Modeling the Effect of Prestressing on Ultimate Shear Behavior of Deep-to-Slender Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Modeling the Effect of Prestressing on Ultimate Shear Behavior of Deep-to-Slender Concrete Beams

Author(s): Boyan I. Mihaylov, Jian Liu, and Muhammed F. Ozkan

Publication: Structural Journal

Volume: 118

Issue: 2

Appears on pages(s): 89-100

Keywords: arch action; deformation patterns; kinematic model; prestressed beams; shear; strut-and-tie model

DOI: 10.14359/51729353

Date: 3/1/2021

Abstract:
Deep concrete beams with shear span-depth ratios a/d ≤ 2.5 are used to resist large shear forces due to their ability to develop arch action. In high-rise buildings, deep transfer girders are typically loaded by discontinuous columns from multiple floors, while in bridges, deep pier caps support the girders of the superstructure. In these situations, prestressing is typically applied to limit the opening of cracks under service loads, but its favorable effect on the shear strength is either neglected or underestimated. This paper examines experimental evidence for the shear behavior of prestressed beams and proposes a kinematics-based model for predicting their strength and deformations at failure. It is shown that prestressing alters the crack patterns of concrete beams, and consequently results in the development of arch action in beams with a/d reaching 6 or 7. Therefore, the proposed model, which stems from a two-parameter kinematic theory for deep reinforced concrete beams, is extended and applied to prestressed test specimens with a/d varying from 0.55 to 6.73, producing adequate predictions of strength and deformations.

Related References:

1. Tan, K. H., and Mansur, M. A., “Partial Prestressing in Concrete Corbels and Deep Beams,” ACI Structural Journal, V. 89, No. 3, May-June 1992, pp. 251-262.

2. AASHTO, “AASHTO LRFD Bridge Design Specifications and Commentary, sixth edition,” American Association of State Highway Transportation Officials, Washington, DC, 2012, 1264 pp.

3. Committee, C. S. A., A23.3-14, “Design of Concrete Structures,” Canadian Standards Association, Mississauga, ON, Canada, 2014, 290 pp.

4. Vecchio, F. J., and Collins, M. P., “The Modified Compression Field Theory for Reinforced Concrete Elements Subjected to Shear,” ACI Journal Proceedings, V. 83, No. 2, Mar.-Apr. 1986, pp. 219-231.

5. Liu, J., and Mihaylov, B. I., “A Comparative Study of Models for Shear Strength of Reinforced Concrete Deep Beams,” Engineering Structures, V. 112, 2016, pp. 81-89. doi: 10.1016/j.engstruct.2016.01.012

6. Mihaylov, B. I.; Bentz, E. C.; and Collins, M. P., “Two-Parameter Kinematic Theory for Shear Behavior of Deep Beams,” ACI Structural Journal, V. 110, No. 3, May-June 2013, pp. 447-456.

7. Mihaylov, B. I.; Liu, J.; Simionopoulos, K.; Bentz, E. C.; and Collins, M. P., “Effect of Member Size and Tendon Layout on Shear Behavior of Post-Tensioned Beams,” ACI Structural Journal, V. 116, No. 4, July 2019, pp. 265-274. doi: 10.14359/51715633

8. Collins, M. P., and Daniel, K., “How Safe Are Our Large, Lightly Reinforced Concrete Beams, Slabs, and Footings?,” ACI Structural Journal, V. 96, No. 4, July-Aug. 1999, pp. 482-490.

9. Zink, M., For the Flexural Failure of Slender Components Made of High-Performance Concrete with and without Prestressing, Springer-Verlag, 2013.

10. Kueres, D., and Hegger, J., “Two-Parameter Kinematic Theory for Punching Shear in Reinforced Concrete Slabs without Shear Reinforcement,” Engineering Structures, V. 175, 2018, pp. 201-216. doi: 10.1016/j.engstruct.2018.08.023

11. Mihaylov, B. I.; Hannewald, P.; and Beyer, K., “Three-Parameter Kinematic Theory for Shear-Dominated Reinforced Concrete Walls,” Journal of Structural Engineering, ASCE, V. 142, No. 7, 2016, p. 04016041 doi: 10.1061/(ASCE)ST.1943-541X.0001489

12. Sozen, M. A.; Zwoyer, E. M.; and Siess, C. P., “Investigation of Prestressed Concrete for Highway Bridges: Part I Strength in Shear of Beams without Web Reinforcement,” University of Illinois at Urbana Champaign, College of Engineering, Engineering Experiment Station, 1959.

13. Tan, K. H.; Lu, H. Y.; and Teng, S., “Size Effect in Large Prestressed Concrete Deep Beams,” ACI Structural Journal, V. 96, No. 6, Nov.-Dec. 1999, pp. 937-946.

14. Teng, S.; Kong, F. K.; and Poh, S. P., “Shear Strength of Reinforced and Prestressed Concrete Deep Beams. Part II: The Supporting Evidence,” Proceedings of the Institution of Civil Engineers. Structures and Buildings, V. 128, No. 2, 1998, pp. 124-143. doi: 10.1680/istbu.1998.30120

15. Cederwall, K.; Hedman, O.; and Loeberg, A., “Shear Strength of Partially Prestressed Beams with Pretensioned Reinforcement of High-Grade Deformed Bars,” Shear in Reinforced Concrete, SP-42, American Concrete Institute, Farmington Hills, MI, 1974, pp. 215-230.

16. Okada, K.; Kobayashi, K.; and Toyofuku, T., “Flexural Shear Behavior of Prestressed Reinforced Concrete Beams,” Transactions of the Japan Cement Association, V. 34, 1980, pp. 425-428. (in Japanese)

17. Muguruma, A.; Watanabe, F.; and Fujii, M., “Experimental Study on Shear Resisting Behavior of Prestressed Reinforced Concrete Beams,” Transactions of the Japan Concrete Institute, V. 5, 1983, pp. 453-456. (in Japanese)

18. Sato, T.; Ishibashi, T.; Yamashita, Y.; and Takada, S., “Shear Strength and Failure Mode of Prestressed Concrete Beams,” Transactions of the Japan Concrete Institute, V. 9, No. 2, 1987, pp. 323-328. (in Japanese)

19. Nakamura, E.; Takeuchi, Y.; Aoyama, H.; Murakoshi, J.; and Kimura, Y., “Study on Shear Resisting Behavior of Corroded Prestressed Concrete Beams,” Proceedings of the Concrete Structure Scenarios, V. 9, 2009, pp. 411-416. (in Japanese)

20. Reineck, K. H., and Dunkelberg, D., “ACI-DAfStb Databases 2015 with Shear Tests for Evaluating Relationships for the Shear Design of Structural Concrete Members Without and with Stirrups,” Beuth Verlag GmbH, 2017.

21. Bentz, E. C.; Vecchio, F. J.; and Collins, M. P., “Simplified Modified Compression Field Theory for Calculating Shear Strength of Reinforced Concrete Elements,” ACI Materials Journal, V. 103, No. 4, July-Aug. 2006, pp. 614-624.

22. Dunkelberg, D.; Sneed, L. S.; Zilch, K.; and Reineck, K. H., “The 2015 ACI‐DAfStb Database of Shear Tests on Slender Prestressed Concrete Beams without Stirrups - Overview and Evaluation of Current Design Approaches,” Structural Concrete, V. 19, No. 6, 2018, pp. 1740-1759.


ALSO AVAILABLE IN:

Electronic Structural Journal