Experimental Study on Fracture Behavior of Dam Concrete under Cyclic Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study on Fracture Behavior of Dam Concrete under Cyclic Loading

Author(s): Xudong Chen, Yuzhu Guo, and Shengtao Li

Publication: Structural Journal

Volume: 118

Issue: 2

Appears on pages(s): 193-202

Keywords: acoustic emission; dam concrete; dynamic load; fracture mechanism

DOI: 10.14359/51729346

Date: 3/1/2021

Abstract:
To study the fracture behavior of dam concrete subjected to elevated-amplitude cyclic loading, the three-point bending test was carried out. During the loading process, the internal acoustic emission (AE) signal and surface cracks of dam concrete beams under cyclic loading were recorded using three-dimensional digital image correlation (3-D DIC) technique. The results show that with the increase of loading rate, AE events are concentrated near the peak load. There is a safe range of the historical index and signal intensity before failure of concrete. The analysis of load-crack mouth opening displacement (CMOD) curves shows a rate effect on the stiffness attenuation. In addition, the crack propagation mechanism under different load rates and the relationship between crack tip opening displacement (CTOD) and CMOD under different elevated-amplitudes of load are analyzed.

Related References:

1. Dong, Y.; Xiao, K.; and Yang, H., “Experimental Studies on Properties of Fully-Graded Arch Dam Concrete with Natural Aggregate,” Chinese Journal of Concrete, V. 2013, 2013, pp. 140-143. (in Chinese)

2. Zheng, D.; Han, W.; and Zhang, Y., “Research on Strength Ratio of Full Grade and Wet-Sieving Hydraulic Concrete,” Chinese Journal of Water Resources and Architectural Engineering, V. 9, 2011, pp. 10-14. (in Chinese)

3. Brühwiler, E., and Wittmann, F. H., “Failure of Dam Concrete Subjected to Seismic Loading Conditions,” Engineering Fracture Mechanics, V. 35, No. 1-3, 1990, pp. 565-571. doi: 10.1016/0013-7944(90)90231-5

4. Deng, Z.; Li, Q.; and Fu, H., “Comparison between Mechanical Properties of Dam and Sieved Concretes,” Journal of Materials in Civil Engineering, ASCE, V. 20, No. 4, 2008, pp. 321-326. doi: 10.1061/(ASCE)0899-1561(2008)20:4(321)

5. Khaloo, A. R.; Mohamadi Shooreh, M. R.; and Askari, S. M., “Size Influence of Specimens and Maximum Aggregate on Dam Concrete: Compressive Strength,” Journal of Materials in Civil Engineering, ASCE, V. 21, No. 8, 2009, pp. 349-355. doi: 10.1061/(ASCE)0899-1561(2009)21:8(349)

6. Saouma, V. E.; Broz, J. J.; Brühwiler, E.; and Boggs, H. L., “Effect of Aggregate and Specimen Size on Fracture Properties of Dam Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 3, No. 3, 1991, pp. 204-218. doi: 10.1061/(ASCE)0899-1561(1991)3:3(204)

7. Shi, D., and Chen, X., “Flexural Tensile Fracture Behavior of Pervious Concrete under Static Preloading,” Journal of Materials in Civil Engineering, ASCE, V. 30, No. 11, 2018, p. 06018015. doi: 10.1061/(ASCE)MT.1943-5533.0002477

8. Chen, X.; Shi, D.; Shen, N.; Li, S.; and Liu, S., “Experimental Study and Analytical Modeling on Fatigue Properties of Pervious Concrete Made with Natural and Recycled Aggregates,” International Journal of Concrete Structures and Materials, V. 13, No. 1, 2019, p. 10 doi: 10.1186/s40069-018-0305-0

9. Chen, X.; Liu, Z.; Guo, S.; Huang, Y.; and Xu, W., “Experimental Study on Fatigue Properties of Normal and Rubberized Self-Compacting Concrete under Bending,” Construction and Building Materials, V. 205, 2019, pp. 10-20. doi: 10.1016/j.conbuildmat.2019.01.207

10. Tang, T.; Duan, S.; and Duan, Y., “Analysis on Full-Graded and Wetscreened Tests for Jinping I Arch Dam Concrete,” Chinese Journal of Yellow River, V. 34, 2012, pp. 111-112. (in Chinese)

11. Xie, J.; Tang, Y.; and Chen, G., “Study on the Properties of Concrete for Arch Dam of Xiaowan Hydropower Station,” Chinese Journal of Water Power, V. 35, 2009, pp. 38-41. (in Chinese)

12. Li, Q.; Deng, Z.; and Fu, H., “Effect of Aggregate Type on Mechanical Behavior of Dam Concrete,” ACI Materials Journal, V. 101, No. 6, Nov.-Dec. 2004, pp. 483-492.

13. Song, Y.; Xu, X.; and Liu, H., “Comparison of Mechanical Properties of Fully-Graded Concrete and Sieved Concrete,” Journal of Hydraulic Engineering, V. 43, No. 1, 2012, pp. 69-75. (in Chinese)

14. Vilardell, J.; Aguado, A.; Agullo, L.; and Gettu, R., “Estimation of the Modulus of Elasticity for Dam Concrete,” Cement and Concrete Research, V. 28, No. 1, 1998, pp. 93-101. doi: 10.1016/S0008-8846(97)00214-7

15. Guan, J.; Li, Q.; Wu, Z.; Zhao, S.; Dong, W.; and Zhou, S., “Fracture Parameters of Site-Cast Dam and Sieved Concrete,” Magazine of Concrete Research, V. 68, No. 1, 2016, pp. 43-54. doi: 10.1680/macr.15.00008

16. Serra, C.; Batista, A. L.; and Monteiro Azevedo, N., “Effect of Wet Screening in the Elastic Properties of Dam Concrete: Experimental In Situ Test Results and Fit to Composite Models,” Journal of Materials in Civil Engineering, ASCE, V. 28, No. 12, 2016, p. 04016146 doi: 10.1061/(ASCE)MT.1943-5533.0001672

17. Serra, C.; Batista, A. L.; Azevedo, N. M.; and Custódio, J., “Prediction of Dam Concrete Compressive and Splitting Tensile Strength Based on Wet-Screened Concrete Test Results,” Journal of Materials in Civil Engineering, ASCE, V. 29, No. 10, 2017, p. 04017188. doi: 10.1061/(ASCE)MT.1943-5533.0002012

18. Huang, Y.; Xiao, L.; Gao, J.; and Liu, Y., “Tensile Creep and Unloading Creep Recovery Testing of Dam Concrete with Fly Ash,” Journal of Materials in Civil Engineering, ASCE, V. 31, No. 5, 2019, p. 05019001 doi: 10.1061/(ASCE)MT.1943-5533.0002682

19. Talboys, L. N.; Lubell, A. S.; and Bindiganavile, V. S., “Determining Specimen Size Influences on FRC Response Using the Digital Image Correlation Technique,” High Performance Fiber Reinforced Cement Composites, V. 2, 2012, pp. 35-42. doi: 10.1007/978-94-007-2436-5_5

20. Shih, M. H., and Sung, W. P., “Application of Digital Image Correlation Method for Analysing Crack Variation of Reinforced Concrete Beams,” Sadhana, V. 38, No. 4, 2013, pp. 723-741. doi: 10.1007/s12046-013-0141-5

21. Xie, Z. L.; Zhou, H. F.; Lu, L. J.; and Chen, Z. A., “An Investigation into Fracture Behavior of Geopolymer Concrete with Digital Image Correlation Technique,” Construction and Building Materials, V. 155, 2017, pp. 371-380. doi: 10.1016/j.conbuildmat.2017.08.041

22. Shahidan, S.; Pulin, R.; Bunnori, N. M.; and Holford, K. M., “Damage Classification in Reinforced Concrete Beam by Acoustic Emission Signal Analysis,” Construction and Building Materials, V. 45, 2013, pp. 78-86. doi: 10.1016/j.conbuildmat.2013.03.095

23. Nguyen-Tat, T.; Ranaivomanana, N.; and Balayssac, J. P., “Characterization of Damage in Concrete Beams under Bending with Acoustic Emission Technique (AET),” Construction and Building Materials, V. 187, 2018, pp. 487-500. doi: 10.1016/j.conbuildmat.2018.07.217

24. Li, B.; Chi, Y.; Xu, L.; Li, C.; and Shi, Y., “Cyclic Tensile Behavior of SFRC: Experimental Research and Analytical Model,” Construction and Building Materials, V. 190, 2018, pp. 1236-1250. doi: 10.1016/j.conbuildmat.2018.09.140

25. Matthews, J. R., ed., Acoustic Emission, V. 2, CRC Press, Boca Raton, FL, 1983.

26. Gutenberg, B., and Richter, C. F., “Frequency of Earthquakes in California,” Bulletin of the Seismological Society of America, V. 34, No. 4, 1944, pp. 185-188.

27. Guo, Y.; Chen, X.; Yang, H.; Hu, L.; Zhang, J.; and Fan, X., “Experimental Study on Direct Tension Behavior of Concrete through Combined Digital Image Correlation and Acoustic Emission Techniques,” Structural Concrete, V. 20, No. 6, 2019, pp. 2042-2055. doi: 10.1002/suco.201800354

28. Colombo, I. S.; Main, I. G.; and Forde, M. C., “Assessing Damage of Reinforced Concrete Beam Using “b-Value” Analysis of Acoustic Emission Signals,” Journal of Materials in Civil Engineering, ASCE, V. 15, No. 3, 2003, pp. 280-286. doi: 10.1061/(ASCE)0899-1561(2003)15:3(280)

29. Rao, M. V. M. S., and Lakshmi, K. J. P., “Analysis of b-Value and Improved b-Value of Acoustic Emissions Accompanying Rock Fracture,” Current Science, V. 89, No. 10, 2005, pp. 1577-1582.

30. Han, Q.; Yang, G.; Xu, J.; Fu, Z.; Lacidogna, G.; and Carpinteri, A., “Acoustic Emission Data Analyses Based on Crumb Rubber Concrete Beam Bending Tests,” Engineering Fracture Mechanics, V. 210, 2019, pp. 189-202. doi: 10.1016/j.engfracmech.2018.05.016

31. Li, D.; Cao, H.; and Ou, J. P., “Fracture Behavior and Damage Evaluation of Polyvinyl Alcohol Fiber Concrete Using Acoustic Emission Technique,” Materials & Design, V. 40, 2012, pp. 205-211. doi: 10.1016/j.matdes.2012.03.051

32. Di Benedetti, M., and Nanni, A., “Acoustic Emission Intensity Analysis for In Situ Evaluation of Reinforced Concrete Slabs,” Journal of Materials in Civil Engineering, ASCE, V. 26, No. 1, 2014, pp. 6-13. doi: 10.1061/(ASCE)MT.1943-5533.0000794

33. Fowler, T. J.; Blessing, J. A.; Conlisk, P. J.; and Swanson, T. L., “The MONPAC System,” Journal of Acoustic Emission, V. 8, No. 3, 1989, pp. 1-8.

34. Schreier, H.; Orteu, J. J.; and Sutton, M. A., Image Correlation for Shape, Motion and Deformation Measurements, Springer-Verlag US, 2009.

35. Kolanu, N. R.; Prakash, S. S.; and Ramji, M., “Experimental Study on Compressive Behavior of GFRP Stiffened Panels Using Digital Image Correlation,” Ocean Engineering, V. 114, 2016, pp. 290-302. doi: 10.1016/j.oceaneng.2016.01.034

36. Srikar, G.; Anand, G.; and Prakash, S. S., “A Study on Residual Compression Behavior of Structural Fiber Reinforced Concrete Exposed to Moderate Temperature Using Digital Image Correlation,” International Journal of Concrete Structures and Materials, V. 10, No. 1, 2016, pp. 75-85. doi: 10.1007/s40069-016-0127-x

37. Chen, X.; Wu, S.; and Zhou, J., “Large-Beam Tests on Mechanical Behavior of Dam Concrete under Dynamic Loading,” Journal of Materials in Civil Engineering, ASCE, V. 27, No. 10, 2015, p. 06015001. doi: 10.1061/(ASCE)MT.1943-5533.0001263


ALSO AVAILABLE IN:

Electronic Structural Journal