Composite Reinforcing Bars for Future Infrastructure

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Composite Reinforcing Bars for Future Infrastructure

Author(s): Ginger Gardiner

Publication: Concrete International

Volume: 43

Issue: 2

Appears on pages(s): 23-26

Keywords: pultrusion, project, technology, channel

DOI: 10.14359/51731554

Date: 2/1/2021

Abstract:
A 23 km (14 mile) long and up to 80 m (262 ft) wide flood mitigation channel in Jizan, Saudi Arabia, is the largest glass fiber-reinforced polymer (GFRP) reinforcing bar project in the world. GFRP bar manufacturer Mateenbar, based in Dubai, United Arab Emirates (UAE), was awarded 50% of the contract. The factory produced almost 6000 km (3730 miles) of GFRP reinforcing bars over 7 months.