A Thermodynamics-based Framework Production of Porous Lightweight Aggregate (LWA) from Waste Coal Combustion Ash (W-CCA)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Thermodynamics-based Framework Production of Porous Lightweight Aggregate (LWA) from Waste Coal Combustion Ash (W-CCA)

Author(s): Mohammad Balapour

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/25/2020

Abstract:
Presentations of original, unpublished results from ongoing research projects and leading-edge concrete technology and research throughout the world.