Review of Several Experimental Methods for Characterization of Micro- and Nano-Scale Pores in Cement-Based Material

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Review of Several Experimental Methods for Characterization of Micro- and Nano-Scale Pores in Cement-Based Material

Author(s): Abudushalamu Aili, Ippei Maruyama

Publication: IJCSM

Volume: 14

Issue:

Appears on pages(s):

Keywords: cement, pore size distribution, specific surface area, sorption isotherm, 1H-NMR, SAS

DOI: 10.1186/s40069-020-00431-y

Date: 11/30/2020

Abstract:
Mechanical properties and durability of cement-based materials are largely affected by pore structures. This paper provides an overview of several experimental techniques to characterize pore size distribution and specific surface area, with focus on pores in calcium silicate hydrates. The reviewed experimental techniques are nitrogen and water vapor sorption isotherm, proton nuclear magnetic resonance (1H-NMR) and small-angle scattering (SAS). Different pretreatment methods are compared for sorption measurements. Pore size distribution and specific surface area are analyzed using data from different methods to understand difference and consistency of these methods. It is found that pore size distribution calculated from sorption isotherm is very sensitive to adsorption model. Though specific surface areas from different techniques are quite different from each other, they are all able to detect the microstruc-tural alteration due to long-term drying.