Use of a Probabilistic Explicit Cracking Model for Analysing the mechanical behaviour of an Ultra-High Performance Fibre Reinforced Concrete (UHPFRC) Beam Subjected to Shear Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use of a Probabilistic Explicit Cracking Model for Analysing the mechanical behaviour of an Ultra-High Performance Fibre Reinforced Concrete (UHPFRC) Beam Subjected to Shear Loading

Author(s): Rossi, P.; Davian-Desnoyers, D.; Tailhan, J.L.

Publication: Symposium Paper

Volume: 343

Issue:

Appears on pages(s): 484-493

Keywords: Ultra-High Performance Fibre Reinforced Concrete; Numerical Model; Shear, Bending, Cracking

DOI:

Date: 10/1/2020

Abstract:
The objective of this paper is to verify the validity of the probabilistic explicit cracking model developed for SFRC to simulate the behaviour of a reinforced UHPFRC beam subjected to a bending load leading to shear failure. The relevancy of the model is evaluated through the simulation of the mechanical behaviour of the beam. The parameters characterizing the tensile behaviour of the studied UHPFRC are determined from the 3-point bending tests performed on beams sawed from the reinforced UHPFRC beam. The results suggest that the probabilistic explicit cracking model is relevant to analyze the mechanical behaviour of a reinforced UHPFRC beam and provide precise information about the cracking process of this type of material. The good agreement between the experimental result and the numerical simulations suggests that the studied UHPFRC behaves like usual FRC as the tensile strength and the mechanical effect of the fibres may be modelled by a perfectly brittle behaviour and a nonlinear softening behaviour.