Abstract:
The intent of this paper is to provide an illustrative example of a municipal bridge replacement design project utilizing fiber reinforced polymer materials approved for use by the Florida Department of Transportation. Specifically this paper describes the design of the Nathaniel J. Upham (40th Avenue NE) Bridge replacement project and illustrates the application of carbon fiber reinforced polymer (CFRP) prestressing tendons and glass fiber
reinforced polymer (GFRP) reinforcing bars in both precast and cast-in-place concrete elements. Due to the structure’s high level of exposure in the extremely aggressive environment, the design for the replacement bridge focused on concrete elements that were durable and resilient to the effects of corrosion in those conditions. Prestressed and castin-place concrete elements with GFRP and CFRP reinforcement and prestressing tendons were utilized for the primary structural elements with direct exposure to salt water. In addition, link slabs with GFRP reinforcing were utilized at each intermediate bent to improve the bridge’s performance. The design of the bridge elements followed the Florida Department of Transportation’s design guidelines and requirements. The bridge replacement project is currently at the completion of the design phase and is scheduled to be advertised in the early summer of 2020 with the start of construction anticipated in the fall of 2020.
Related References:
1. FDOT, 2017, Bridge Inspection Report for Bridge No. 157154, Regular NBI, Inspection Date 7/31/2017, Florida Department of Transportation, Tallahassee, FL.
2. Yam, J. and Gamache, C., 2018, Bridge improvements at 40th Ave NE over Placido Bayou Bridge No. 157154, Construction Plans, Engineering & Capital Improvements Department, City of St. Petersburg, FL.
3. FDOT, 2020, Structures Manual, Florida Department of Transportation, Tallahassee, FL.
4. AASHTO, 2017, AASHTO LRFD Bridge Design Specifications, 8th Edition, American Association of State Highway Transportation Officials, Washington, DC.
5. FDOT, 2020, Fiber Reinforced Polymer Guidelines, Florida Department of Transportation, Tallahassee, FL.
6. FDOT, 2020, Structures Design Guidelines, Florida Department of Transportation, Tallahassee, FL.
7. FDOT, 2020, Square CFRP & SS Prestressed Concrete Piles - Typical Details & Notes, FY 2020-21 Standard Plans, Index 455-101, Florida Department of Transportation, Tallahassee, FL.
8. FDOT, 2020, 24” Square CFRP & SS Prestressed Concrete Piles, FY 2020-21 Standard Plans, Index 455-124, Florida Department of Transportation, Tallahassee, FL.
9. AASHTO, 2008, Guide Specifications for Bridges Vulnerable to Coastal Storms, 1st Edition, American Association of State Highway Transportation Officials, Washington, DC.
10. FDOT, 2020, Index 455-101 Series Square CFRP & SS Prestressed Concrete Piles, FY 2020-21 Standard Plans Instructions, Index 455-101, Florida Department of Transportation, Tallahassee, FL.
11. ASCE, 2010, Pre-Standard for Load & Resistance Factor Design (LRFD) of Pultruded Fiber Reinforced Polymer (FRP) Structures, American Society of Civil Engineers, Reston, VA.
12. AASHTO, 2018, AASHTO LRFD Bridge Design Guide Specifications for GFRP-Reinforced Concrete, 2nd Edition, American Association of State Highway Transportation Officials, Washington, DC.
13. FDOT, 2020, Standard Specifications for Road and Bridge Construction, January 2020, Florida Department of Transportation, Tallahassee, FL.
14. FDOT, 2017, Pultruded FRP Bar Bending Details, Developmental Design Standards, Index D21310, Florida Department of Transportation, Tallahassee, FL.
15. AASHTO, 2018, Guide Specifications for Bridges for the Design of Concrete Bridge Beams Prestressed with CFRP Systems, 1st Edition, American Association of State Highway Transportation Officials, Washington, DC.
16. ACI Committee 440, 2004, Prestressing Concrete Structures with FRP Tendons, ACI 440.4R-04, American Concrete Institute, Farmington Hills, MI.
17. FDOT, 2016, Typical Florida Slab Beam Details and Notes, Developmental Design Standards, Index D20450, Florida Department of Transportation, Tallahassee, FL.
18. FDOT, 2016, 18” Florida Slab Beam, Developmental Design Standards, Index D20450, Florida Department of Transportation, Tallahassee, FL.
19. FDOT, 2016, Index D20450 Series Florida Slab Beams, Instructions for Developmental Design Standards, Index D20450, Florida Department of Transportation, Tallahassee, FL.