Shrinkage-Reducing Admixture Effect on Rubberized Cement Performance

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shrinkage-Reducing Admixture Effect on Rubberized Cement Performance

Author(s): Robbie M. Damiani, Paramita Mondal, and David A. Lange

Publication: Materials Journal

Volume: 118

Issue: 3

Appears on pages(s): 101-116

Keywords: dynamic properties; Fourier transform infrared spectroscopy; mechanical properties; rubberized cement; shrinkage-reducing admixture; waste rubber

DOI: 10.14359/51730424

Date: 5/1/2021

Abstract:
Within the last decade, interest in using waste rubber in concrete has been increasing due to sustainability concerns. However, previous work has shown a surface mismatch between rubber and paste, leading to diminished performance. The objective of this work is to determine the efficacy of shrinkage-reducing admixture (SRA) on the performance of rubberized cement samples; beyond reducing shrinkage, the use of SRA is believed to improve the adhesive bond at the interface. From initial testing, another effect was observed: adsorption of SRA on the rubber surface. Various mechanical tests and characterization techniques were implemented to understand the efficacy of these modifications. Results concluded that SRA implementation within the bulk mixture or as a pre-treatment lowered rubber contact angle, which subsequently improved compressive and pullout strength, as well as damping ratio of rubberized cement samples. By pretreating rubber, limitations associated with using SRA in the mixture design may be bypassed.

Related References:

1. Eldin, N. N., and Senouci, A. B., “Rubber‐Tire Particles as Concrete Aggregate,” Journal of Materials in Civil Engineering, ASCE, V. 5, No. 4, 1993, pp. 478-496. doi: 10.1061/(ASCE)0899-1561(1993)5:4(478)

2. Blackman, A., and Palma, A., “Scrap Tires in Ciudad Juárez and El Paso: Ranking the Risks,” Journal of Environment & Development, V. 11, No. 3, 2002, pp. 247-266. doi: 10.1177/107049602237157

3. Joy, J. E.; Hanna, A. A.; and Kennedy, B. A., “Spatial and Temporal Variation in the Mosquitoes (Diptera: Culicidae) Inhabiting Waste Tires in Nicholas County, West Virginia,” Journal of Medical Entomology, V. 40, No. 1, 2003, pp. 73-77. doi: 10.1603/0022-2585-40.1.73

4. Kim, C.-H.; Lampman, R. L.; and Muturi, E. J., “Bacterial Communities and Midgut Microbiota Associated with Mosquito Populations from Waste Tires in East-Central Illinois,” Journal of Medical Entomology, V. 52, No. 1, 2015, pp. 63-75. doi: 10.1093/jme/tju011

5. Paine, K. A., and Dhir, R. K., “Research on New Applications for Granulated Rubber in Concrete,” Proceedings of the Institution of Civil Engineers - Construction Materials, V. 163, No. 1, 2010, pp. 7-17.

6. Leung, C. K., and Grasley, Z. C., “Effect of Micrometric and Nanometric Viscoelastic Inclusions on Mechanical Damping Behavior of Cementitious Composites,” Construction and Building Materials, V. 35, 2012, pp. 444-451. doi: 10.1016/j.conbuildmat.2012.04.021

7. Kaloush, K. E.; Way, G. B.; and Zhu, H., “Properties of Crumb Rubber Concrete,” Transportation Research Record: Journal of the Transportation Research Board, V. 1914, No. 1, 2005, pp. 8-14. doi: 10.1177/0361198105191400102

8. Ismail, M. K., and Hassan, A. A. A., “Impact Resistance and Acoustic Absorption Capacity of Self-Consolidating Rubberized Concrete,” ACI Materials Journal, V. 113, No. 6, Nov.-Dec. 2016, pp. 725-736. doi: 10.14359/51689359

9. Gupta, T.; Sharma, R. K.; and Chaudhary, S., “Impact Resistance of Concrete Containing Waste Rubber Fiber and Silica Fume,” International Journal of Impact Engineering, V. 83, 2015, pp. 76-87. doi: 10.1016/j.ijimpeng.2015.05.002

10. Fattuhi, N. I., and Clark, L. A., “Cement-Based Materials Containing Shredded Scrap Truck Tyre Rubber,” Construction and Building Materials, V. 10, No. 4, 1996, pp. 229-236. doi: 10.1016/0950-0618(96)00004-9

11. Nehdi, M., and Khan, A., “Cementitious Composites Containing Recycled Tire Rubber: An Overview of Engineering Properties and Potential Applications,” Cement, Concrete and Aggregates, V. 23, No. 1, 2001, p. 3. doi: 10.1520/CCA10519J

12. Ghaly, A. M., and Cahill, J. D., IV, “Correlation of Strength, Rubber Content, and Water to Cement Ratio in Rubberized Concrete,” Canadian Journal of Civil Engineering, V. 32, No. 6, 2005, pp. 1075-1081. doi: 10.1139/l05-063

13. Paine, K. A.; Dhir, R. K.; Moroney, R.; and Kopasakis, K., “Use of Crumb Rubber to Achieve Freeze Thaw Resisting Concrete,” Proceedings of the International Conference on Concrete for Extreme Conditions, University of Dundee, Dundee, UK, 2002. pp. 486-498.

14. Chou, L. H.; Lu, C.-K.; Chang, J.-R.; and Lee, M. T., “Use of Waste Rubber as Concrete Additive,” Waste Management & Research, V. 25, No. 1, 2007, pp. 68-76. doi: 10.1177/0734242X07067448

15. Mohammed, B. S.; Anwar Hossain, K. M.; Eng Swee, J. T.; Wong, G.; and Abdullahi, M., “Properties of Crumb Rubber Hollow Concrete Block,” Journal of Cleaner Production, V. 23, No. 1, 2012, pp. 57-67. doi: 10.1016/j.jclepro.2011.10.035

16. Najim, K. B., and Hall, M. R., “A Review of the Fresh/Hardened Properties and Applications for Plain- (PRC) and Self-Compacting Rubberised Concrete (SCRC),” Construction and Building Materials, V. 24, No. 11, 2010, pp. 2043-2051. doi: 10.1016/j.conbuildmat.2010.04.056

17. Youssf, O., and ElGawady, M., “An Overview of Sustainable Concrete Made with Scrap Rubber,” From Materials to Structures: Advancement through Innovation, CRC Press, Boca Raton, FL, 2012, pp. 1039-1044.

18. Bala, A.; Sehgal, V. K.; and Saini, B., “Effect of Fly ash and Waste Rubber on Properties of Concrete Composite,” Concrete Research Letters, V. 5, No. 3, 2014, pp. 842-857.

19. Güneyisi, E., “Fresh Properties of Self-Compacting Rubberized Concrete Incorporated with Fly Ash,” Materials and Structures, V. 43, No. 8, 2010, pp. 1037-1048. doi: 10.1617/s11527-009-9564-1

20. Gesoğlu, M., and Özbay, E., “Effects of Mineral Admixtures on Fresh and Hardened Properties of Self-Compacting Concretes: Binary, Ternary and Quaternary Systems,” Materials and Structures, V. 40, No. 9, 2007, pp. 923-937. doi: 10.1617/s11527-007-9242-0

21. Güneyisi, E.; Gesoğlu, M.; and Özturan, T., “Properties of Rubberized Concretes Containing Silica Fume,” Cement and Concrete Research, V. 34, No. 12, 2004, pp. 2309-2317. doi: 10.1016/j.cemconres.2004.04.005

22. Elchalakani, M., “High Strength Rubberized Concrete Containing Silica Fume for the Construction of Sustainable Road Side Barriers,” Structures, V. 1, 2015, pp. 20-38. doi: 10.1016/j.istruc.2014.06.001

23. Gupta, T.; Chaudhary, S.; and Sharma, R. K., “Mechanical and Durability Properties of Waste Rubber Fiber Concrete with and without Silica Fume,” Journal of Cleaner Production, V. 112, 2016, pp. 702-711. doi: 10.1016/j.jclepro.2015.07.081

24. Gesoğlu, M., and Güneyisi, E., “Strength Development and Chloride Penetration in Rubberized Concretes with and without Silica Fume,” Materials and Structures, V. 40, No. 9, 2007, pp. 953-964. doi: 10.1617/s11527-007-9279-0

25. Segre, N., and Joekes, I., “Use of Tire Rubber Particles as Addition to Cement Paste,” Cement and Concrete Research, V. 30, No. 9, 2000, pp. 1421-1425. doi: 10.1016/S0008-8846(00)00373-2

26. Mohammadi, I.; Khabbaz, H.; and Vessalas, K., “Enhancing Mechanical Performance of Rubberised Concrete Pavements with Sodium Hydroxide Treatment,” Materials and Structures, V. 49, No. 3, 2016, pp. 813-827. doi: 10.1617/s11527-015-0540-7

27. Rostami, H., “Use of recycled Rubber Tires in Concrete,” Proceedings of the International Conference on Concrete, 2000, pp. 391-399.

28. Najim, K. B., and Hall, M. R., “Crumb Rubber Aggregate Coatings/Pre-Treatments and their Effects on Interfacial Bonding, Air Entrapment and Fracture Toughness in Self-Compacting Rubberised Concrete (SCRC),” Materials and Structures, V. 46, No. 12, 2013, pp. 2029-2043. doi: 10.1617/s11527-013-0034-4

29. Mohammadi, I.; Khabbaz, H.; and Vessalas, K., “In-Depth Assessment of Crumb Rubber Concrete (CRC) Prepared by Water-Soaking Treatment Method for Rigid Pavements,” Construction and Building Materials, V. 71, 2014, pp. 456-471. doi: 10.1016/j.conbuildmat.2014.08.085

30. Tantala, M. W.; Lepore, J. A.; and Zandi, I., “Quasi-Elastic Behavior of Rubber Included Concrete (RIC) Using Waste Rubber Tires,” Proceedings of the International Conference on Solid Waste Technology and Management, 1996, p. 8.

31. Smith, D. M., and Chughtai, A. R., “The Surface Structure and Reactivity of Black Carbon,” Colloids and Surfaces. A, Physicochemical and Engineering Aspects, V. 105, No. 1, 1995, pp. 47-77. doi: 10.1016/0927-7757(95)03337-1

32. Bandyopadhyay, S.; De, P. P.; Tripathy, D. K.; and De, S. K., “Influence of Surface Oxidation of Carbon Black on its Interaction with Nitrile Rubbers,” Polymer, V. 37, No. 2, 1996, pp. 353-357. doi: 10.1016/0032-3861(96)81110-4

33. Gagnon, D. R., and McCarthy, T. J., “Polymer Surface Reconstruction by Diffusion of Organic Functional Groups from and to the Surface,” Journal of Applied Polymer Science, V. 29, No. 12, 1984, pp. 4335-4340. doi: 10.1002/app.1984.070291262

34. Siddique, R., and Naik, T. R., “Properties of Concrete Containing Scrap-Tire Rubber – An Overview,” Waste Management (New York, N.Y.), V. 24, No. 6, 2004, pp. 563-569. doi: 10.1016/j.wasman.2004.01.006

35. Turatsinze, A.; Granju, J.-L.; and Bonnet, S., “Positive Synergy between Steel-Fibres and Rubber Aggregates: Effect on the Resistance of Cement-Based Mortars to Shrinkage Cracking,” Cement and Concrete Research, V. 36, No. 9, 2006, pp. 1692-1697. doi: 10.1016/j.cemconres.2006.02.019

36. Li, G.; Stubblefield, M. A.; Garrick, G.; Eggers, J.; Abadie, C.; and Huang, B., “Development of Waste Tire Modified Concrete,” Cement and Concrete Research, V. 34, No. 12, 2004, pp. 2283-2289. doi: 10.1016/j.cemconres.2004.04.013

37. Segre, N.; Monteiro, P. J. M.; and Sposito, G., “Surface Characterization of Recycled Tire Rubber to Be Used in Cement Paste Matrix,” Journal of Colloid and Interface Science, V. 248, No. 2, 2002, pp. 521-523. doi: 10.1006/jcis.2002.8217

38. Huang, B.; Shu, X.; and Cao, J., “A Two-Staged Surface Treatment to Improve Properties of Rubber Modified Cement Composites,” Construction and Building Materials, V. 40, 2013, pp. 270-274. doi: 10.1016/j.conbuildmat.2012.11.014

39. Dong, Q.; Huang, B.; and Shu, X., “Rubber Modified Concrete Improved by Chemically Active Coating and Silane Coupling Agent,” Construction and Building Materials, V. 48, 2013, pp. 116-123. doi: 10.1016/j.conbuildmat.2013.06.072

40. Xi, Y.; Li, Y.; Xie, Z.; and Lee, J. S., “Utilization of Solid Wastes (Waste Glass and Rubber Particles) as Aggregates in Concrete,” International Workshop on Sustainable Development and Concrete Technology, Beijing, China, 2004, pp. 45-52.

41. Yue, L.; Qianqian, Y.; Xi, Y.; et al. “Study on Properties of Premixed Rubber Aggregate Thermal Insulation,” New Building Materials Journal, V. 7, 2008, pp. 16-27.

42. Collepardi, M.; Borsoi, A.; Collepardi, S.; Ogoumah Olagot, J. J.; and Troli, R., “Effects of Shrinkage Reducing Admixture in Shrinkage Compensating Concrete under Non-Wet Curing Conditions,” Cement and Concrete Composites, V. 27, No. 6, 2005, pp. 704-708. doi: 10.1016/j.cemconcomp.2004.09.020

43. Bentz, D. P.; Geiker, M. R.; and Hansen, K. K., “Shrinkage-Reducing Admixtures and Early-Age Desiccation in Cement Pastes and Mortars,” Cement and Concrete Research, V. 31, No. 7, 2001, pp. 1075-1085. doi: 10.1016/S0008-8846(01)00519-1

44. He, L.; Ma, Y.; Liu, Q.; and Mu, Y., “Surface Modification of Crumb Rubber and its Influence on the Mechanical Properties of Rubber-Cement Concrete,” Construction and Building Materials, V. 120, 2016, pp. 403-407. doi: 10.1016/j.conbuildmat.2016.05.025

45. Rongbing, B., and Jian, S., “Synthesis and Evaluation of Shrinkage-Reducing Admixture for Cementitious Materials,” Cement and Concrete Research, V. 35, No. 3, 2005, pp. 445-448. doi: 10.1016/j.cemconres.2004.07.009

46. Meshgin, P.; Xi, Y.; and Li, Y., “Utilization of Phase Change Materials and Rubber Particles to Improve Thermal and Mechanical Properties of Mortar,” Construction and Building Materials, V. 28, No. 1, 2012, pp. 713-721. doi: 10.1016/j.conbuildmat.2011.10.039

47. Gheni, A. A.; ElGawady, M. A.; and Myers, J. J., “Mechanical Characterization of Concrete Masonry Units Manufactured with Crumb Rubber Aggregate,” ACI Materials Journal, V. 114, No. 1, Jan.-Feb. 2017, pp. 65-76. doi: 10.14359/51689482

48. Sgobba, S.; Carlo Marano, G.; Borsa, M.; and Molfetta, M., “Use of Rubber Particles from Recycled Tires as Concrete Aggregate for Engineering Applications,” The University of Wisconsin Milwaukee Centre for By-products Utilization, Second International Conference on Sustainable Construction Materials and Technologies, Milwaukee, WI, 2010.

49. Ghavibazoo, A., and Abdelrahman, M., “Composition Analysis of Crumb Rubber During Interaction with Asphalt and Effect on Properties of Binder,” The International Journal of Pavement Engineering, V. 14, No. 5, 2013, pp. 517-530. doi: 10.1080/10298436.2012.721548

50. Rajabipour, F.; Sant, G.; and Weiss, J., “Interactions between Shrinkage Reducing Admixtures (SRA) and Cement Paste’s Pore Solution,” Cement and Concrete Research, V. 38, No. 5, 2008, pp. 606-615. doi: 10.1016/j.cemconres.2007.12.005

51. Bentz, D. P., “Influence of Shrinkage-Reducing Admixtures on Early-Age Properties of Cement Pastes,” Journal of Advanced Concrete Technology, V. 4, No. 3, 2006, pp. 423-429. doi: 10.3151/jact.4.423

52. Brooks, J. J.; Megat Johari, M. A.; and Mazloom, M., “Effect of Admixtures on the Setting Times of High-Strength Concrete,” Cement and Concrete Composites, V. 22, No. 4, 2000, pp. 293-301. doi: 10.1016/S0958-9465(00)00025-1

53. Eisenberg, D., and Kauzmann, W., The Structure and Properties of Water, Oxford University Press, Oxford, UK, 2005.

54. Palacios, M., and Puertas, F., “Effect of Superplasticizer and Shrinkage-Reducing Admixtures on Alkali-Activated Slag Pastes and Mortars,” Cement and Concrete Research, V. 35, No. 7, 2005, pp. 1358-1367. doi: 10.1016/j.cemconres.2004.10.014

55. Colom, X.; Faliq, A.; Formela, K.; and Cañavate, J., “FTIR Spectroscopic and Thermogravimetric Characterization of Ground Tyre Rubber Devulcanized by Microwave Treatment,” Polymer Testing, V. 52, 2016, pp. 200-208. doi: 10.1016/j.polymertesting.2016.04.020

56. Aoudia, K.; Azem, S.; Aït Hocine, N.; Gratton, M.; Pettarin, V.; and Seghar, S., “Recycling of Waste Tire Rubber: Microwave Devulcanization and Incorporation in a Thermoset Resin,” Waste Management (New York, N.Y.), V. 60, 2017, pp. 471-481. doi: 10.1016/j.wasman.2016.10.051

57. Hirayama, D., and Saron, C., “Chemical Modifications in Styrene–Butadiene Rubber after Microwave Devulcanization,” Industrial & Engineering Chemistry Research, V. 51, No. 10, 2012, pp. 3975-3980. doi: 10.1021/ie202077g

58. Grigoryeva, O.; Fainleib, A.; Starostenko, O.; Danilenko, I.; Kozak, N.; and Dudarenko, G., “Ground Tire Rubber (GTR) Reclamation: Virgin Rubber / Reclaimed GTR (RE)Vulcanizates,” Rubber Chemistry and Technology, V. 77, No. 1, 2004, pp. 131-146. doi: 10.5254/1.3547806

59. Leemann, A.; Nygaard, P.; and Lura, P., “Impact of Admixtures on the Plastic Shrinkage Cracking of Self-Compacting Concrete,” Cement and Concrete Composites, V. 46, 2014, pp. 1-7. doi: 10.1016/j.cemconcomp.2013.11.002

60. Fu, X., and Chung, D. D. L., “Vibration Damping Admixtures for Cement,” Cement and Concrete Research, V. 26, No. 1, 1996, pp. 69-75. doi: 10.1016/0008-8846(95)00177-8

61. Pan, T.; Melgar, C.; and Robinson, T., “Damping Capacity of Styrene-Butadiene Latex Admixed Concrete: A Micromechanical Study,” Journal of Materials in Civil Engineering, ASCE, V. 24, No. 9, 2012, pp. 1237-1244. doi: 10.1061/(ASCE)MT.1943-5533.0000499

62. Terrill, E. R.; Centea, M.; Evans, L. R. et al., “Dynamic Mechanical Properties of Passenger and Light Truck Tire Treads,” Report No. DOT HS 811 270, National Highway Traffic Safety Administration, U.S. Department of Transportation, Washington, DC, 2010, 28 pp.

63. Kamijo, T., and Chiba, M., “Microwave Properties of Rock Salt and Limestone for Detection of Ultra-High Energy Neutrinos,” Particle Astrophysics Instrumentation, P. W. Gorham, ed., 2003. p. 151.

64. Fall, M.; Esquenazi, G.; Allan, S.; and Shulman, H., “Rapid Limestone Calcination Using Microwave Assist Technology,” 35th International Conference & Exposition on Advanced Ceramics and Composites, 2011, pp. 1-9.

65. Bekkedahl, N., “Forms of Rubber as Indicated by Temperature-Volume Relationship,” Journal of Research of the National Bureau of Standards, V. 13, No. 3, 1934, p. 411 doi: 10.6028/jres.013.029

66. Sellevold, E. J., and Bjøntegaard, Ø., “Coefficient of Thermal Expansion of Cement Paste and Concrete: Mechanisms of Moisture Interaction,” Materials and Structures, V. 39, No. 9, 2006, pp. 809-815. doi: 10.1617/s11527-006-9086-z

67. Honorio, T.; Bary, B.; and Benboudjema, F., “Thermal Properties of Cement-Based Materials: Multiscale Estimations at Early-Age,” Cement and Concrete Composites, V. 87, 2018, pp. 205-219. doi: 10.1016/j.cemconcomp.2018.01.003


ALSO AVAILABLE IN:

Electronic Materials Journal