Retrofitting a full-scale two-story hollow clay block masonry building by Steel Fiber Reinforced Mortar coating

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Retrofitting a full-scale two-story hollow clay block masonry building by Steel Fiber Reinforced Mortar coating

Author(s): Lucchini, S.S.; Facconi, L.; Minelli, F.; Plizzari, G.A.

Publication: Symposium Paper

Volume: 343

Issue:

Appears on pages(s): 462-472

Keywords: Steel Fiber Reinforced Mortar; Mortar coating; Retrofitting; Hollow block masonry; Cyclic test; Full-scale masonry test.

DOI:

Date: 10/1/2020

Abstract:
The use of mortar coating reinforced only with randomly diffused steel fibers represents an effective technique for seismic retrofitting of masonry buildings. The present work aims at proving the effectiveness of that technique by testing a full-scale two-story hollow clay block masonry building subjected to a quasi-static cyclic lateral loading. The experimental program includes two tests involving the same building. The first test performed on the building without coating is carried out to pre-damage masonry in order to simulate the effects of a seismic action significant for ultimate conditions. The second test is performed to assess the behavior of the pre-damaged building after retrofitting. The paper presents the main properties and details of both the test building and the proposed retrofitting technique. As the test on the retrofitted specimen is still ongoing, only the main results concerning the unstrengthened building are reported and discussed. To predict the response of the two experimental tests, 3D non-linear finite element simulations have been carried out and presented in the last section of the paper. The latter includes the comparison between the numerical prediction and the available experimental results.

Related References:

ASTM E519-02: 2002, Standard Test Method for Diagonal Tension (Shear) in Masonry Assemblages, ASTM International, West Conshohocken, PA.

Dehghani, A., Nateghi-Alahi, F., Fischer, G., “Engineered cementitious composites for strengthening masonry infilled reinforced concrete frames.” Engineering Structures, 105, 197-208, 2015.

Diana 10.1. Diana Finite Element Analysis – User’s Manual. TNO-Diana BV, Delft, The Netherlands, 2016

El Gawady, M., Lestuzzi, P., Badoux, M., “A review of conventional seismic retrofitting techniques for URM”. Proc., 4th Int. Conf. on Advanced Composite Materials in Bridges and Structures, Calgary, Alta, Canada, 2004

EN 1052-1:2001 – Methods of Test for Masonry. Determination of Compressive Strength.

EN 14651-5: 2005, Precast concrete products – test method for metallic fibre concrete – Measuring the flexural tensile strength, European Standard.

EN 1015-11:2007: Methods of test for mortar for masonry - Part 11: Determination of flexural and compressive strength of hardened mortar.

EN 772-1:2011 - Methods of tests for masonry units - Part 1: Determination of compressive strength.

EN 12390-13: 2013. Testing hardened concrete - Part 13: Determination of secant modulus of elasticity in compression. Eurocode (2006). Basis of Structural Design. EN 1990:2006.

Facconi, L., Conforti, A., Minelli, F., Plizzari, G., “Improving shear strength of unreinforced masonry walls by nano-reinforced fibrous mortar coating”. Materials and Structures 48

(2015): 2557–2574. doi: 10.1617/s11527-014-0337-0

Facconi, L., Minelli, F., & Giuriani, E., “Response of infilled RC frames retrofitted with a cementitious fiber-mesh reinforced coating in moderate seismicity areas.” Construction and Building Materials, 160, 574-587., 2018.

Facconi, L., Minelli, F., Lucchini, S., & Plizzari, G., “Experimental study of solid and hollow clay brick masonry walls retrofitted by steel fiber-reinforced mortar coating.” Journal of Earthquake Engineering, 24(3), 381-402, 2020.

Facconi, L., & Minelli, F., “Retrofitting RC infills by a glass fiber mesh reinforced overlay and steel dowels: experimental and numerical study.” Construction and Building Materials, 231, 117133, 2020.

Gattesco, N., Boem, I., Dudine, A., “Diagonal compression tests on masonry walls strengthened with a GFRP mesh reinforced mortar coating.” Bulletin of Earthquake Engineering, 13(6), 1703-1726, 2015.

Lin, Y.W., Lawley, D., Wotherspoon, L., Ingham, J.M., “Seismic retrofitting of an unreinforced masonry building using ECC shotcrete”. The New Zealand Concrete Industry Conference 2010, Wellington, New Zealand, 7-9 October, 2010

Papanicolaou, C.G., Triantafillou, T.C., Papathanasiou, M., Karlos, K., “Textile reinforced mortar (TRM) versus FRP as strengthening material of URM walls: out-of-plane cyclic

loading” Materials and Structures (2008) 41:143–157

Tomaževič, M., Klemenc, I., Weiss, P., “Seismic upgrading of old masonry buildings by seismic isolation and CFRP laminates: a shaking-table study of reduced scale models”. Bulletin of earthquake engineering, 7(1), 293-321, 2009.