Effect of Axial Load and Web Reinforcement Ratio on Seismic Behavior of Glass Fiber-Reinforced Polymer-Reinforced Concrete Squat Walls

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Axial Load and Web Reinforcement Ratio on Seismic Behavior of Glass Fiber-Reinforced Polymer-Reinforced Concrete Squat Walls

Author(s): Islam Shabana, Ahmed Sabry Farghaly, and Brahim Benmokrane

Publication: Structural Journal

Volume: 118

Issue: 4

Appears on pages(s): 109-121

Keywords: deformability; drift; energy dissipation; fiber-reinforced polymer (FRP) bar; hysteretic response; reinforced concrete; seismic; squat wal

DOI: 10.14359/51730540

Date: 7/1/2021

Abstract:
A laboratory test program was undertaken to characterize the seismic performance of concrete squat walls entirely reinforced with glass fiber-reinforced polymer (GFRP) bars. Four large-scale specimens were constructed and tested under the combined action of constant axial and quasi-static lateral reversed cyclic loads. The specimens were 150 mm (6 in.) in thickness, 1400 mm (55 in.) in length, and 1600 mm (63 in.) in height, with a corresponding aspect ratio of 1.14. The primary test variables were the axial load ratio (ALR) and web reinforcement ratio (horizontal and vertical). The test results were analyzed in terms of cracking behavior, failure mechanisms, hysteretic response, and web and boundary reinforcement strains. The effect of the test variables on the lateral load and drift capacity, energy dissipation, and deformability aspects were carefully examined. Overall, the ALR impacted neither the lateral load and drift capacity nor the energy dissipated by a specimen prior to failure. The web reinforcement, on the other hand, had a direct impact on the lateral load and drift capacity as well as on the wall deformability and energy dissipation characteristics.

Related References:

ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

ACI Committee 349, “Code Requirements for Nuclear Safety-Related Concrete Structures (ACI 349-13) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2013, 196 pp.

ACI Committee 440, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 2015, 88 pp.

Arafa, A.; Farghaly, A. S.; and Benmokrane, B., 2018a, “Effect of Web Reinforcement on the Seismic Response of Concrete Squat Walls Reinforced with Glass-FRP Bars,” Engineering Structures, V. 174, Nov., pp. 712-723. doi: 10.1016/j.engstruct.2018.07.092

Arafa, A.; Farghaly, A. S.; and Benmokrane, B., 2018b, “Experimental Behavior of GFRP-Reinforced Concrete Squat Walls Subjected to Simulated Earthquake Load,” Journal of Composites for Construction, ASCE, V. 22, No. 2, p. 04018003. doi: 10.1061/(ASCE)CC.1943-5614.0000836

Baek, J. W.; Park, H. G.; Lee, J. H.; and Bang, C. J., 2017, “Cyclic Loading Test for Walls of Aspect Ratio 1.0 and 0.5 with Grade 550 MPa (80 ksi) Shear Reinforcing Bars,” ACI Structural Journal, V. 114, No. 4, July-Aug., pp. 969-982. doi: 10.14359/51689680

Bimschas, M., and Dazio, A., 2008, “Large Scale Quasi-Static Cyclic Tests of Existing Bridge Piers,” Proceedings, Fourteenth World Conference on Earthquake Engineering, Beijing, China.

CAN/CSA A23.3, 2014, “Design of Concrete Structures,” CSA Group, Mississauga, ON, Canada, 297 pp.

CAN/CSA S806, 2012, “Design and Construction of Building Components with Fibre-Reinforced Polymers,” CSA Group, Mississauga, ON, Canada, 208 pp.

CAN/CSA S807, 2019, “Specification for Fibre-Reinforced Polymers,” CSA Group, Mississauga, ON, Canada, 48 pp.

El-Gendy, M. G., and El-Salakawy, E. F., 2020, “GFRP Shear Reinforcement for Slab-Column Edge Connections Subjected to Reversed Cyclic Lateral Load,” Journal of Composites for Construction, ASCE, V. 24, No. 2, p. 04020003. doi: 10.1061/(ASCE)CC.1943-5614.0001000

Eladawy, M.; Hassan, M.; and Benmokrane, B., 2019, “Experimental Study of Interior Glass Fiber-Reinforced Polymer-Reinforced Concrete Slab-Column Connections under Lateral Cyclic Load,” ACI Structural Journal, V. 116, No. 6, Nov., pp. 165-180. doi: 10.14359/51716803

Elshamandy, M. G.; Farghaly, A. S.; and Benmokrane, B., 2018, “Experimental Behavior of Glass Fiber-Reinforced Polymer- Reinforced Concrete Columns under Lateral Cyclic Load,” ACI Structural Journal, V. 115, No. 2, Mar., pp. 337-349. doi: 10.14359/51700985

FEMA 461, 2007, “Interim Testing Protocols for Determining the Seismic Performance Characteristics of Structural and Nonstructural Components,” Federal Emergency Management Agency, Washington, DC, 113 pp.

Gulec, C. K., and Whittaker, A. S., 2009, “Performance-Based Assessment and Design of Squat Reinforced Concrete Shear Walls,” Report No. MCEER-09-0010, University at Buffalo, Buffalo, NY, 664 pp.

Kappos, A., and Penelis, G. G., 2014, Earthquake Resistant Concrete Structures, CRC Press, Oxfordshire, UK, 585 pp.

Luna, B. N.; Rivera, J. P.; and Whittaker, A. S., 2015, “Seismic Behavior of Low-Aspect-Ratio Reinforced Concrete Shear Walls,” ACI Structural Journal, V. 112, No. 5, Sept.-Oct., pp. 593-604. doi: 10.14359/51687709

Moehle, J. P., Seismic Design of Reinforced Concrete Buildings, McGraw Hill Professional, New York, 2014, 782 pp.

Mohamed, N.; Farghaly, A. S.; Benmokrane, B.; and Neale, K. W., 2014a, “Experimental Investigation of Concrete Shear Walls Reinforced with Glass Fiber-Reinforced Bars under Lateral Cyclic Loading,” Journal of Composites for Construction, ASCE, V. 18, No. 3, p. 04014001. doi: 10.1061/(ASCE)CC.1943-5614.0000393

Mohamed, N.; Farghaly, A. S.; Benmokrane, B.; and Neale, K. W., 2014b, “Flexure and Shear Deformation of GFRP-Reinforced Shear Walls,” Journal of Composites for Construction, ASCE, V. 18, No. 2, p. 04013044. doi: 10.1061/(ASCE)CC.1943-5614.0000444

Mun, J. H.; Yang, K. H.; and Song, J. K., 2017, “Shear Behavior of Squat Heavyweight Concrete Shear Walls with Construction Joints,” ACI Structural Journal, V. 114, No. 4, July-Aug., pp. 1019-1029. doi: 10.14359/51689785

Paulay, T.; Priestley, M. J. N.; and Synge, A. J., 1982, “Ductility in Earthquake Resisting Squat Shearwalls,” ACI Journal Proceedings, V. 79, No. 4, Apr., pp. 257-269.

Paulay, T., and Priestley, M. J. N., 1992, Seismic Design of Reinforced Concrete and Masonry Buildings, John Wiley & Sons, Inc., New York, July-Aug., 735 pp.

Pultrall, Inc., 2018, “Data Sheet—V-ROD GFRP Rebars,” Pultrall, Thetford Mines, QC, Canada.

Tomăzevič, M., 1999, Earthquake-Resistant Design of Masonry Buildings: Seismic Resistance Verification of Structural Walls, Imperial College Press, London, UK, pp. 127-141.

Whyte, C. A., and Stojadinovic, B., 2014, “Effect of Ground Motion Sequence on Response of Squat Reinforced Concrete Shear Walls,” Journal of Structural Engineering, ASCE, V. 140, No. 8, p. A4014004. doi: 10.1061/(ASCE)ST.1943-541X.0000912