Abstract:
There is a great demand in the world for low-cost and functional pipeline systems due to the renovation requirements of pipes in use and the continuous development of new settlements. Previously used pipeline systems made of steel reinforced concrete are economical and sufficiently resistant. However, due to the corrodibility of steel
reinforcement and to enable sufficient crack reduction, large wall thicknesses and thus heavy constructions are required. Textile reinforced concrete (TRC) eliminates these disadvantages by enabling the production of light and thin-walled structures.
The aim of this research is the development of a concept for the realization of smart pipes made of sensory TRC by using the advantages of lightweight, thin-walled structures, focusing on the production process. Based on different warp knitted textile variations with different coating concentrations, preliminary tests were carried out using the fourpoint bending test. As a result of the preliminary tests, the textile variation of counterlaid tricot with a maximum coating concentration was selected as a suitable reinforcing material for the concept development. Concepts for the
production of smart TRC pipes are developed accordingly. As a result, a casting mold and process were created which allowed a production with reduced diameter and depth of pores and concentric positioning of the reinforcement structure.
Related References:
1. Cherif, C.; Schorn, H.; Horlacher, H.-B.; Offermann, P.: Entwicklung und Erprobung neuer, innovativer Verbundrohr-systeme (Kunststoff-Textilbeton-Verbundsystem) einschließlich ihrer Herstellungstechnologie Schlussbericht zum AiF-Forschungsprojekt, 2006, Tu Dresden
2. Colombo, I. G.; Magri, A., Zani, G.; Colombo, M.; di Prisco, M.: Erratum to: Textile Reinforced Concrete: experimental investigation on design parameters Materials and Structures, 2013, Volume 46, pp 1953-1971
3. Quadflieg, T.; Goldfeld, Y.; Dittel, G.; Gries, T.: New Age Advanced Smart Water Pipe Systems Using Textile Reinforced Concrete, Procedia Manufacturing, Volume 21, 2018, pp 376-383
4. Quadflieg, T.: Gewirkte Verstärkungstextilien mit kohlenstofffaserbasierter Sensorik im Verbundwerkstoff mit mineralischer Matrix, Dissertation, 2017, RWTH Aachen, Aachen
5. Goldfeld, Y., Ben-Arosh, S., Rabinovitsch, O., Quadflieg, T., and Gries, T: Micor and macro crack sensing in TRC beam under cyclic loading, Journal of Mechanics of Material Structures, 2017, Volume 12, No. 5, pp 579-601
6. Goldfeld, Y., Quadflieg, T., Ben-Arosh, S., O., and Gries, T: Integrated Self-Monitoring of Carbon Based Textile Reinforced Concrete Beams under Repeated Loading in the Un-Cracked Region, Carbon, 2016, Volume 98, pp 238-249
7. Goldfeld, Y.; Quadflieg, T. and Gries, T.: Sensing Capabilities of Carbon Cased TRC Beam from Slack to Pull-out Mechanism, Composite Structures, 2017, Volume 181, pp 294-305
8. Hartig, C. A.: Experimental Analysis of the Effects of organic and inorganic Coatings on the mechanical Properties of Basalt Fibre Rein-forcement in textile-reinforced Concrete, Bachelorarbeit, RWTH Aachen University, Aachen, März 2018
9. Brameshuber, W.; Hegger, J.; Gries, T.; Dilger, K.; Böhm, S.; Mott, R.; Voss, S.; Barlé, M.; Hartung, I.: Serielle Einzelfertigung (Stückfertigung) von Bauteilen aus textilbewehrtem Beton
10. Peled, A.; Bentur, A.; Mobasher, B.: Textile reinforced Concrete, CRC Press, 2007, Boca Ranton, Florida, USA
11. R. Fangueiro, F. Soutinho: 3 - Textile structures, Editor(s): R. Fangueiro, In Woodhead Publishing Series in Textiles, Fibrous and Composite Materials for Civil Engineering Appli-cations, Woodhead Publishing, 2011, Pages 62-91
12. Yin, S.; Xu, S.; Li, H.: Improved mechanical properties of textile reinforced concrete thin plate, Journal of Wuhan University of Technology-Mater. Sci. Ed., 2013, Volume 28, Issue 1, pp 92-98
13. Sonderforschungsbereich 532: Textilbewehrter Beton – Grundlagen für die Entwicklung einer neuartigen Technologie, Abschlussbericht, 2011
14. Kimm, M.; Gerstein, N.; Schmitz, P.; Simons, M.; Gries, T.: On the separation and recycling behaviour of textile reinforced concrete: an experimental study, Material and Structures, 2018, 51:122
15. Park, S.-J.; Carbon Fibers, Springer Nature Singapore Pte Ltd., 2018, 2. Auflage 16. Goldfeld, Y.; Quadflieg, T.; Ben-Aarosh, S.; Gries, T.:Mircro and Macro Crack Sensong in TRC Beam under Cyclic Loading Journal of mechanics of Materials and Structures, 2017
17. Goldfeld, Y., and Perry, G.: Electrical characterization of smart sensory system using carbon based textile reinforced concrete for leakage detection, Materials and Structures, 2018, Volume 51, No. 17, pp 1-17
18. Goldfeld, Y. and Perry g.: A-R Glass/Carbon-Based Textile Reinforced Concrete Elements for Detection Water Infiltration within Cracked Zones, Structural Health Monitoring, 2019, doi: 10.1177/1475921918808223
19. Goldfeld, Y.; Quadflieg, T.; Gries, T.; Rabinovitch, O.: Smart textile reinforcement with embedded stainless steel yarns for the detection of wetting and infiltration in TRC structures Sensors and Actuators, A 234, 2016, pp 139 – 150
20. DIN EN 1170-5: Prüfverfahren für Glasfaserbeton, Teil 5: Bestimmung der Biegezugfestigkeit, Vollständige Biegezugprüfung, Deutsche Fassung EN 1170-5: 1997
21. Perry, G., Goldfeld, Y., Dittel, G., Gries, T.: Mutual Effect of Textile Binding and Coating on the Structural Performance of TRC Beams, Volume 32, Issue 8 - August 2020, Journal of Materials in Civil Engineering, 2020, 32(8): 04020232 doi: 10.1061/(ASCE)MT.1943-5533.0003331
22. DIN1916: Rohre und Formstücke aus Beton, Stahlfaserbeton und Stahlbeton ; Deutsche Fassung EN 1916:2002; April 2003
23. Lorenz, E., Ortlepp, R.: Effizienzsteigerung von Textilbeton durch Einsatz textile Bewehrungen nach dem erweiterten Nähwirkverfahren, Beton- und Stahlbetonbau, 106 (1): 21-30, January 2011
24. Dittel, G., Wangler, M., Maiworm, B., Gries, T. (in press): Experimental Investigation of Mechanical Properties of Smart Textile Reinforced Concrete Pipes, Proceedings of the RILEM-fib X International Symposium on Fibre Reinforced Concrete BEFIB2020