Torsion of Carbon Fiber-Reinforced Polymer-Strengthened Inverted T-Beams under Combined Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Torsion of Carbon Fiber-Reinforced Polymer-Strengthened Inverted T-Beams under Combined Loading

Author(s): Yail J. Kim and Abdulalziz Alqurashi

Publication: Structural Journal

Volume: 119

Issue: 1

Appears on pages(s): 27-40

Keywords: carbon fiber-reinforced polymer (CFRP); rehabilitation; strengthening; torsion

DOI: 10.14359/51730532

Date: 1/1/2022

Abstract:
This paper presents the torsional behavior of inverted T-beams strengthened with carbon fiber-reinforced polymer (CFRP) sheets when simultaneously subjected to shear- and flexure-combined loading. Two types of CFRP bonding are tested: complete wrapping and side-bonding with single and double layers at variable coverage areas. The capacity of the beams with completely wrapped sheets is higher than that of the beams with side-bonded sheets, whereas such a tendency diminishes as the intensity of the combined loading increases. Moreover, the torsional stress of the test beams is in part relieved by the interaction with the flexural component. For the side-bonded beams, the cross-sectional area of the CFRP controls the load-carrying capacity. While the completely wrapped sheets enhance the ductility of the beams, the wide side-coverage of the CFRP benefits their polar moment of inertia that is concerned with the torsional rigidity and rotations. The degree of stress redistribution under the combined loading is not as significant as the case under pure torsion. Crack localization leads to the failure of the beams subjected to pure torsion, accompanied by partial delamination of the side-bonded sheets; however, torsional cracks spread over the loading span with the presence of shear and bending. The loading scheme affects the magnitude of the effective strain in the CFRP, and the applicability of existing equations is assessed. Based on the proposed effective confinement index, the influence of CFRP layers on the shear-flow path of the concrete section is examined. For design recommendations, analytical modeling with uncertainty simulations generates interaction envelopes, which demarcate the safe and unsafe regions of the strengthened beams under the combined loading.

Related References:

1. Alexander, M., and Beushausen, H., “Durability, Service Life Prediction, and Modelling for Reinforced Concrete Structures: Review and Critique,” Cement and Concrete Research, V. 122, Aug. 2019, pp. 17-29. doi: 10.1016/j.cemconres.2019.04.018

2. Ghobarah, A.; Ghorbel, M. N.; and Chidiac, S. E., “Upgrading Torsional Resistance of Reinforced Concrete Beams Using Fiber-Reinforced Polymer,” Journal of Composites for Construction, ASCE, V. 6, No. 4, Nov. 2002, pp. 257-263. doi: 10.1061/(ASCE)1090-0268(2002)6:4(257)

3. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

4. Salom, P. R.; Gergely, J.; and Young, D. T., “Torsional Strengthening of Spandrel Beams with Fiber-Reinforced Polymer Laminates,” Journal of Composites for Construction, ASCE, V. 8, No. 2, Apr. 2004, pp. 157-162. doi: 10.1061/(ASCE)1090-0268(2004)8:2(157)

5. Elsanadedy, H. M.; Abbas, H.; Almusallam, T. H.; and Al-Salloum, Y. A., “Organic Versus Inorganic Matrix Composites for Bond-Critical Strengthening Applications of RC Structures – State-of-the-Art Review,” Composites Part B: Engineering, V. 174, Oct. 2019, p. 106947. doi: 10.1016/j.compositesb.2019.106947

6. ACI Committee 440, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-17),” American Concrete Institute, Farmington Hills, MI, 2017, 112 pp.

7. Ameli, M.; Ronagh, H. R.; and Dux, P. F., “Behavior of FRP Strengthened Reinforced Concrete Beams under Torsion,” Journal of Composites for Construction, ASCE, V. 11, No. 2, Apr. 2007, pp. 192-200. doi: 10.1061/(ASCE)1090-0268(2007)11:2(192)

8. Ma, S.; Bunnori, N. M.; and Choong, K. K., “Behavior of Reinforced Concrete Box Beam Strengthened with CFRP U-Wrap Strips Under Torsion,” MATEC Web of Conferences, V. 47, 2016, 8 pp.

9. Alabdulhady, M. Y., and Sneed, L. H., “Torsional Strengthening of Reinforced Concrete Beams with Externally Bonded Composites: A State of the Art Review,” Construction and Building Materials, V. 205, Apr. 2019, pp. 148-163. doi: 10.1016/j.conbuildmat.2019.01.163

10. Jing, M., and Grünberg, J., “Mechanical Analysis of Reinforced Concrete Box Beam Strengthened with Carbon Fiber Sheets Under Combined Actions,” Composite Structures, V. 73, No. 4, 2006, pp. 488-494. doi: 10.1016/j.compstruct.2005.02.020

11. Deifalla, A., and Ghobarah, A., “Full Torsional Behavior of RC Beams Wrapped with FRP: Analytical Model,” Journal of Composites for Construction, ASCE, V. 14, No. 3, June 2010, pp. 289-300. doi: 10.1061/(ASCE)CC.1943-5614.0000085

12. Hii, A. K. Y., and Al-Mahaidi, R., “Torsional Capacity of CFRP Strengthened Reinforced Concrete Beams,” Journal of Composites for Construction, ASCE, V. 11, No. 1, Feb. 2007, pp. 71-80. doi: 10.1061/(ASCE)1090-0268(2007)11:1(71)

13. Chai, H. K.; Majeed, A. A.; and Allawi, A. A., “Torsional Analysis of Multicell Concrete Girders Strengthened with CFRP Using a Modified Softened Truss Model,” Journal of Bridge Engineering, ASCE, V. 20, No. 8, Aug. 2015, p. B4014001. doi: 10.1061/(ASCE)BE.1943-5592.0000621

14. Mirza, S. A.; Furlong, R. W.; and Ma, J. S., “Flexural Shear and Ledge Reinforcement in Reinforced Concrete Inverted T-Girders,” ACI Structural Journal, V. 85, No. 5, Sept.-Oct. 1988, pp. 509-520.

15. Fédération internationale du béton, “Externally Bonded FRP Reinforcement for RC Structures (fib Bulletin 14),” fib, Lausanne, Switzerland, Oct. 2001, 138 pp.

16. TRB, “Recommended Guide Specifications for the Design of Externally Bonded FRP Systems for Repair and Strengthening of Concrete Bridge Elements,” NCHRP Report 655, Transportation Research Board, Washington, DC, 2010, 106 pp.

17. ASTM C39/C39M-15a, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2015, 7 pp.

18. Chalioris, C. E., “Torsional Strengthening of Rectangular and Flanged Beams Using Carbon Fibre-Reinforced-Polymers – Experimental Study,” Construction and Building Materials, V. 22, No. 1, Jan. 2008, pp. 21-29. doi: 10.1016/j.conbuildmat.2006.09.003

19. Wight, J. K., and MacGregor, J. G., Reinforced Concrete: Mechanics and Design, fifth edition, Prentice Hall, Upper Saddle River, NJ, 2009, 1112 pp.

20. Montgomery, D. C., Design and Analysis of Experiments, eighth edition, John Wiley & Sons, Inc., Hoboken, NJ, 2013, 752 pp.

21. Nawy, E. G., Reinforced Concrete: A Fundamental Approach, sixth edition, Prentice Hall, Upper Saddle River, NJ, 2008, 944 pp.

22. Huang, L.; Lu, Y.; and Shi, C., “Unified Calculation Method for Symmetrically Reinforced Concrete Section Subjected to Combined Loading,” ACI Structural Journal, V. 110, No. 1, Jan.-Feb. 2013, pp. 127-136.

23. Lasdon, L. S.; Fox, R. L.; and Ratner, M. W., “Nonlinear Optimization Using the Generalized Reduced Gradient Method,” Technical Memorandum No. 325, National Technical Information Service, Springfield, VA, 1973, 63 pp.

24. Oldershaw, B., “Combined Effects of Freeze-Thaw and Sustained Loads on Reinforced Concrete Beams Strengthened with FRPs,” MS thesis, Queen’s University, Kingston, ON, Canada, 2008, 134 pp.

25. Lu, R.; Luo, Y.; and Conte, J. P., “Reliability Evaluation of Reinforced Concrete Beams,” Structural Safety, V. 14, No. 4, July 1994, pp. 277-298. doi: 10.1016/0167-4730(94)90016-7

26. Nowak, A. S., and Collins, K. R., Reliability of Structures, second edition, CRC Press, Boca Raton, FL, 2013, 407 pp.

27. Sánchez-Heres, L. F.; Ringsberg, J. W.; and Johnson, E., “Influence of Mechanical and Probabilistic Models on the Reliability Estimates of Fibre-Reinforced Cross-Ply Laminates,” Structural Safety, V. 51, Nov. 2014, pp. 35-46. doi: 10.1016/j.strusafe.2014.06.001

28. Atadero, R. A., and Karbhari, V. M., “Calibration of Resistance Factors for Reliability Based Design of Externally-Bonded FRP Composites,” Composites Part B: Engineering, V. 39, No. 4, June 2008, pp. 665-679. doi: 10.1016/j.compositesb.2007.06.004

29. Okeil, A. M.; El-Tawil, S.; and Shahawy, M., “Flexural Reliability of Reinforced Concrete Bridge Girders Strengthened with Carbon Fiber-Reinforced Polymer Laminates,” Journal of Bridge Engineering, ASCE, V. 7, No. 5, Sept. 2002, pp. 290-299. doi: 10.1061/(ASCE)1084-0702(2002)7:5(290)

30. Mirza, S. A.; Kikuchi, D. K.; and MacGregor, J. G., “Flexural Strength Reduction Factor for Bonded Prestressed Concrete Beams,” ACI Journal Proceedings, V. 77, No. 4, July-Aug. 1980, pp. 237-246.

31. Elwan, S. K., “Torsion Strengthening of RC Beams Using CFRP (Parametric Study),” KSCE Journal of Civil Engineering, V. 21, No. 4, May 2017, pp. 1273-1281. doi: 10.1007/s12205-016-0156-7


ALSO AVAILABLE IN: