An Overview of The Tensile and Bond Behavior of Fabric Reinforced Cementitious Matrix (FRCM) Composites

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: An Overview of The Tensile and Bond Behavior of Fabric Reinforced Cementitious Matrix (FRCM) Composites

Author(s): Gianmarco de Felice, Stefano De Santis, and Pietro Meriggi

Publication: Symposium Paper

Volume: 345

Issue:

Appears on pages(s): 207-220

Keywords: Round Robin Test (RRT), Steel Reinforced Grout (SRG), Shear bond tests, Tensile tests, Test methods, Textile Reinforced Mortar (TRM).

DOI: 10.14359/51731582

Date: 2/1/2021

Abstract:
In 2017, the Rilem Technical Committee 250-CSM coordinated a Round Robin initiative, in which 19 research institutions tested 28 Fabric Reinforced Cementitious Matrix (FRCM) composites, with the support of 11 industrial partners. Two years after the publication of the first papers on the results of this wide investigation, it is still worth further analysing its outcomes to highlight the fundamental properties of mortar-based reinforcements and give an overview of the various available fabrics and matrices, which are currently used in structural rehabilitation activities. Equally, a better understanding still needs to be gained on the causes of the variability observed in test results. These include the quasibrittle behaviour of the inorganic matrix and its sensitivity to manufacturing, curing and handling. Test implementation, such as gripping method and measuring techniques, also plays a crucial role in the reliability and repeatability of experimental outcomes.

Related References:

1. Loreto, G., Babaeidarabad, S., Leardini, L., Nanni, A., “RC beams shear-strengthened with fabric-reinforcedcementitious-matrix (FRCM) composite”, International Journal of Advanced Structural Engineering, Vol. 7, No. 4, 2015, pp. 341-352.

2. Napoli, A., Realfonzo, R., “Reinforced concrete beams strengthened with SRP/SRG systems: Experimental investigation”, Construction and Building Materials, Vol. 93, 2015, pp. 654-677.

3. Pino, V., Akbari Hadad, H., De Caso y Basalo, F., Nanni, A., Ali Ebead, U., El Refai, A., “Performance of FRCM-Strengthened RC Beams Subject to Fatigue”, Journal of Bridge Engineering, Vol. 22, No. 10, 2017, 04017079.

4. Raoof, S.M., Koutas, L.N., Bournas, D.A. “Textile-reinforced mortar (TRM) versus fibre-reinforced polymers (FRP) in flexural strengthening of RC beams”, Construction and Building Materials, Vol. 151, 2017, pp. 279-291.

5. Borri, A., Casadei, P., Castori, G., Hammond, J., “Strengthening of brick masonry arches with externally bonded steel reinforced composites”, Journal of Composites for Construction, Vol. 13, No. 6, 2009, pp. 468-475.

6. Papanicolaou, C.G., Triantafillou, T.C., Lekka, M., “Externally bonded grids as strengthening and seismic retrofitting materials of masonry panels”, Construction and Building Materials, Vol. 25, No. 2, 2011, pp. 504-515.

7. Balsamo, A., Di Ludovico, M., Prota, A., Manfredi, G., “Masonry walls strengthened with innovative composites”, ACI Special Publication, Vol. 275, 2011, pp. 769-786.

8. Babaeidarabad, S., De Caso, F., Nanni, A., “Out-of-Plane Behavior of URM Walls Strengthened with Fabric-Reinforced Cementitious Matrix Composite”, Journal of Composites for Construction, Vol. 18, No. 4, 2014, e04013057.

9. Marcari, G., Basili, M., Vestroni, F., “Experimental investigation of tuff masonry panels reinforced with surface bonded basalt textile-reinforced mortar”, Composites Part B: Engineering, Vol. 108, 2017, pp. 131-142.

10. De Santis, S., Roscini, F., de Felice, G. “Full-scale tests on masonry vaults strengthened with Steel Reinforced Grout”, Composites Part B: Engineering, Vol. 141, 2018, pp. 20-36.

11. Bellini, A., Incerti, A., Bovo, M., Mazzotti, C., “Effectiveness of FRCM reinforcement applied to masonry walls subject to axial force and out-of-plane loads evaluated by experimental and numerical studies”, International Journal of Architectural Heritage, Vol. 12, No. 3, 2018, pp. 376-394.

12. De Santis, S., De Canio, G., de Felice, G., Meriggi, P., Roselli, I., “Out‑of‑plane seismic retrofitting of masonry walls with Textile Reinforced Mortar composites”, Bulletin of Earthquake Engineering, Vol. 17, No. 11, 2019, pp. 6265-6300.

13. De Santis, S., Roscini, F., de Felice, G., “Retrofitting of masonry vaults by basalt-textile reinforced mortar overlays”, International Journal of Architectural Heritage, Vol. 13, No. 7, 2019, pp. 1061-1077.

14. D'Ambrisi, A., Feo, L., Focacci, F., “Experimental and analytical investigation on bond between Carbon-FRCM materials and masonry”, Composites Part B: Engineering, Vol. 46, 2013, pp. 15-20.

15. Carozzi, F.G., Poggi, C., “Mechanical properties and debonding strength of Fabric Reinforced Cementitious Matrix (FRCM) systems for masonry strengthening”, Composites Part B: Engineering, Vol. 70, 2015, pp. 215-230.

16. Sneed, L.H., D'Antino, T., Carloni, C., “Investigation of bond behavior of polyparaphenylene benzobisoxazole fiber-reinforced cementitious matrix composite-concrete interface”, ACI Materials Journal, Vol. 111, No. 5, 2014, pp. 569-580.

17. Alecci, V., Focacci, F., Rovero, L., Stipo, G., De Stefano, M., “Extrados strengthening of brick masonry arches with PBO–FRCM composites: Experimental and analytical investigations”, Composite Structures, Vol. 149, 2016, pp. 184-196.

18. D’Antino, T., Colombi, P., Carloni, C., Sneed, L.H., “Estimation of a matrix-fiber interface cohesive material law in FRCM-concrete joints”, Composite Structures, Vol. 193, 2018, pp. 103-112.

19. De Santis, S., “Bond behaviour of Steel Reinforced Grout for the extrados strengthening of masonry vaults”, Construction and Building Materials, Vol. 150, 2017, pp. 367-382.

20. De Santis, S., Carozzi, F.G., de Felice, G., Poggi, C., “Test methods for Textile Reinforced Mortar systems”, Composites Part B: Engineering, Vol. 127, 2017, pp. 121-132.

21. D’Antino, T., Papanicolaou, C., “Comparison between different tensile test set-ups for the mechanical characterization of inorganic-matrix composites”, Construction and Building Materials, Vol. 171, 2018, pp. 140-151.

22. de Felice, G., Aiello, M.A., Caggegi, C., Ceroni, F., De Santis, S., Garbin, E., Gattesco, N., Hojdys, Ł., Krajewski, P., Kwiecień, A., Leone, M., Lignola, G.P., Mazzotti, C., Oliveira, D.V., Papanicolaou, C., Poggi, C., Triantafillou, T., Valluzzi, M.R., Viskovic, A., “Recommendation of RILEM TC 250-CSM: Test method for Textile Reinforced Mortar to substrate bond characterization”, Materials and Structures, Vol. 51, No. 4, 2018, 95.

23. De Santis, S., Hadad, H.A., De Caso y Basalo FJ, de Felice G, Nanni A., “Acceptance Criteria for Tensile Characterization of Fabric Reinforced Cementitious Matrix (FRCM) Systems for Concrete and Masonry Repair”, Journal of Composites for Construction, Vol. 22, No. 6, 2018, 04018048.

24. Lignola, G.P., Caggegi, C., Ceroni, F., De Santis, S., Krajewski, P., Lourenço, P.B., Morganti, M., Papanicolaou, C., Pellegrino, C., Prota, A., Zuccarino, L., “Performance assessment of basalt FRCM for retrofit applications on masonry”, Composites Part B: Engineering, Vol. 128, 2017, pp. 1-18.

25. Carozzi, F.G., Bellini, A., D’Antino, T., de Felice, G., Focacci, F., Hojdys, L., Laghi, L., Lanoye, E., Micelli, F., Panizza, M., Poggi, C., “Experimental investigation of tensile and bond properties of Carbon-FRCM composites for strengthening masonry elements”, Composites Part B: Engineering, Vol. 128, 2017, pp. 100-119.

26. Leone, M., Aiello, M.A., Balsamo, A., Carozzi, F.G., Ceroni, F., Corradi, M., Gams, M., Garbin, E., Gattesco, N., Krajewski, P., Mazzotti, C., Oliveira, D.V., Papanicolaou, C.G., Ranocchiai, G., Roscini, F., Saenger, D. “Glass fabric reinforced cementitious matrix: Tensile properties and bond performance on masonry

substrate”, Composites Part B: Engineering, Vol. 127, 2017, pp. 196-214.

27. Caggegi, C., Carozzi, F.G., De Santis, S., Fabbrocino, F., Focacci, F., Hojdys, L., Lanoye, E., Zuccarino, L., “Experimental analysis on tensile and bond properties of PBO and Aramid fabric reinforced cementitious matrix for strengthening masonry structures”, Composites Part B: Engineering, Vol. 127, 2017, pp. 175-195.

28. De Santis, S., Ceroni, F., de Felice, G., Fagone, M., Ghiassi, B., Kwiecień, A., Lignola, G.P., Morganti, M., Santandrea, M., Valluzzi, M.R., Viskovic, A., “Round Robin Test on tensile and bond behaviour of Steel Reinforced Grout systems”, Composites Part B: Engineering, Vol. 127, 2017, pp. 100-120.

29. de Felice, G., D’Antino, A., De Santis, S., Meriggi, P., Roscini, F., “Lessons learned on the tensile and bond behaviour of Fabric Reinforced Cementitious Matrix (FRCM) composites”, Frontiers in Built Environment, Vol. 6, 2020, 5.

30. European Committee for Standardization, “EN 1990:2002. Eurocode 0: Basis of structural design”.

31. D'Antino, T., Papanicolaou, C., “Mechanical characterization of textile reinforced inorganic-matrix composites”, Composites Part B: Engineering, Vol. 127, 2017, pp. 78-91.