Stressing State Analysis of Reinforcement Concrete Beams Strengthened with Carbon Fiber Reinforced Plastic

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Stressing State Analysis of Reinforcement Concrete Beams Strengthened with Carbon Fiber Reinforced Plastic

Author(s): Jie Huang, Jun Shi, Hengheng Xiao, Jiyang Shen, Baisong Yang

Publication: IJCSM

Volume: 14

Issue:

Appears on pages(s):

Keywords: stressing state, leap, failure load, stressing state mode, numerical shape function, CFRP, reinforcement concrete beam

DOI: 10.1186/s40069-020-00417-w

Date: 9/30/2020

Abstract:
This paper investigated the working behavior characteristics of six reinforcement concrete (RC) beams subjected to bending based on the numerical shape function (NSF) method and structural stressing state theory. Firstly, the structural stressing state mode is expressed based on the generalized strain energy density (GSED) derived from the measured strain data. Then, one of the Carbon Fiber Reinforced Plastic (CFRP)-strengthened RC beams is taken as an example and the leap characteristics of RC beam’s stressing state are detected by applying the Mann–Kendall (M–K) criterion, updating the existing definition of the structural failure load. Accordingly, the stressing state modes and strain fields of the CFRP-strengthened RC beam are proposed to reveal their leap characteristics. Furthermore, through comparing the working performance of six RC beams, the effects of different strengths and different reinforcement ratios on CFRP strengthening performance are investigated. Finally, the NSF method is applied to reasonably interpo-late the limited strain data for further revealing the stressing state characteristics of the RC beams. The research results explore a new analysis method to conduct an accurate estimation of the structural failure load and provide a refer-ence for the future design of CFRP-strengthened RC beams.