Use of Higher‑Harmonic and Intermodulation Generation of Ultrasonic Waves to Detecting Cracks due to Steel Corrosion in Reinforced Cement Mortar

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use of Higher‑Harmonic and Intermodulation Generation of Ultrasonic Waves to Detecting Cracks due to Steel Corrosion in Reinforced Cement Mortar

Author(s): Miguel Ángel Climent‑Llorca, Marina Miró‑Oca, Pedro Poveda‑Martínez and Jaime Ramis‑Soriano

Publication: IJCSM

Volume: 14

Issue:

Appears on pages(s):

Keywords: reinforced concrete, steel corrosion, cracking, non‑linear ultrasonic test, non‑destructive detection

DOI: 10.1186/s40069-020-00432-x

Date: 11/30/2020

Abstract:
The aim of this work was to provide further confirmation of the possible use of non‑linear ultrasonic techniques for detecting the cracking due to corrosion of steel reinforcements in concrete. To this end accelerated steel corrosion tests have been conducted on model reinforced cement mortar specimens, while monitoring the appearance and width evolution of visible surface cracks, and performing non‑linear ultrasonic measurements based on the phenom‑ ena of harmonic distortion and intermodulation. A new parameter, based on the difference between the amplitude of the fundamental frequency and the sum of the amplitudes of all the first‑order and second‑order intermodulation products, has been proposed in this work. The results confirm that the appearance of visible surface micro‑cracks are preceded and accompanied by the observation of strong non‑linear features in the received signal. Furthermore, the new parameter proposed in this work is as efficient as the relative non‑linearity parameters, classically used in har‑ monic distortion non‑linear ultrasonic studies, for detecting the non‑linear features associated with the critical events of the cracking of cement mortar due to embedded steel corrosion. A hypothesis has been developed considering the possible effect of the filling of the void space by liquid containing rust products after the formation of new cracks or the enlargement of its width. This filling process, which might be particularly enhanced by net convective transport of liquid, would explain the evolution of the values of all the parameters used for putting in evidence the non‑linear elastic features after the critical events of the cracking process.