Influence of Initial Damage Degree on the Degradation of Concrete Under Sulfate Attack and Wetting–Drying Cycles

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Initial Damage Degree on the Degradation of Concrete Under Sulfate Attack and Wetting–Drying Cycles

Author(s): Yujing Lv, Wenhua Zhang, Fan Wu, Huang Li, Yunsheng Zhang, Guodong Xu

Publication: IJCSM

Volume: 14

Issue:

Appears on pages(s):

Keywords: initial damage, sulfate attack, wetting–drying cycles, mass loss, relative dynamic modulus, compressive strength

DOI: 10.1186/s40069-020-00422-z

Date: 9/30/2020

Abstract:
The previous researches on the degradation process of concrete under sulfate attack mainly focus on non-damaged concrete. It may lead to an excessive evaluation of the durability of the structure, which is detrimental to the safety of the structure. In this paper, three different damage degrees of concrete specimens with non-damaged (D0) and initial damage of 10% (D1) and 20% (D2) were prefabricated and subjected to sulfate attack and wetting–drying cycles. With the increase of sulfate attack cycles (0, 30, 60, 90, 120, 150 cycles), the changes in mass loss, relative dynamic modulus of elasticity, and the stress–strain curve were studied. The results show that the mass of the D0 specimen had been increasing continuously before 150 sulfate attack cycles. The mass of D1 and D2 had been increasing before 60 cycles, and decreasing after 60 cycles. At 150 cycles, the mass loss of D0, D1, D2 were − 1.054%, 0.29% and 3.20%, respectiv ely. The relative dynamic modulus of elasticity (RDME) of D0 specimen increases continuously before 90 sulfate attack cycles. After 90 cycles, the RDME gradually decreases. However, for D1 and D2 specimens, the RDME began to decrease after 30 cycles. The damage degree has an obvious influence on the compressive strength and elastic modulus. For the D0 specimen, the compressive strength and elastic modulus increased continuously before 90 cycles and decreased after 90 cycles. The compressive strength and elastic modulus of D1 and D2 specimens began to decrease after 30 cycles. The stress–strain curves of concrete with different initial damage degrees were established, and the fitting results were good. Finally, based on the analysis of experimental data, the degradation mechanism of concrete with initial damage under the sulfate wetting–drying cycle was discussed.