Mass Shotcrete Wall Construction and Thermal Control Plan

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mass Shotcrete Wall Construction and Thermal Control Plan

Author(s): Lihe Zhang, Dudley R. Morgan, Iain Kirk, Anastasia Rolland, and Robert Karchewski

Publication: Materials Journal

Volume: 118

Issue: 3

Appears on pages(s): 71-82

Keywords: compaction; consolidation; encapsulation; mass concrete; mass shotcrete; nozzleman; shotcrete; temperature differential; thermal control plan

DOI: 10.14359/51730423

Date: 5/1/2021

Abstract:
Wet-mix shotcrete has been used more and more for structural applications in the past few decades. Recently, wet-mix shotcrete was successfully used to construct a mass structural wall with congested reinforcement and minimum dimensions of 1.0 m in a sewage treatment plant. A low-heat shotcrete mixture that included up to 40% slag was proposed for shotcrete application. A preconstruction mockup was shot to established proper work procedures for shotcrete application and qualify the shotcrete mixture and shotcrete nozzlemen. Extraction of cores and cut windows from the mockup confirmed proper consolidation around the congested reinforcement. A thermal control plan was developed, which included laboratory and field testing requirements, thermal analysis modeling with a three-dimensional (3-D) finite element program, and thermal control requirements, including installation of cooling pipes and thermal blankets. Shotcrete proved to be an efficient means for mass concrete structural construction. Thermal control for mass shotcrete construction was studied, and the proposed thermal control plan was proved to function properly. The general guidance for mass shotcrete construction is provided.

Related References:

1. ACI Committee 506, “Guide to Shotcrete (ACI 506R-16),” American Concrete Institute, Farmington Hills, MI, 2016, 8 pp.

2. ACI Committee C660, “CP-60 Craftsman Workbook for ACI Certification of Shotcrete Nozzleman,” American Concrete Institute, Farmington Hills, MI, 2015, 120 pp.

3. Zhang, L.; Morgan, D. R.; and Mindess S., “Comparative Evaluation of the Transport Properties of Shotcrete Compared to Cast-in-Place Concrete,” ACI Materials Journal, V. 113, No. 3, May-June 2016, pp. 373-384.

4. Zhang, L., “Air Content in Shotcrete: As-Shot vs. As-Batched,” Shotcrete, Winter 2012, pp. 50-54.

5. Zhang, L., “President’s Memo,” Shotcrete, Winter 2019, pp. 4-5.

6. Hanskat, C.; Holland, T. C.; and Suprenant, B. A., “Shotcrete Incorporated into ACI 318-19 Building Code,” Concrete International, V. 41, No. 12, Dec. 2019, pp. 31-35.


ALSO AVAILABLE IN:

Electronic Materials Journal