Time-Dependent Behavior of Concrete Beams Externally Prestressed with Carbon Fiber-Reinforced Polymer Tendons for 1000 Days

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Time-Dependent Behavior of Concrete Beams Externally Prestressed with Carbon Fiber-Reinforced Polymer Tendons for 1000 Days

Author(s): Weichen Xue and Ting Liu

Publication: Structural Journal

Volume: 118

Issue: 3

Appears on pages(s): 15-26

Keywords: calculation method; carbon fiber-reinforced polymer (CFRP); concrete beams; deflection; finite element analysis; maximum crack width; time-dependent behavior

DOI: 10.14359/51730522

Date: 5/1/2021

Abstract:
This paper presents an experimental program designed to examine the time-dependent behavior of concrete beams externally prestressed with carbon fiber-reinforced polymer (CFRP) tendons under sustained load for 1000 days. The experimental parameters included the type of prestressed tendon (CFRP or steel), type of non-prestressed reinforcement (glass fiber-reinforced polymer [GFRP] or steel), and the cracking situation (cracked or uncracked). The general trend was a high rate of increase in deflections for the early period (~100 days) after applying the sustained load, followed by a more gradual rate of increase in deflections. The ratios of terminal deflection on the 1000th day to initial deflection at the midspan for the externally prestressed concrete (PC) beams with cracked sections ranged from 1.31 to 1.34, whereas the ratio for the uncracked beam was 4.45. The results revealed that the long-term deflection of uncracked PC beams increased more rapidly than those of cracked PC beams, owing to relatively high compressive stress throughout the cross section. Furthermore, a validated step-by-step finite element analysis program was developed. The values calculated by the program corresponded well with the test results. Based on parametric analysis results of 46 beams in conjunction with regression analysis, a revised calculation method for predicting the midspan deflections of externally PC beams was suggested. It was found that the values calculated by the proposed method were in good agreement with the experimental results.

Related References:

1. American Society of Civil Engineers, “2017 Infrastructure Report Card: A Comprehensive Assessment of America’s Infrastructure,” ASCE, Reston, VA, 2017, www.infrastructurereportcard.org.

2. National Association for Corrosion Engineers International, “Cor­rosion Cost and Preventive Strategies in the United States,” Publication No. FHWA-RD-01-156, NACE International, Houston, TX, 2012, http://www.nace.org.

3. Brockmann, C., and Rogenhofer, H., “Bang Na Expressway, Bangkok, Thailand—World’s Longest Bridge and Largest Precasting Operation,” PCI Journal, V. 45, No. 1, 2000, pp. 26-38. doi: 10.15554/pcij.01012000.26.38

4. Manabe, H., “The Ultimate Strength of PC Segmental T-Girders Using an FRP External Prestressing System,” Proceedings, Third Symposium on Fiber Reinforced Plastic Reinforcement for Concrete Structures, Sapporo, Japan, 1997, pp. 791-798.

5. Ander, B., “Reinforced Concrete T-Beams Externally Prestressed with Unbonded Carbon Fiber-Reinforced Polymer Tendons,” ACI Structural Journal, V. 109, No. 4, July-Aug. 2012, pp. 521-530.

6. Saeki, N., “Strengthening of Damaged Concrete Beams by External Prestressing of Aramid Fiber Cable,” Fiber-Reinforced-Plastic Reinforcement for Concrete Structures - International Symposium, SP-138, A. Nanni and C. W. Dolan, eds., American Concrete Institute, Farmington Hills, MI, 1993, pp. 913-932.

7. Nabil, F. G., and George, A. S., “Behavior of Externally Draped CFRP Tendons in Prestressed Concrete Bridges,” PCI Journal, V. 43, No. 5, 1998, pp. 88-101. doi: 10.15554/pcij.09011998.88.101

8. Tan, Y., and Xue, W. C., “Discussion of ‘Flexural Response of Concrete Beams Prestressed with AFRP Tendons: Numerical Investigation’ by Yail J. Kim,” Journal of Composites for Construction, ASCE, V. 16, No. 3, 2012, pp. 354-356. doi: 10.1061/(ASCE)CC.1943-5614.0000247

9. Currier, J.; Dolan, C.; and O’Neil, E., “Deflection Control of Fiber Reinforced Plastic Pretensioned Concrete Beams,” Non-Metallic (FRP) Reinforcement for Concrete Structures, L. Taerwe, ed., RILEM, Paris, 1995, pp. 413-415.

10. PCI Industry Handbook Committee, PCI Design Handbook—Precast and Prestressed Concrete, eighth edition, Precast/Prestressed Concrete Institute, Chicago, IL, 2017, 880 pp.

11. Braimah, A.; Green, M. F.; and Soudki, K. A., “Long-Term Behavior of CFRP Prestressed Concrete Beams,” PCI Journal, V. 48, No. 2, 2003, pp. 98-107. doi: 10.15554/pcij.03012003.98.107

12. Zou, P. X. W., “Long-Term Deflection and Cracking Behavior of Concrete Beams Prestressed with Carbon Fiber-Reinforced Polymer Tendons,” Journal of Composites for Construction, ASCE, V. 7, No. 3, 2003, pp. 187-193. doi: 10.1061/(ASCE)1090-0268(2003)7:3(187)

13. Zou, P. X. W., “Theoretical Study on Short-Term and Long-Term Deflections of Fiber Reinforced Polymer Prestressed Concrete Beams,” Journal of Composites for Construction, ASCE, V. 7, No. 4, 2003, pp. 285-291. doi: 10.1061/(ASCE)1090-0268(2003)7:4(285)

14. Zou, P. X. W., and Shang, S., “Time-Dependent Behaviour of Concrete Beams Pretensioned by Carbon Fibre-Reinforced Polymers (CFRP) Tendons,” Construction and Building Materials, V. 21, No. 4, 2007, pp. 777-788. doi: 10.1016/j.conbuildmat.2006.06.008

15. ACI Committee 440, “Prestressing Concrete Structures with FRP Tendons (ACI 440.4R-04) (Reapproved 2011),” American Concrete Institute, Farmington Hills, MI, 2011, 35 pp.

16. ACI Committee 440, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 2015, 83 pp.

17. Canadian Standards Association, “Design and Construction of Building Structures with Fibre-Reinforced Polymers (CAN/CSA-S806-12),” CSA, Mississauga, ON, Canada, 2012, 187 pp.

18. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

19. China Metallurgical Construction Research Institute, “Technical Code for Infrastructure Application of FRP Composites (GB 50608-2010) (in Chinese),” The National Standards Complication Group of People’s Republic of China, China Architecture & Building Press, Beijing, China, 2010, 183 pp.

20. Scott, D. W., and Zureick, A. H., “Compression Creep of a Pultruded E-Glass/Vinylester Composite,” Composites Science and Technology, V. 58, No. 8, 1998, pp. 1361-1369. doi: 10.1016/S0266-3538(98)00009-8

21. Ahmed, G., “Calculating Ultimate Tendon Stress in Externally Prestressed Continuous Concrete Beams Using Simplified Formulas,” Engineering Structures, V. 46, No. 1, 2013, pp. 417-430.

22. Bažant, Z. P., “Prediction of Concrete Creep Effects Using Age-Adjusted Effective Modulus Method,” ACI Journal Proceedings, V. 69, No. 4, Apr. 1972, pp. 212-217.

23. Xue, W. C.; Ding, M.; He, C.; and Li, J., “Long-Term Behavior of Prestressed Composite Beams at Service Loads for One Year,” Journal of Structural Engineering, ASCE, V. 134, No. 6, 2008, pp. 930-937. doi: 10.1061/(ASCE)0733-9445(2008)134:6(930)

24. Xue, W. C.; Liu, T.; Wang, W.; and Hu, Y. M., “Creep Behavior of High-Speed Railway Prestressed Concrete Girders for 500 Days,” ACI Structural Journal, V. 108, No. 4, July-Aug. 2011, pp. 497-504.

25. European Committee for Standardization, “Eurocode 2: Design of Concrete Structures—Part 1-1: General Rules and Rules for Buildings (EN 1992-1-1:2004),” CEN, Brussels, Belgium, 2004, 225 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal