Title: Cathodic Protection and Concrete Repairs at Sound of the Sea II Condominiums

Author(s): David G. Tepke, Clement A. Firlotte, and Stephen P. Robinson

Publication: Concrete International

Volume: 42

Issue: 11

Appears on pages(s): 18-23

Keywords: balconies, steel, corrosion, distress

DOI: 10.14359/51729297

Date: 11/1/2020

Abstract:
Constructed in 1984, Sound of the Sea II condominiums, Emerald Isle, NC, USA, underwent comprehensive repairs in 2007 and 2008. Repair and preservation technologies implemented on this project included impressed current cathodic protection (ICCP) on balconies and localized galvanic cathodic protection in corridors and roof parapet repairs. After 11 years in service, ICCP continues to provide protection within the original design parameters.

Related References:

1. “One Hundred Millivolt (mV) Cathodic Polarization Criterion,” NACE Publication 35108-2008-SG, NACE International, Houston, TX, 2008, 33 pp.