Influence of Incorporation and Dimension of Expanded Polystyrene on Lightweight Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Incorporation and Dimension of Expanded Polystyrene on Lightweight Concrete

Author(s): Guilherme S. Araujo, Lui C. Iwamoto, Rosa C. C. Lintz, and Luisa A. Gachet

Publication: Materials Journal

Volume: 118

Issue: 1

Appears on pages(s): 79-90

Keywords: expanded clay; expanded polystyrene; mechanical properties; self-compacting; structural lightweight concrete

DOI: 10.14359/51728280

Date: 1/1/2021

Abstract:
For the production of this lightweight concrete, expanded polystyrene (EPS) associated with expanded clay sintered lightweight aggregates were used to replace nature aggregates. Materials characterization tests were performed, as well as tests of the concrete in the fresh and hardened state. It is worth noting that the fresh tests displayed that the EPS concretes produced met the requirements of ABNT NBR 15823-1: 2017, classifying them as self-compacting. The hardened concrete tests observed the compressive strength, tensile strength, water absorption, void index, and specific mass. All concretes achieved resistances above 20 MPa, considered structural, and presented low specific mass, below 2000 kg/m3, classifying them as light concrete. Scanning electron microscopy (SEM) images allowed a better understanding of the microstructure, justifying the mechanical results obtained. The transition zone between the cement paste and the light aggregates, the number of voids in the cement paste, and the appearance of microcracks were considered.

Related References:

1. Rossignolo, J. A., Concreto Leve Estrutural: Produção, Propriedades, Microestrutura e Aplicações, Pini, São Paulo, Brasilia, 2009.

2. Li, J.; Niu, J.; Wan, C.; Liu, X.; and Jin, Z., “Comparison of Flexural Properties between High Performance Polypropylene Fiber Reinforced Lightweight Aggregate Concrete and Steel Fiber Reinforced Lightweight Aggregate Concrete,” Construction and Building Materials, V. 157, 2017, pp. 729-736. doi: 10.1016/j.conbuildmat.2017.09.149

3. Cruz, T. T., “Uso da Avaliação do Ciclo de Vida para a Determinação na Redução de Emissões de Gases do Efeito Estufa e do Consumo de Energia Associados a Reciclagem de EPS,” Faculdade de Engenharia de Guaratinguetá, Universidade Estadual Paulista, 2015.

4. Grote, Z. V., and Silveira, J. L., “Estudo Energético e Econômico Aplicado a um Processo de Reciclagem de Poliestireno Expandido (ISOPOR),” Congresso Brasileiro de Engenharia e Ciências Térmicas, 2002.

5. Tayal, A.; Gupta, G.; Choudhary, P.; Tomar, T.; Kumar, N.; and Mittal, S., “Lightweight Concrete Using Recycled Expanded Polystyrene Beads,” International Research Journal of Engineering and Technology, V. 5, 2018, pp. 91-93.

6. Catoia, T., “Concreto Ultraleve Estrutural com Pérolas de EPS: Caracterização do Material e Estudo de sua Aplicação em Lajes,” doctoral dissertation, Escola de Engenharia de São Carlos, Universidade de São Paulo, 2012.

7. Xu, Y.; Jiang, L.; Xu, J.; and Li, Y., “Mechanical Properties of Expanded Polysterene Lightweight Aggregate Concrete and Brick,” Construction and Building Materials, V. 27, No. 1, 2012, pp. 32-38. doi: 10.1016/j.conbuildmat.2011.08.030

8. Alcantara, M. A. M.; Kumayama R.; Cruz, W. S.; Segantini, A. A. S.; and Pinheiro, L. M., “Estudo das Propriedades Mecânicas do Concreto Autoadensável com o Emprego de pó de Mármore e Substituição Parcial dos Agregados por Pérolas de Poliestireno Expandido,” Congresso Brasileiro do Concreto, 2014.

9. Trussoni, M.; Hays, C. D.; and Zollo, R. F., “Fracture Properties of Concrete Containing Expanded Polystyrene Aggregate Replacement,” ACI Materials Journal, V. 110, No. 5, Sept.-Oct. 2013, pp. 549-557.

10. Monte, F. L.; Bamonte, P.; and Gambarova, P. G., “Physical and Mechanical Properties of Heat-Damage Structural Concrete Containing Expanded Polystyrene Synthesized Particles,” Fire and Materials, V. 39, No. 1, 2015, pp. 58-71. doi: 10.1002/fam.2230

11. Pereira, J. J.; Vanalli, L.; and Souza, R. A., “Aplicação de Resíduos de Poliestireno Expandido (EPS) para a Fabricação de Lajotas de Concreto Leve,” Congresso Brasileiro do Concreto, 2014.

12. Calheiros, C. S.; Almeida, M.; and Araújo, V. S., “Placas Cimentícias de Vedação com EPS: Dosagem, Produção e Controle Tecnológico,” Congresso Brasileiro do Concreto, 2015.

13. ABNT NBR 15270-1, “Componentes Cerâmicos – Blocos e Tijolos para Alvenaria – Parte 1,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brasilia, 2017.

14. Sartorti, A. L.; Pinheiro, L. M.; Da Silva, R. M.; and Cesar, T. G., “Adherence between Steel Bars and Lightweight Concrete with EPS Beads,” Revista IBRACON de Estruturas e Materiais, V. 10, No. 1, 2017, pp. 122-140. doi: 10.1590/s1983-41952017000100007

15. Fathi, M.; Yousefipour, A.; and Farokhy, E. H., “Mechanical and Physical Properties of Expanded Polystyrene Structural Concretes Containing Micro-Silica and Nano-Silica,” Construction & Building Materials, V. 136, 2017, pp. 590-597. doi: 10.1016/j.conbuildmat.2017.01.040

16. Chung, S.-Y.; Abd Elrahman, M.; and Stephan, D., “Effects of Expanded Polystyrene (EPS) Sizes and Arrangements on the Properties of Lightweight Concrete,” Materials and Structures, V. 51, No. 3, 2018, p. 57 doi: 10.1617/s11527-018-1182-3

17. Ozório, B. P. M., and Pinheiro, L. M., “Desempenho Térmico de Painéis Pré-Moldados de Concreto com Pérolas de EPS e de Argamassa Aerada,” Congresso Brasileiro do Concreto, 2014.

18. ABNT NBR 5738, “Concreto – Procedimento para Moldagem e Cura de Corpos-de-Prova,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brasilia, 2015.

19. Angelin, A. F., “Concreto Leve Estrutural – Desempenhos Físicos, Térmicos, Mecânico e Microestruturais,” master’s dissertation, Faculdade de Tecnologia, Universidade Estadual de Campinas, São Paulo, Brasilia, 2014.

20. Ozório, B. P. M., “Concreto Leve com Pérolas de EPS: Estudo de Dosagens e de Características Mecânicas,” doctoral thesis, Escola de Engenharia de São Carlos, Universidade de São Paulo, São Paulo, Brasilia, 2017.

21. Le Roy, R.; Parant, E.; and Boulay, C., “Taking into Account the Inclusions’ Size in Lightweight Concrete Compressive Strength Prediction,” Cement and Concrete Research, V. 35, No. 4, 2005, pp. 770-775. doi: 10.1016/j.cemconres.2004.06.002

22. ABNT NBR 15823-2, “Concreto Auto-Adensável. Determinação do Espalhamento e do Tempo de Escoamento - Método do Cone de Abrams,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brasilia, 2010.

23. ABNT NBR 15823-4, “Concreto Auto-Adensável. Determinação da Habilidade Passante - Método da Caixa L,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brasilia, 2010.

24. ABNT NBR 15823-5, “Concreto Auto-Adensável. Determinação da Viscosidade - Método do Funil V,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brasilia, 2010.

25. ABNT NBR 5739, “Concreto – Ensaio de Compressão de Corpos-de-Prova Cilíndricos,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brasilia, 2007.

26. ABNT NBR 7222, “Argamassa e Concreto – Determinação da Resistência à Tração por Compressão Diametral de Corpos-de-Prova,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brasilia, 2011.

27. Babu, K. G., and Babu, D. S., “Behaviour of Lightweight Expanded Polystyrene Concrete Containing Silica Fume,” Cement and Concrete Research, V. 33, No. 5, 2003, pp. 755-762. doi: 10.1016/S0008-8846(02)01055-4

28. ABNT NBR 9778, “Argamassa e Concreto Endurecidos - Determinação da Absorção de Água, Índice de Vazios e Massa Específica,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brasilia, 2009.

29. Madandoust, R.; Ranjbar, M. M.; and Yasin Mousavi, S., “An Investigation on the Fresh Properties of Self-Compacted Lightweight Concrete Containing Expanded Polystyrene,” Construction and Building Materials, V. 25, No. 9, 2011, pp. 3721-3731. doi: 10.1016/j.conbuildmat.2011.04.018

30. ABNT NBR 15823-1, “Concreto Auto-Adensável: Classificação, Controle e Aceitação no Estado Fresco,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brasilia, 2010.

31. Silva, F. M., “Concreto Leve Estrutural – Desempenhos Físicos, Térmicos, Mecânico e Microestruturais,” master’s dissertation, Faculdade de Tecnologia, Universidade Estadual de Campinas, São Paulo, Brasilia, 2014.

32. Liu, N., and Chen, B., “Experimental Study of the Influence of EPS Particle Size on the Mechanical Properties of EPS Lightweight Concrete,” Construction and Building Materials, V. 68, 2014, pp. 227-232. doi: 10.1016/j.conbuildmat.2014.06.062

33. ABNT NBR 6118, “Projeto de Estruturas De Concreto – Procedimento, Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brasilia, 2007.

34. ACI Committee 213, “Guide for Structural Lightweight-Aggregate Concrete (ACI 213R-03),” American Concrete Institute, Farmington Hills, MI, 2003.

35. Nili, M., and Ehsani, A., “Investigating the Effect of the Cement Paste and Transition Zone on Strength Development of Concrete Containing Nanosilica and Silica Fume,” Journal of Materials & Design, V. 75, 2015, pp. 174-183. doi: 10.1016/j.matdes.2015.03.024


ALSO AVAILABLE IN:

Electronic Materials Journal