Influence of Silica Fume on Freezing-and-Thawing Resistance of Cement Paste at Early Age

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Silica Fume on Freezing-and-Thawing Resistance of Cement Paste at Early Age

Author(s): Jiayin Tao, Rita Maria Ghantous, Ming Jin, and Jason Weiss

Publication: Materials Journal

Volume: 118

Issue: 2

Appears on pages(s): 107-116

Keywords: degree of saturation; freezing and thawing; residual strain; silica fume

DOI: 10.14359/51730414

Date: 3/1/2021

Abstract:
The objective of this study is to determine whether the addition of silica fume (SF) can accelerate a reduction in the degree of saturation (DOS) of sealed cementitious materials at early ages, thereby increasing the freezing-and-thawing (F-T) resistance of the paste. This study investigated the influence of SF on the F-T resistance of cementitious materials using two techniques. The first technique consists of quantifying the DOS of cementitious materials at early ages and compares it to the critical degree of saturation (DOSCR). The second technique consists of determining the difference in the length of the cement paste sample before and after exposure to an F-T cycle at early ages. The change in length during the F-T cycle is an indicator of the development of damage caused by F-T. The DOS decreases faster when a higher amount of SF replaces cement. Consequently, the DOS of SF cement paste samples are more likely to be below DOSCR faster than plain cement paste samples when the samples are sealed.

Related References:

1. Fagerlund, G., “Critical Degrees of Saturation at Freezing of Porous and Brittle Materials,” Report Lund University, Division of Building Technology, Lund, Sweden, 1973.

2. Fagerlund, G., “The International Cooperative Test of the Critical Degree of Saturation Method of Assessing the Freeze/Thaw Resistance of Concrete,” Materiales de Construcción, V. 10, July 1977, pp. 231-253.

3. Li, W.; Pour-Ghaz, M.; Castro, J.; and Weiss, J., “Water Absorption and Critical Degree of Saturation Relating to Freeze-Thaw Damage in Concrete Pavement Joints,” Journal of Materials in Civil Engineering, ASCE, V. 24, No. 3, 2011, pp. 299-307. doi: 10.1061/(ASCE)MT.1943-5533.0000383

4. Ghantous, R. M.; Madland, H.; Kwong, J.; and Weiss, J., “Examining the Influence of the Degree of Saturation on Length Change and Freeze-Thaw Damage,” Advances in Civil Engineering Materials, V. 8, No. 1, 2019, pp. 365-374. doi: 10.1520/ACEM20190001

5. Trofimov, B. Y.; Kramar, L. Y.; and Schuldyakov, K. V., “On Deterioration Mechanism of Concrete Exposed to Freeze-Thaw Cycles,” IOP Conference Series. Materials Science and Engineering, V. 262, Sept, 2017, pp. 12-19. doi: 10.1088/1757-899X/262/1/012019

6. Beaudoin, J. J., and Macinnis, C., “Dimensional Changes of Hydrated Portland Cement Paste during Slow Cooling and Warming,” Cement and Concrete Research, V. 2, No. 2, 1972, pp. 225-240. doi: 10.1016/0008-8846(72)90044-0

7. Vuorinen, J., “On Use of Dilation Factor and Degree of Saturation in Testing Concrete for Frost Resistance,” Materials Science, V. 14, No. 1, 1970, pp. 37-64.

8. Chan, C. T., and Hover, K. C., “Assessing Freeze-Thaw Damage in Segmental Retaining Walls Units by Mass Loss, Moisture Gain, and Relative Dynamic Modulus,” Transportation Research Record: Journal of the Transportation Research Board, V. 2673, No. 11, 2019, pp. 309-318. doi: 10.1177/0361198119851449

9. Fagerlund, G., “A Service Life Model for Internal Frost Damage in Concrete,” Report TVBM, V. 3119, Division of Building Materials, LTH, Lund University, Lund, Sweden, 2004.

10. Fagerlund, G., “The Critical Degree of Saturation Method of Assessing the Freeze/Thaw Resistance of Concrete,” Materiales de Construcción, V. 10, Jul, 1977, pp. 217-229.

11. Malhotra, V. M., “Fly Ash, Silica Fume, Slag, and Natural Pozzolans in Concrete,” Proceedings, International Conference on Fly Ash, Silica Fume, Slag, and Natural Pozzolans in Concrete, Trondheim, Norway, 1989.

12. Khan, M. I., and Siddique, R., “Utilization of Silica Fume in Concrete: Review of Durability Properties,” Resources, Conservation and Recycling, V. 57, Dec. 2011, pp. 30-35. doi: 10.1016/j.resconrec.2011.09.016

13. Aïtcin, P. C., and Vezina, D., “Resistance to Freezing and Thawing of Silica Fume Concrete,” Cement, Concrete and Aggregates, V. 6, No. 1, 1984, pp. 38-42. doi: 10.1520/CCA10352J

14. Cohen, M. D.; Olek, J.; and Dolch, W. L., “Mechanism of Plastic Shrinkage Cracking in Portland Cement and Portland Cement-Silica Fume Paste and Mortar,” Cement and Concrete Research, V. 20, No. 1, 1990, pp. 103-119. doi: 10.1016/0008-8846(90)90121-D

15. Chung, C. W.; Shon, C. S.; and Kim, Y. S., “Chloride Ion Diffusivity of Fly Ash and Silica Fume Concretes Exposed to Freeze-Thaw Cycles,” Construction and Building Materials, V. 24, No. 9, 2010, pp. 1739-1745. doi: 10.1016/j.conbuildmat.2010.02.015

16. Pigeon, M.; Pleau, R.; and Aïtcin, P. C., “Freeze-Thaw Durability of Concrete with and without Silica Fume in ASTM C 666 (Procedure A) Test Method: Internal Cracking Versus Scaling,” Cement, Concrete and Aggregates, V. 8, No. 2, 1986, pp. 76-85. doi: 10.1520/CCA10060J

17. Sabir, B. B., “Mechanical Properties and Frost Resistance of Silica Fume Concrete,” Cement and Concrete Composites, V. 19, No. 4, 1997, pp. 285-294. doi: 10.1016/S0958-9465(97)00020-6

18. Litvan, G. G., “Freeze-Thaw Durability of Porous Building Materials,” Durability of Building Materials and Components, P. Sereda and G. Litvan, eds., ASTM International, West Conshohocken, PA, 1980, pp. 455-463.

19. Thomas, M., Supplementary Cementing Materials in Concrete, CRC Press, Taylor & Francis Group, Boca Raton, FL, 2017, 201 pp.

20. Carette, G. G., and Malhotra, V. M., “Mechanical Properties, Durability, and Drying Shrinkage of Portland Cement Concrete Incorporating Silica Fume,” Cement, Concrete and Aggregates, V. 5, No. 1, 1983, pp. 3-13. doi: 10.1520/CCA10244J

21. Cheng-Yi, H., and Feldman, R. F., “Dependence of Frost Resistance on the Pore Structure of Mortar Containing Silica Fume,” ACI Journal Proceedings, V. 82, No. 5, Sept.-Oct. 1985, pp. 740-743.

22. Kevern, J. T.; Schaefer, V. R.; Wang, K.; and Suleiman, M. T., “Pervious Concrete Mixture Proportions for Improved Freeze-Thaw Durability,” Journal of ASTM International, V. 5, No. 2, 2008, pp. 1-12.

23. Yang, Z., “Freezing-and-Thawing Durability of Pervious Concrete under Simulated Field Conditions,” ACI Materials Journal, V. 108, No. 2, Mar.-Apr. 2011, pp. 187-195.

24. Powers, T. C., “Basic Considerations Pertaining to Freezing- and-Thawing Tests,” ASTM Proceedings, V. 55, 1955, pp. 1132-1155.

25. Du, P.; Yao, Y.; Wang, L.; Xu, D. Y.; Zhou, Z. H.; Huang, S. F.; and Cheng, X., “Deformation of Concrete Matrix Subject to Cyclic Freeze-Thaw,” Royal Society of Chemistry Advances, V. 6, No. 63, 2016, pp. 58417-58425. doi: 10.1039/C6RA01472K

26. Wang, Z.; Yao, Y.; and Wang, L., “Deformation and Deterioration Analysis of Concrete Exposed to Freeze-Thaw Cycles and Chloride Salt Attack,” Journal of the Chinese Ceramic Society, V. 40, No. 8, 2012, pp. 1133-1138.

27. Zhao, X.; Lv, X.; Wang, L.; Zhu, Y.; Dong, H.; Chen, W.; Li, J.; Ji, B.; and Ding, Y., “Research of Concrete Residual Strains Monitoring Based on WLI and FBG Following Exposure to Freeze-Thaw Tests,” Cold Regions Science and Technology, V. 116, Aug, 2015, pp. 40-48. doi: 10.1016/j.coldregions.2015.04.007

28. Powers, T. C., and Helmuth, R. A., “Theory of Volume Changes in Hardened Portland-Cement Paste during Freezing,” Proceedings, Thirty-Second Annual Meeting of the Highway Research Board, Washington, DC, V. 32, 1953, pp. 285-297.

29. ASTM C305-14, “Standard Practice for Mechanical Mixing of Hydraulic Cement Pastes and Mortars of Plastic Consistency,” ASTM International, West Conshohocken, PA, 2014, 3 pp.

30. Taylor, H. F. W., Cement Chemistry, second edition, University of Aberdeen, Thomas Telford, New York, 1997, pp. 1-469.

31. Pane, I., and Hansen, W., “Investigation of Blended Cement Hydration by Isothermal Calorimetry and Thermal Analysis,” Cement and Concrete Research, V. 35, No. 6, 2005, pp. 1155-1164. doi: 10.1016/j.cemconres.2004.10.027

32. Fagerlund, G., “Chemically Bound Water as Measure of Degree of Hydration: Method and Potential Errors,” Report TVBM; V. 3150, Division of Building Materials, Lund Institute of Technology, Lund, Sweden, 2009, p. 28.

33. Neithalath, N.; Persun, J.; and Hossain, A., “Hydration in High-Performance Cementitious Systems Containing Vitreous Calcium Aluminosilicate or Silica Fume,” Cement and Concrete Research, V. 39, No. 6, 2009, pp. 473-481. doi: 10.1016/j.cemconres.2009.03.006

34. Papadakis, V. G., “Experimental Investigation and Theoretical Modeling of Silica Fume Activity in Concrete,” Cement and Concrete Research, V. 29, No. 1, 1999, pp. 79-86. doi: 10.1016/S0008-8846(98)00171-9

35. Lura, P.; Jensen, O. M.; and Van Breugel, K., “Autogenous Shrinkage in High-Performance Cement Paste: An Evaluation of Basic Mechanisms,” Cement and Concrete Research, V. 33, No. 2, 2003, pp. 223-232. doi: 10.1016/S0008-8846(02)00890-6

36. Ramachandran, V. S.; Paroli, R. M.; Beaudoin, J. J.; and Delgado, A. H., “Handbook of Thermal Analysis of Construction Materials,” Institute for Research in Construction, National Research Council of Canada, Noyes Publications, William Andrew Publishing, Norwich, NY, 2002, 691 pp.

37. Villain, G.; Thiery, M.; and Platret, G., “Measurement Methods of Carbonation Profiles in Concrete: Thermogravimetry, Chemical Analysis and Gammadensimetry,” Cement and Concrete Research, V. 37, No. 8, 2007, pp. 1182-1192. doi: 10.1016/j.cemconres.2007.04.015

38. Kim, T., and Olek, J., “Effects of Sample Preparation and Interpretation of Thermogravimetric Curves on Calcium Hydroxide in Hydrated Pastes and Mortars,” Transportation Research Record: Journal of the Transportation Research Board, V. 2290, No. 1, 2012, pp. 10-18. doi: 10.3141/2290-02

39. Suraneni, P.; Azad, V. J.; Isgor, O. B.; and Weiss, J., “Role of Supplementary Cementitious Material Type in the Mitigation of Calcium Oxychloride Formation in Cementitious Pastes,” Journal of Materials in Civil Engineering, ASCE, V. 30, No. 10, 2018, pp. 1-10. doi: 10.1061/(ASCE)MT.1943-5533.0002425

40. Banthia, N.; Pigeon, M.; and Lachance, L., “Calorimetric Study of Freezable Water in Cement Paste,” Cement and Concrete Research, V. 19, No. 6, 1989, pp. 939-950. doi: 10.1016/0008-8846(89)90107-5

41. Montanari, L., “Toward a Mixture Design Methodology for Internally Cured Concrete That Considers Filling Specific Pore Sizes Caused by Self-Desiccation,” master’s thesis, Oregon State University, Corvallis, OR, 2017, pp. 1-123.

42. Zelić, J.; Rušić, D.; Veža, D.; and Krstulović, R., “The Role of Silica Fume in the Kinetics and Mechanisms during the Early Stage of Cement Hydration,” Cement and Concrete Research, V. 30, No. 10, 2000, pp. 1655-1662. doi: 10.1016/S0008-8846(00)00374-4

43. Lawrence, P.; Cyr, M.; and Ringot, E., “Mineral Admixtures in Mortars: Effect of Inert Materials on Short-Term Hydration,” Cement and Concrete Research, V. 33, No. 12, 2003, pp. 1939-1947. doi: 10.1016/S0008-8846(03)00183-2

44. Stumm, W., Chemistry of the Solid-Water Interface: Processes at the Mineral-Water and Particle-Water Interface in Natural Systems, A Wiley-Interscience Publication, New York, 1992, pp. 1-432.

45. Mitchell, D. R. G.; Hinczak, I.; and Day, R. A., “Interaction of Silica Fume with Calcium Hydroxide Solutions and Hydrated Cement Pastes,” Cement and Concrete Research, V. 28, No. 11, 1998, pp. 1571-1584. doi: 10.1016/S0008-8846(98)00133-1

46. Muller, A. C. A.; Scrivener, K. L.; Skibsted, J.; Gajewicz, A. M.; and McDonald, P. J., “Influence of Silica Fume on the Microstructure of Cement Pastes: New Insights from 1H NMR Relaxometry,” Cement and Concrete Research, V. 74, Aug. 2015, pp. 116-125. doi: 10.1016/j.cemconres.2015.04.005

47. Rossen, J. E.; Lothenbach, B.; and Scrivener, K. L., “Composition of C–S–H in Pastes with Increasing Levels of Silica Fume Addition,” Cement and Concrete Research, V. 75, Sept. 2015, pp. 14-22. doi: 10.1016/j.cemconres.2015.04.016

48. Sun, Z., and Scherer, G. W., “Effect of Air Voids on Salt Scaling and Internal Freezing,” Cement and Concrete Research, V. 40, No. 2, 2010, pp. 260-270. doi: 10.1016/j.cemconres.2009.09.027

49. Sun, Z., and Scherer, G. W., “Pore Size and Shape in Mortar by Thermoporometry,” Cement and Concrete Research, V. 40, No. 5, 2010, pp. 740-751. doi: 10.1016/j.cemconres.2009.11.011

50. Sun, Z., and Scherer, G. W., “Measurement and Simulation of Dendritic Growth of Ice in Cement Paste,” Cement and Concrete Research, V. 40, No. 9, 2010, pp. 1393-1402. doi: 10.1016/j.cemconres.2010.03.008

51. Esmaeeli, H. S.; Farnam, Y.; Bentz, D. P.; Zavattieri, P. D.; and Weiss, J., “Numerical Simulation of the Freeze-Thaw Behavior of Mortar Containing Deicing Salt Solution,” Materials and Structures, V. 50, Feb. 2017, pp. 1-20. doi: 10.1617/s11527-016-0964-8

52. Ahmet, B.; Kazim, T.; and Ceren, K., “Influence of Silica Fume and Class F Fly Ash on Mechanical and Rheological Properties and Freeze-Thaw Durability of Self-Compacting Mortars,” Journal of Cold Regions Engineering, V. 32, No. 3, 2018, pp. 1-8.

53. Ghantous, R. M.; Khanzadeh, M. M.; Hall Becker, H.; Ley, M. T.; and Weiss, W. J., “Determining the Freeze-Thaw Performance of Mortar Samples Using Length Change Measurements During Freezing,” Cement and Concrete Composites, V. 116, Feb, 2021, p. 36.


ALSO AVAILABLE IN:

Electronic Materials Journal