Interface Shear Strength between Ultra-High-Performance Concrete and Normal-Strength Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Interface Shear Strength between Ultra-High-Performance Concrete and Normal-Strength Concrete

Author(s): Hyun-Soo Youm, Woo-Young Lim, Sung-Gul Hong, and Changbin Joh

Publication: Structural Journal

Volume: 118

Issue: 2

Appears on pages(s): 287-298

Keywords: failure criteria; failure modes; interface shear strength; slant shear test; ultra-high-performance concrete (UHPC)

DOI: 10.14359/51729350

Date: 3/1/2021

Abstract:
Section enlargement and jacketing using ultra-high-performance concrete (UHPC) have been used to strengthen existing reinforced concrete structures. The structural performance of these strengthened structures is highly dependent on the bond performance at the interface between the UHPC and normal-strength concrete (NSC) substrates. This study investigates the shear strength and ultimate failure mode of the interface in UHPC-NSC composites using an experimental program of slant shear test. The main test parameters include the roughness and inclination angle of the interface and the curing condition of the UHPC. Both the roughness at the interface due to sand-blasting and the inclination angle of the interface control the failure modes showing distinct transitions of the failure modes between concrete crushing and near-interface concrete cracking. The failure criteria for the interface of UHPC-NSC composites can be explained using the theory of plasticity by identifying the failure modes.

Related References:

1. Charron, J. P.; Denarié, E.; and Brühwiler, E., “Permeability of Ultra High Performance Fiber Reinforced Concretes (UHPFRC) under High Stresses,” Materials and Structures, V. 40, No. 3, 2007, pp. 269-277. doi: 10.1617/s11527-006-9105-0

2. Graybeal, B., and Tanesi, J., “Durability of an Ultrahigh-Performance Concrete,” Journal of Materials in Civil Engineering, ACSE, V. 19, No. 10, 2007, pp. 848-854. doi: 10.1061/(ASCE)0899-1561(2007)19:10(848)

3. Haber, Z. B.; Munoz, J. F.; De La Varga, I.; and Graybeal, B. A., “Bond Characterization of UHPC Overlays for Concrete Bridge Decks: Laboratory and Field Testing,” Construction and Building Materials, V. 190, 2018, pp. 1056-1068. doi: 10.1016/j.conbuildmat.2018.09.167

4. Brühwiler, E., and Denarié, E., “Rehabilitation and Strengthening of Concrete Structures Using Ultra-High Performance Fibre Reinforced Concrete,” Structural Engineering International, V. 23, No. 4, 2013, pp. 450-457. doi: 10.2749/101686613X13627347100437

5. Brühwiler, E.; Bastien Masse, M.; Hartmut, M.; Bernard, H.; Blaise, F.; Stéphane, C.; Philippe, S.; Frédéric, B.; and Marco, M., 2015, “Strengthening the Chillon Viaducts Deck Slabs with Reinforced UHPFRC,” IABSE Symposium Report, V. 105, No. 24, Geneva, Switzerland, 2015, pp. 1171-1178.

6. Denarié, E.; Jacomo, D.; Fady, N.; and Corvez, D., “Rejuvenation of Maritime Signalisation Structures with UHPFRC,” RILEM-fib-AFGC International Symposium on Ultra-High Performance Fibre-Reinforced Concrete, UHPFRC 2013, Marseille, France, 2013, pp. 157-166.

7. Farzad, M.; Shafieifar, M.; and Azizinamini, A., “Retrofitting of Bridge Columns Using UHPC,” Journal of Bridge Engineering, ACSE, V. 24, No. 12, 2019, p. 04019121. doi: 10.1061/(ASCE)BE.1943-5592.0001497

8. Momayez, A.; Ehsani, M.; Ramezanianpour, A.; and Rajaie, H., “Comparison of Methods for Evaluating Bond Strength between Concrete Substrate and Repair Materials,” Cement and Concrete Research, V. 35, No. 4, 2005, pp. 748-757. doi: 10.1016/j.cemconres.2004.05.027

9. Kreigh, J. D., “Arizona Slant Shear Test: A Method to Determine Epoxy Bond Strength,” ACI Journal Proceedings, V. 73, No. 7, July 1976, pp. 372-373.

10. Austin, S.; Robins, P.; and Pan, Y., “Shear Bond Testing of Concrete Repairs,” Cement and Concrete Research, V. 29, No. 7, 1999, pp. 1067-1076. doi: 10.1016/S0008-8846(99)00088-5

11. Zanotti, C.; Banthia, N.; and Plizzari, G., “A Study of Some Factors Affecting Bond in Cementitious Fiber Reinforced Repairs,” Cement and Concrete Research, V. 63, 2014, pp. 117-126. doi: 10.1016/j.cemconres.2014.05.008

12. Feng, S.; Xiao, H.; and Geng, J., “Bond Strength between Concrete Substrate and Repair Mortar: Effect of Fibre Stiffness and Substrate Surface Roughness,” Cement and Concrete Composites, V. 114, 2020, p. 103746. doi: 10.1016/j.cemconcomp.2020.103746

13. ACI Committee 546, “Guide to Materials Selection for Concrete Repair (ACI 546.3R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 72 pp.

14. ASTM C882/C882M-20, “Standard Test Method for Bond Strength of Epoxy‐Resin Systems Used with Concrete by Slant Shear,” ASTM International, West Conshohocken, PA, 2020, 4 pp.

15. Carbonell Muñoz, M. A.; Harris, D. K.; Ahlborn, T. M.; and Froster, D. C., “Bond Performance between Ultrahigh-Performance Concrete and Normal-Strength Concrete,” Journal of Materials in Civil Engineering, ACSE, V. 26, No. 8, 2014, p. 04014031. doi: 10.1061/(ASCE)MT.1943-5533 .000089010.1061/(ASCE)MT.1943-5533

16. Farzad, M.; Shafieifar, M.; and Azizinamini, A., “Experimental and Numerical Study on Bond Strength between Conventional Concrete and Ultra High-Performance Concrete (UHPC),” Engineering Structures, V. 186, 2019, pp. 297-305. doi: 10.1016/j.engstruct.2019.02.030

17. Ganesh, P., and Murthy, A. R., “Simulation of Surface Preparations to Predict the Bond Behaviour between Normal Strength Concrete and Ultra-High Performance Concrete,” Construction and Building Materials, V. 250, 2020, p. 118871 doi: 10.1016/j.conbuildmat.2020.118871

18. Harris, D. K.; Carbonell Muñoz, M. A.; Gheitasi, A.; Ahlborn, T. M.; and Rush, S. V., “The Challenges Related to Interface Bond Characterization of Ultra-High-Performance Concrete with Implications for Bridge Rehabilitation Practices,” Advances in Civil Engineering Materials, V. 4, No. 2, 2015, pp. 75-101. doi: 10.1520/ACEM20140034

19. Lim, W. Y., and Hong, S. G., “Slant Shear Test for Determining the Interfacial Shear Strength of Concrete Strengthened with Ultra-High Performance Fiber Reinforced Concrete,” Journal of the Korea Concrete Institute, V. 28, No. 6, 2016, pp. 637-646. doi: 10.4334/JKCI.2016.28.6.637

20. Semendary, A. A., and Svecova, D., “Factors Affecting Bond between Precast Concrete and Cast in Place Ultra High Performance Concrete (UHPC),” Engineering Structures, V. 216, 2020, p. 110746 doi: 10.1016/j.engstruct.2020.110746

21. Tayeh, B. A.; Bakar, B. A.; Johari, M. M.; and Ratnam, M. M., “The Relationship between Substrate Roughness Parameters and Bond Strength of Ultra High-Performance Fiber Concrete,” Journal of Adhesion Science and Technology, V. 27, No. 16, 2013, pp. 1790-1810. doi: 10.1080/01694243.2012.761543

22. Valikhani, A.; Jahromi, A. J.; Mantawy, I. M.; and Azizinamini, A., “Experimental Evaluation of Concrete-to-UHPC Bond Strength with Correlation to Surface Roughness for Repair Application,” Construction and Building Materials, V. 238, 2020, p. 117753 doi: 10.1016/j.conbuildmat.2019.117753

23. Zhang, Y.; Zhang, C.; Zhu, Y.; Cao, J.; and Shao, X., “An Experimental Study: Various Influence Factors Affecting Interfacial Shear Performance of UHPC-NSC,” Construction and Building Materials, V. 236, 2020, p. 117480 doi: 10.1016/j.conbuildmat.2019.117480

24. Zhang, Y.; Zhu, P.; Liao, Z.; and Wang, L., “Interfacial Bond Properties between Normal Strength Concrete Substrate and Ultra-High Performance Concrete as a Repair Material,” Construction and Building Materials, V. 235, 2020, p. 117431 doi: 10.1016/j.conbuildmat.2019.117431

25. Zanotti, C.; Borges, P. H.; Bhutta, A.; and Banthia, N., “Bond Strength between Concrete Substrate and Metakaolin Geopolymer Repair Mortar: Effect of Curing Regime and PVA Fiber Reinforcement,” Cement and Concrete Composites, V. 80, 2017, pp. 307-316. doi: 10.1016/j.cemconcomp.2016.12.014

26. Beushausen, H.; Höhlig, B.; and Talotti, M., “The Influence of Substrate Moisture Preparation on Bond Strength of Concrete Overlays and the Microstructure of the OTZ,” Cement and Concrete Research, V. 92, 2017, pp. 84-91. doi: 10.1016/j.cemconres.2016.11.017

27. Talbot, C.; Pigeon, M.; Beaupre, D.; and Morgan, D. R., “Influence of Surface Preparation on Long-Term Bonding of Shotcrete,” ACI Materials Journal, V. 91, No. 6, Nov.-Dec. 1995, pp. 560-566.

28. Lothenbach, B.; Scrivener, K.; and Hooton, R. D., “Supplementary Cementitious Materials,” Cement and Concrete Research, V. 41, No. 12, 2011, pp. 1244-1256. doi: 10.1016/j.cemconres.2010.12.001

29. Zhou, J.; Ye, G.; and Van Breugel, K., “Cement Hydration and Microstructure in Concrete Repairs with Cementitious Repair Materials,” Construction and Building Materials, V. 112, 2016, pp. 765-772. doi: 10.1016/j.conbuildmat.2016.02.203

30. Júlio, E. N. B. S.; Branco, F. A. B.; and Silva, V. D., “Concrete-to-Concrete Bond Strength. Influence of the Roughness of the Substrate Surface,” Construction and Building Materials, V. 18, No. 9, 2004, pp. 675-681. doi: 10.1016/j.conbuildmat.2004.04.023

31. Randl, N., “Design Recommendations for Interface Shear Transfer in Fib Model Code 2010,” Structural Concrete, V. 14, No. 3, 2013, pp. 230-241. doi: 10.1002/suco.201300003

32. Santos, P. M. D., and Júlio, E. N. B. S., “Interface Shear Transfer on Composite Concrete Members,” ACI Structural Journal, V. 111, No. 1, Jan.-Feb. 2014, doi: 10.14359.51686543

33. ASTM C39/C39M-18, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2018, 8 pp.

34. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318M-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 628 pp.

35. ASTM C469/C469M-14, “Standard Test Method for Static Modulus of Elasticity and Poisson’s Ratio of Concrete in Compression,” ASTM International, West Conshohocken, PA, 2014, 5 pp.

36. AASHTO-LRFD, “Bridge Design Specifications,” American Association of State Highway and Transportation Officials (AASHTO), Washington, DC, 2012, 1661 pp.

37. CSA, “Design of Concrete Structures,” Canadian Standards Association, Mississauga, Ontario, Canada, 2004, 214 pp.

38. fib, “fib Model Code for Concrete Structures 2010,” Fédération Internationale du déton (fib), Lausanne, Switzerland, 2013, 434 pp.

39. Randl, N.; Peyerl, M.; and Steiner, M., “Investigations on Adhesive Bond between High Performance Concrete Overlays and NSC Substrates,” Proceedings of fib Symposium 2016: Performance-Based Approaches for Concrete Structures, Cape Town, South Africa, 2016, 11 pp.

40. Aaleti, S.; Sritharan, S.; and Abu-Hawash, A., “Innovative UHPC-Normal Concrete Composite Bridge Deck,” RILEM-fib-AFGC International Symposium on Ultra-High Performance Fibre-Reinforced Concrete, UHPFRC 2013, Marseille, France, 2013, pp. 217-226.

41. He, M. Y., and Hutchinson, J. W., “Kinking of a Crack out of an Interface,” Journal of Applied Mechanics, V. 56, No. 2, 1989, pp. 270-278. doi: 10.1115/1.3176078

42. Wall, J. S., and Shrive, N. G., “Factors Affecting Bond between New and Old Concrete,” ACI Materials Journal, V. 85, No. 2, Mar.-Apr. 1988, pp. 117-125. doi: 10.14359/2329

43. Santos, P. M. D., and Júlio, E. N. B. S., “Factors Affecting Bond between New and Old Concrete,” ACI Materials Journal, V. 108, No. 4, July-Aug. 2011, pp. 449-456. doi: 10.14359/51683118

44. Júlio, E. N. B. S.; Branco, F. A. B.; Silva, V. D.; and Lourenço, J. F., “Influence of Added Concrete Compressive Strength on Adhesion to an Existing Concrete Substrate,” Building and Environment, V. 41, No. 12, 2006, pp. 1934-1939. doi: 10.1016/j.buildenv.2005.06.023

45. Tayeh, B. A.; Abu Bakar, B. H.; Megat Johari, M. A.; and Zeyad, A. M., “Microstructural Analysis of the Adhesion Mechanism between Old Concrete Substrate and UHPFC,” Journal of Adhesion Science and Technology, V. 28, No. 18, 2014, pp. 1846-1864. doi: 10.1080/01694243.2014.925386

46. Lura, P.; Van Breugel, K.; and Maruyama, I., “Effect of Curing Temperature and Type of Cement on Early-Age Shrinkage of High-Performance Concrete,” Cement and Concrete Research, V. 31, No. 12, 2001, pp. 1867-1872. doi: S0008-8846(01)00601-9

47. Jiang, C.; Yang, Y.; Wang, Y.; Zhou, Y.; and Ma, C., “Autogenous Shrinkage of High Performance Concrete Containing Mineral Admixtures under Different Curing Temperatures,” Construction and Building Materials, V. 61, 2014, pp. 260-269. doi: 10.1016/j.conbuildmat.2014.03.023

48. Hussein, H. H.; Walsh, K. K.; Sargand, S. M.; and Steinberg, E. P., “Interfacial Properties of Ultrahigh-Performance Concrete and High-Strength Concrete Bridge Connections,” Journal of Materials in Civil Engineering, ACSE, V. 28, No. 5, 2016, p. 04015208 doi: 10.1061/(ASCE)MT.1943-5533.0001456

49. Espeche, A. D., and León, J., “Estimation of Bond Strength Envelopes for Old-to-New Concrete Interfaces Based on a Cylinder Splitting Test,” Construction and Building Materials, V. 25, No. 3, 2011, pp. 1222-1235. doi: 10.1016/j.conbuildmat.2010.09.032

50. Jensen, B. C., “Nogle Plasticitetsteoretiske Beregninger Af Beton Og Jernbeton,” PhD thesis, Technical University of Denmark, Copenhagen, Denmark, 1976.

51. Nielsen, M. P., and Hoang, L. C., Limit Analysis and Concrete Plasticity, third edition, CRC Press, Boca Raton, FL, 2011, pp. 629-668.

52. Carol, I.; Prat, P. C.; and López, C. M., “Normal/Shear Cracking Model: Application to Discrete Crack Analysis,” Journal of Engineering Mechanics, ACSE, V. 123, No. 8, 1997, pp. 765-773. doi: 10.1061/(ASCE)0733-9399(1997)123:8(765)


ALSO AVAILABLE IN:

Electronic Structural Journal