Nano-Modified Concrete as Repair Material in Cold Weather

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Nano-Modified Concrete as Repair Material in Cold Weather

Author(s): A. M. Yasien, M. T. Bassuoni, A. Abayou, and A. Ghazy

Publication: Materials Journal

Volume: 118

Issue: 2

Appears on pages(s): 149-160

Keywords: antifreeze admixture; cold weather; fly ash; nanosilica; repair

DOI: 10.14359/51729331

Date: 3/1/2021

Abstract:
With aging, concrete structures exhibit deterioration due to multiple reasons. Consequently, repair processes become overwhelmingly essential to extend the service life of structures. This experimental study investigated nano-modified concrete cast and cured under cyclic freezing/low temperatures, including its applicability to partial-depth repair. Seven mixtures, incorporating general-use cement, fly ash (0 to 25%), and nanosilica (0 to 4%) with a cold weather admixture system (antifreeze/accelerator) were tested. The mixtures were evaluated based on fresh, hardened, and durability properties as well as their compatibility with parent/substrate concrete. In addition, mercury intrusion porosimetry and thermogravimetric analysis were conducted to assess the evolution of microstructure under cold temperatures. The incorporation of 4% nanosilica in the cementitious binder, even with the presence of 15% fly ash, markedly enhanced the performance of concrete cast and cured under low temperatures without protection; thus, it may present a viable option for cold weather applications including repair.

Related References:

1. Karagöl, F.; Demirboga, R.; and Khushefati, W. H., “Behavior of Fresh and Hardened Concretes with Antifreeze Admixture in Deep-Freeze Low Temperatures and Exterior Winter Conditions,” Construction and Building Materials, V. 76, Feb. 2015, pp. 388-395. doi: 10.1016/j.conbuildmat.2014.12.011

2. Ratinov, V. B., and Rozenberg, T. I., “Antifreezing Admixtures,” Concrete Admixtures Handbook, second edition, William Andrew Publisher, New York, Dec. 1996, pp. 740-799.‏

3. Korhonen, C. L.; Cortez, E. R.; and Charest, B. A., “Strength Development of Concrete Cured at Low Temperature,” Concrete International, V. 14, No. 12, Jan. 1992, pp. 34-39.

4. Prado, P. J.; Balcom, B. J.; Beyea, T. W.; Bremner, T. W.; Armstrong, R. L.; and Grattan-Bellew, P. E., “Concrete Freeze/Thaw as Studied by Magnetic Resonance Imagine,” Cement and Concrete Research, V. 28, No. 2, 1998, pp. 261-270. doi: 10.1016/S0008-8846(97)00222-6

5. Powers, T. C., and Helmuth, R. A., “Theory of Volume Changes in Hardened Portland-Cement Paste during Freezing,” Proceedings of the Annual Meeting—Highway Research Board, V. 32, Jan, 1953, pp. 285-297.

6. ACI Committee 306, “Guide to Cold Weather Concreting (ACI 306R-16),” American Concrete Institute, Farmington Hills, MI, 2016, 24 pp.

7. CSA-A23.1/A23.2, “Concrete Materials and Methods of Concrete Construction/ Test Methods and Standard Practices for Concrete,” Canadian Standard Association (CSA), Mississauga, ON, Canada, 2019.

8. Barna, L. A.; Seman, P. M.; and Korhonen, C. J., “Energy-Efficient Approach to Cold-Weather Concreting,” Journal of Materials in Civil Engineering, ASCE, V. 23, No. 11, 2011, pp. 1544-1551. doi: 10.1061/(ASCE)MT.1943-5533.0000262

9. Korhonen, C.; Charest, B.; and Romisch, K., “Developing New Low-Temperature Admixtures for Concrete: A Field Evaluation,” Cold Regions Research and Engineering Lab, Hanover, NH, Mar. 1997.

10. Ghazy, A.; Bassuoni, M. T.; and Shalaby, A., “Nanomodified Fly Ash Concrete: A Repair Option for Concrete Pavements,” ACI Materials Journal, V. 113, No. 2, Mar.-Apr. 2016, pp. 231-242.

11. Madani, H.; Bagheri, A.; and Parhizkar, T., “The Pozzolanic Reactivity of Monodispersed Nanosilica Hydrosols and Their Influence on the Hydration Characteristics of Portland Cement,” Cement and Concrete Research, V. 42, No. 12, 2012, pp. 1563-1570. doi: 10.1016/j.cemconres.2012.09.004

12. Belkowitz, J. S.; Belkowitz, W. L. B.; Nawrocki, K.; and Fisher, F. T., “Impact of Nanosilica Size and Surface Area on Concrete Properties,” ACI Materials Journal, V. 112, No. 3, May-June 2015, pp. 419-428. doi: 10.14359/51687397

13. Hou, P.; Kawashima, S.; Kong, D.; Corr, D.; Qian, J.; and Shah, S., “Modification Effects of Colloidal NanoSiO2 on Cement Hydration and its Gel Property,” Composites. Part B, Engineering, V. 45, No. 1, 2013, pp. 440-448. doi: 10.1016/j.compositesb.2012.05.056

14. Abayou, A.; Yasien, A.; and Bassuoni, M., “Properties of Nanosilica-Modified Concrete Cast and Cured under Cyclic Freezing/Low Temperatures,” Advances in Civil Engineering Materials, V. 8, No. 3, 2019, pp. 287-306. doi: 10.1520/ACEM20190013

15. Yasien, A., and Bassuoni M., “Nano-Modified Concrete at Sub-Zero Temperatures: Experimental and Statistical Modelling,” Magazine of Concrete Research (published online Jan. 4, 2021).

16. CAN/CSA-A3001, “Cementitious Materials for Use in Concrete,” Canadian Standards Association, Mississauga, ON, Canada, 2013.

17. ASTM C494/C494M-19, “Standard Specification for Chemical Admixtures for Concrete,” ASTM International, West Conshohocken, PA, 2019.

18. ASTM C260/C260M-16, “Standard Specification for Air-Entraining Admixtures for Concrete,” ASTM International, West Conshohocken, PA, 2016.

19. Environment and Climate Change Canada, “Weather Dashboard for Winnipeg,” https://perma.cc/3QGB-6EV6. (last accessed Mar. 8, 2021).

20. ASTM C403/C403M-16, “Standard Test Method for Time of Setting of Concrete Mixtures by Penetration Resistance,” ASTM International, West Conshohocken, PA, 2016.

21. ASTM C39/C39M-20, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2020.

22. ASTM C496/C496M-17, “Standard Test Method for Splitting Tensile Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2017.

23. ASTM C469/C469M-14, “Standard Test Method for Static Modulus of Elasticity and Poisson’s Ratio of Concrete in Compression,” ASTM International, West Conshohocken, PA, 2014.

24. Tiznobaik, M., and Bassuoni, M. T., “A Test Protocol for Evaluating Absorption of Joints in Concrete Pavements,” Journal of Testing and Evaluation, V. 46, No. 4, 2018, pp. 1636-1649. doi: 10.1520/JTE20160297

25. ASTM C672/C672M-12, “Standard Test Method for Scaling Resistance of Concrete Surfaces Exposed to De-Icing Chemicals,” ASTM International, West Conshohocken, PA, 2012.

26. CW3310-R17, “Portland Cement Concrete Pavement Works,” City of Winnipeg Specification, Winnipeg, MB, Canada, Dec. 2015.

27. CSA A23.2-6B, “Determination of Bond Strength of Bonded Toppings and Overlays and of Direct Tensile Strength of Concrete, Mortar, and Grout,” CSA A23.1/A23.2, Canadian Standards Association, Mississauga, ON, Canada, 2019.

28. Nevile, A. M., Properties of Concrete, Prentice Hall, London, UK, 2011.

29. Wesche, K., Fly Ash in Concrete: Properties and Performance, CRC Press, Boca Raton, FL, 2014.

30. MacGregor, J. G.; Wight, J. K.; Teng, S.; and Irawan, P., Reinforced Concrete: Mechanics and Design, third edition, Prentice Hall, Upper Saddle River, NJ, 1997.

31. Kong, D.; Du, X.; Wei, S.; Zhang, H.; Yang, Y.; and Shah, S. P., “Influence of Nano-Silica Agglomeration on Microstructure and Properties of the Hardened Cement-Based Materials,” Construction and Building Materials, V. 37, Dec, 2012, pp. 707-715. doi: 10.1016/j.conbuildmat.2012.08.006

32. MTO LS-412, “Method of Test for Scaling Resistance of Concrete Surfaces Exposed to Deicing Chemicals,” Ontario Lab Testing Manual, Ministry of Transportation, Toronto, ON, Canada, 1997.

33. BNQ NQ 2621-900, “Determination of the Scaling Resistance of Concrete Surfaces Exposed to Freezing-and-Thawing Cycles in the Presence of De-icing Chemicals,” Bureau de Normalisation du Québec, Annexe A, 2002.

34. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” Farmington Hills, MI, 2019, 624 pp.

35. Slatnick, S.; Riding, K. A.; Folliard, K. J.; Juenger, M. C. G.; and Schindler, A. K., “Evaluation of Autogenous Deformation of Concrete at Early Ages,” ACI Materials Journal, V. 108, No. 1, Jan.-Feb. 2011, pp. 21-28.

36. Li, S.; Frantz, G. C.; and Stephens, J. E., “Bond Performance of Rapid-Setting Repair Materials Subjected to De-icing Salt and Freezing-Thawing Cycles,” ACI Materials Journal, V. 96, No. 6, Nov.-Dec. 1999, pp. 692-697.


ALSO AVAILABLE IN:

Electronic Materials Journal