ACI 211.7R-20: Guide for Proportioning Concrete Mixtures with Ground Calcium Carbonate and Other Mineral Fillers

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ACI 211.7R-20: Guide for Proportioning Concrete Mixtures with Ground Calcium Carbonate and Other Mineral Fillers

Author(s): ACI Committee 211

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 16

Keywords: aggregate mineral filler; dust-of-fracture; ground calcium carbonate; ground lime

DOI:

Date: 11/10/2020

Abstract:
The use of ground calcium carbonate (GCC) and other mineral fillers can enhance the performance, economy, and sustainability of concrete mixtures. Modifications to the conventional proportioning method in ACI 211.1 are needed to incorporate these materials. This guide describes GCC and dust-of-fracture aggregate mineral fillers, including their properties, characterization, and qualification, and effects on concrete properties and sustainability. Recommendations are provided for proportioning concrete mixtures with these materials.