Pumping Up Profits

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Pumping Up Profits

Author(s): Tripp Farrell

Publication: Concrete International

Volume: 42

Issue: 12

Appears on pages(s): 45-48

Keywords: shotcrete, wet-mix, dry-mix, pumps

DOI: 10.14359/51730378

Date: 12/1/2020

Abstract:
This article provides guidance on concrete pumps for contractors looking to expand their services into shotcrete. It discusses the use of rotary gunite machines for dry-mix shotcrete and four pump types that are available for delivering wet-mix concrete: swing tube piston, squeeze tube (peristaltic), rotor stator (progressive cavity), and hydraulic ball valve pumps.

Related References:

1. Hanskat, C., “ACI Nozzleman Certification—Why, Who, When, and How,” Shotcrete, Winter 2018, pp. 22-27.

2. Bittner, D., “Shotcrete: Wet Process Versus Dry Process,” Concrete Repair Bulletin, July/Aug. 2015, pp. 20-23.