu, B.; and Dwaikat, M. M. S., “A Simplified Approach for Predicting Temperature in Reinforced Concrete Members Exposed to Standard Fire,” Fire Safety Journal, V. 56, Feb. 2013, pp. 39-51. doi: 10.1016/j.firesaf.2012.12.004

3. Han, L.; Tan, Q.; and Song, T., “Fire Performance of Steel Reinforced Concrete (SRC) Structures,” Procedia Engineering, V. 62, Sept. 2013, pp. 46-55. doi: 10.1016/j.proeng.2013.08.043

4. Tsonos, A. G., “Cyclic Load Behavior of Reinforced Concrete Beam-Column Subassemblages of Modern Structures,” ACI Structural Journal, V. 104, No. 4, July-Aug. 2007, pp. 468-478.

5. Teng, S., and Zhou, H., “Eccentric Reinforced Concrete Beam-Column Joints Subjected to Cyclic Loading,” ACI Structural Journal, V. 100, No. 2, Mar.-Apr. 2003, pp. 139-148.

6. Park, R., “A Summary of Results of Simulated Seismic Load Tests on Reinforced Concrete Beam-Column Joints, Beams and Columns with Substandard Reinforcing Details,” Journal of Earthquake Engineering, V. 6, No. 2, 2002, pp. 147-174. doi: 10.1080/13632460209350413

7. Pauletta, M.; Di Luca, D.; and Russo, G., “Exterior Beam Column Joints—Shear Strength Model and Design Formula,” Engineering Structures, V. 94, July 2015, pp. 70-81. doi: 10.1016/j.engstruct.2015.03.040

8. Liu, C.; Bai, G.; Jia, S.; and Yin, L., “Experimental Study on Seismic Behavior of Recycled Concrete Frame Joints with Different Axial Compression Ratios,” Tumu Gongcheng Xuebao, V. 46, No. 6, 2013, pp. 21-28.

9. Shafaei, J.; Zareian, M.; Hosseini, A.; and Marefat, M., “Effects of Joint Flexibility on Lateral Response of Reinforced Concrete Frames,” Engineering Structures, V. 81, Dec. 2014, pp. 412-431. doi: 10.1016/j.engstruct.2014.09.046

10. Xing, G.; Liu, B.; and Niu, D., “Shear Strength of Reinforced Concrete Frame Joints Using Modified Softened Strut-and-Tie Model,” Engineering Mechanics, V. 30, No. 8, 2013, pp. 60-66.

11. Duan, H. J., and Hueste, M., “Seismic Performance of a Reinforced Concrete Frame Building in China,” Engineering Structures, V. 41, Aug. 2012, pp. 77-89. doi: 10.1016/j.engstruct.2012.03.030

12. ACI Committee 352, “Recommendations for Design of Beam-Column Connections in Monolithic Reinforced Concrete Structures (ACI 352R-02),” American Concrete Institute, Farmington Hills, MI, 2002, 38 pp.

13. European Committee for Standardization, “Eurocode 2: Design of Concrete Structures—Part 1–2: General Rules-Structural Fire Design (EN 1992-1-2),” CEN, Brussels, Belgium, 2004.

14. European Committee for Standardization, “Eurocode 8: Design of Structures for Earthquake Resistance—Part 1: General Rules, Seismic Actions and Rules for Buildings (EN 1998-1),” prEN 1998-1-1/2/3, CEN, Brussels, Belgium, 2004.

15. Xiao, J. Z.; Li, J.; and Huang, Z. F., “Fire Response of High-Performance Concrete Frames and Their Post-Fire Seismic Performance,” ACI Structural Journal, V. 105, No. 5, Sept.-Oct. 2008, pp. 531-540.

16. Mousavi, S.; Bagchi, A.; and Kodur, V. K. R., “Review of Post-Earthquake Fire Hazard to Building Structures,” Canadian Journal of Civil Engineering, V. 35, No. 7, 2008, pp. 689-698. doi: 10.1139/L08-029

17. Kodur, V. K. R.; Garlock, M.; and Iwankiw, N., “Structures in Fire: State-of-the-Art, Research and Training Needs,” Journal of Fire Technology, V. 48, Nov. 2012, pp. 825-839. doi: 10.1007/s10694-011-0247-4

18. Zhu, S., and Jirsa, J., “Study of Bond Deterioration in Reinforced Concrete Beam-Column Joints,” Phil M. Ferguson Structural Engineering Laboratory, The University of Texas at Austin, Austin, TX, 1983.

19. Kamath, P.; Sharma, U.; Kumar, V.; Bhargava, P.; Usmani, A.; Singh, B.; Singh, Y.; Torero, J.; Gillie, M.; and Pankaj, P., “Full-Scale Fire Test on an Earthquake-Damaged Reinforced Concrete Frame,” Fire Safety Journal, V. 73, Apr, 2015, pp. 1-19. doi: 10.1016/j.firesaf.2015.02.013

20. Meacham, B.; Engelhardt, M.; and Kodur, V., “Collection of Data on Fire and Collapse,” Proceedings, 2009 NSF Engineering Research and Innovation Conference, Honolulu, HI, 2009.

21. China Academy of Building Research, “National Standard of the People’s Republic of China: Code for Seismic Design of Buildings (GB50011-2010),” China Architecture and Building Press, Beijing, China, 2010.

22. China Academy of Building Research, “National Standard of the People’s Republic of China: Code for Design of Concrete Structures (GB50010-2010),” China Architecture and Building Press, Beijing, China, 2010.

23. International Organization for Standardization, “Fire-Resistance Tests—Elements of Building Construction—Part 1: General Requirements (ISO 834-1),” ISO, Geneva, Switzerland, 1999.

24. Chen, X.; Wu, S.; and Zhou, J., “Large-Beam Tests on Mechanical Behavior of Dam Concrete under Dynamic Loading,” Journal of Materials in Civil Engineering, ASCE, V. 27, No. 10, 2015, p. 06015001. doi: 10.1061/(ASCE)MT.1943-5533.0001263

25. Al-Salloum, Y., and Almusallam, T., “Seismic Response of Interior RC Beam-Column Joints Upgraded with FRP Sheets. I: Experimental Study,” Journal of Composites for Construction, ASCE, V. 11, No. 6, 2007, pp. 575-589. doi: 10.1061/(ASCE)1090-0268(2007)11:6(575)

26. Park, R., “Evaluation of Ductility of Structures and Structural Assemblages from Laboratory Testing,” Bulletin of the New Zealand National Society for Earthquake Engineering, V. 22, No. 3, 1989, pp. 155-166. doi: 10.5459/bnzsee.22.3.155-166

27. Shannag, M., and Alhassan, A., “Seismic Upgrade of Interior Beam-Column Subassemblages with High-Performance Fiber-Reinforced Concrete Jackets,” ACI Structural Journal, V. 102, No. 1, Jan.-Feb. 2005, pp. 131-138.

28. Shannag, M.; Abu-Dyya, N.; and Abu-Farsakh, G., “Lateral Load Response of High Performance Fiber Reinforced Concrete Beam–Column Joints,” Construction and Building Materials, V. 19, No. 7, 2005, pp. 500-508. doi: 10.1016/j.conbuildmat.2005.01.007

29. Saadatmanesh, H.; Ehsani, M.; and Jin, L., “Repair of Earthquake-Damaged RC Columns with FRP Wraps,” ACI Structural Journal, V. 94, No. 2, Mar.-Apr. 1997, pp. 206-215.


ALSO AVAILABLE IN:

Electronic Structural Journal