Shear Strength of Sand-Lightweight Concrete Deep Beams with Steel Fibers

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength of Sand-Lightweight Concrete Deep Beams with Steel Fibers

Author(s): Sergio Garcia, Allonso Pereira, and Rodrigo Pierott

Publication: Structural Journal

Volume: 118

Issue: 2

Appears on pages(s): 203-214

Keywords: deep beams; sand-lightweight; shear; steel fibers

DOI: 10.14359/51729347

Date: 3/1/2021

Abstract:
Six deep beams without transversal reinforcement made of sand-lightweight concrete and six deep beams made of sand-lightweight concrete with 1.0% of steel fibers were tested and compared with conventional concrete deep beams with and without fibers. The shear-span to deep beam height ratio (a/h) was 0.5, 0.8, and 1.0. The cross section heights were 400, 600, and 700 mm (15.7, 23.6, and 27.6 in.). The deep beams were tested to failure under a four-point bending test, using a hydraulic actuator with 500 kN (674 kip) capacity load cell. After testing, it was concluded that the shear-strength values were smaller in larger span deep beams. The presence of steel fibers increased the maximum strength and contributed quantify to the strength to diagonal cracking. The maximum shear load in steel fiber deep beams increased by approximately 16%. The size effect was more significant in sand-lightweight concrete deep beams. Besides, it was proposed a coefficient to validate the cracking strut-and-tie model (CSTM) to evaluate the applicability in deep beams of sand-lightweight concrete with and without steel fibers and the experimental maximum shear predictions are compared according to some codes for sand-lightweight concrete deep beams and by codes and some codes and researchers for sand lightweight concrete deep beams with steel fibers.

Related References:

1. Mattock, A. H.; Li, W. K.; and Wang, T. C., “Shear Transfer in Lightweight Reinforced Concrete,” PCI Journal, Jan.-Feb. 1976, pp. 20-39.

2. Emiko, L.; Thamaraikkannan, V.; Huan, W. T.; and Thangayah, T., “Shear Transfer in Lightweight Concrete,” Magazine of Concrete Research, V. 63, No. 6, 2011, pp. 393-00. doi: 10.1680/macr.9.00162

3. Sneed, L. H., Krc, K., and Wermager, S., “Interface Shear Transfer of Lightweight-Aggregate Concretes with Different Lightweight Aggregates,” PCI Journal, March-Apr. 2016, pp. 38-55.

4. Floyd, R. W.; Hale, W. M.; and Bymaster, J. C., “Effect of Aggregate and Cementitious Material on Properties of Lightweight Self-Consolidating Concrete for Prestressed Members,” Construction and Building Materials, V. 85, 2015, pp. 91-99. doi: 10.1016/j.conbuildmat.2015.03.084

5. Kong, F. K.. and Robins, P. J., “Web Reinforcement Effects on Lightweight Concrete Deep Beams,” ACI Journal Proceedings, V. 68, No. 7, July 1971, pp. 514-520.

6. Yang, K. H., “Tests on Lightweight Concrete Deep Beams,” ACI Structural Journal, V. 107, No. 6, Nov.-Dec. 2010, pp. 663-670.

7. Yang, K. H., and Ashour, A. F., “Aggregate Interlock in Lightweight Concrete Continuous Deep Beams,” Engineering Structures, V. 33, No. 1, 2011, pp. 136-145. doi: 10.1016/j.engstruct.2010.09.026

8. Yang, K. H.; Chung, H. S.; Lee, E. T.; and Eun, H.-C., “Shear Characteristics of High-Strength Concrete Deep Beams Without Shear Reinforcements,” Engineering Structures, V. 25, No. 10, 2003, pp. 1343-1352. doi: 10.1016/S0141-0296(03)00110-X

9. Sachan, A. K., and Kameswara Rao, C. V. S., “Behaviour of Fibre Reinforced Concrete Deep Beams,” Cement and Concrete Composites, V. 12, No. 3, 1990, pp. 211-218. doi: 10.1016/0958-9465(90)90022-P

10. Li, V. C.; Ward, R.; and Hamza, A. M., “Steel and Synthetic Fibers as Shear Reinforcement,” ACI Materials Journal, V. 89, No. 5, Sept.-Oct. 1992, pp. 499-08.

11. Visalakshia, B. S. S., and G., S. H., “Enhancement of Shear Strength of Deep Beams Using Hybrid Fibres and Suggesting an Alternative for Strut and Tie Model,” Materials Today: Proceedings, V. 33, 2020, pp. 578-582. doi: 10.1016/j.matpr.2020.05.454

12. Moradi, M., and Esfahani, M. R., “Application of the Strut-and-Tie Method for Steel Fiber Reinforced Concrete Deep Beams,” Construction and Building Materials, V. 131, 2017, pp. 423-437. doi: 10.1016/j.conbuildmat.2016.11.042

13. Chen, H.; Yi, W. J.; and Ma, Z. J., “Shear Size Effect in Simply Supported RC Deep Beams,” Engineering Structures, V. 182, 2019, pp. 268-78.

14. Birrcher, D. B.; Tuchscherer, R. G.; Huizinga, M.; and Bayrak, O., “Depth Effect in Deep Beams,” ACI Structural Journal, V. 111, No. 4, July-Aug. 2014, pp. 731-740. doi: 10.14359/51687002

15. Shuraim, A. B., and El-Sayed, A. K., “Experimental Verification of Strut and Tie Model for HSC Deep Beams Without Shear Reinforcement,” Engineering Structures, V. 117, 2016, pp. 71-85. doi: 10.1016/j.engstruct.2016.03.002

16. ABNT, “NBR 5733:1991 High Early Strength Portland Cement – Specification,” Rio de Janeiro, Brazilian Association of Technical Standards, 1991, 5 pp.

17. ABNT, “NBR NM 67:1998 Concrete – Slump Test for Determination of the Consistency,” Rio de Janeiro, Brazilian Association of Technical Standards, 1998, 8 pp.

18. ABNT, “ABNT NBR 5739 Concreto — Ensaio de compressão de corpos de prova cilíndricos,” Rio de Janeiro, Brazilian Association of Technical Standards, 2018, 9 pp.

19. ABNT, “ABNT NBR 722 Argamassa e concreto - Determinação da resistência à tração por compressão diametral de corpos-de-prova cilíndricos,” Rio de Janeiro, Brazilian Association of Technical Standards, 2011, 6 pp.

20. Narayanan, R., and Darwish, I. Y. S., “Fiber Concrete Deep Beams in Shear,” ACI Structural Journal, V. 85, No. 2, Mar.-Apr. 1988, pp. 141-149.

21. Mansur, M. A., and Ong, K. C. G., “Behavior of Reinforced Fiber Concrete Deep Beams in Shear,” ACI Structural Journal, V. 88, No. 1, Jan.-Feb. 1991, pp. 98-05.

22. Chen, H.; Yi, W.; and Hwang, H., “Cracking Strut-and-Tie Model for Shear Strength Evaluation of Reinforced Concrete Deep Beams,” Engineering Structures, V. 163, May 2018, pp. 396-408.

23. ABNT, “ABNT NBR 6118-Projeto de Estruturas de Concreto-Procedimentos,” Rio de Janeiro, Brazilian Association of Technical Standards, 2014, 255 pp.

24. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

25. CSA A23.3, “Design of Concrete Structures,” Mississauga, ON, Canada, Canadian Standards Association, 2004, 240 pp.

26. ACI Committee 544, “Design Considerations for Steel Fiber Reinforced Concrete (ACI 544.4R-88),” American Concrete Institute, Farmington Hills, MI, Reapproved 1999, 18 pp.

27. Shahnewaz, M., and Alam, M. S., “Improved Shear Equations for Steel Fiber-Reinforced Concrete Deep and Slender Beams,” ACI Structural Journal, V. 111, No. 4, July-Aug. 2014, pp. 851-860. doi: 10.14359/51686736


ALSO AVAILABLE IN:

Electronic Structural Journal