Proposed Slenderness Limit for GFRP-RC Columns Based on Experiments and Buckling Analysis

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Slenderness Limit for GFRP-RC Columns Based on Experiments and Buckling Analysis

Author(s): Waseem Abdelazim

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/29/2020

Abstract:
To develop design provisions for concrete columns reinforced with fiber-reinforced polymer (FRP) bar for North American codes and guidelines (ACI 440.1R, CSA S806), a slenderness limit below which it is acceptable to ignore the induced second-order effects must be determined. Nevertheless, limited attempts have been made to define a safe slenderness limit for such columns. Therefore, this study aimed at experimentally and analytically investigating the buckling behavior of 12 full-scale concrete columns reinforced with glass FRP (GFRP) with slenderness ratios of 14, 17, 23, 26, and 33 under concentric loading. The impact of longitudinal reinforcement ratios and confining levels on the performance of slender GFRP-reinforced concrete (GFRP-RC) columns is also presented. Test results indicate that the GFRP reinforcement contributed significantly to resisting the applied compression loads and resulted in failure modes similar to that of the counterpart steel-reinforced concrete columns at different slenderness ratios. In addition, a theoretical buckling analysis considering a total of 50 test specimens, assembled from the current study and the literature, was developed to verify the applicability of Euler-Johnson’s stability envelope as well as the reduced and incremental modulus theories to FRP-RC columns. Good correlation was observed between the experimental results and the models developed analytically. Based on the experimental data and the developed buckling analysis, the safe limit of the slenderness ratio for FRP-RC columns bent in single curvature of 18 is proposed.