An experimental study on the use of polypropylene macrofibers in precast segments for hydraulic and metro tunnel lining

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: An experimental study on the use of polypropylene macrofibers in precast segments for hydraulic and metro tunnel lining

Author(s): Conforti, A.; Trabucchi, I.; Tiberti, G.; Plizzari, G.A.; Caratelli, A; Meda, A.; Moro, S.; Hunger, M.

Publication: Symposium Paper

Volume: 343

Issue:

Appears on pages(s): 185-194

Keywords: Fiber reinforced concrete; Polypropylene macrofibers; Point load test; Precast tunnel segments; TBM thrust jack phase.

DOI:

Date: 10/1/2020

Abstract:
There is a growing interest in the scientific community on the structural applicability of polypropylene macrofibers without or in combination with conventional reinforcement as spread reinforcement for precast tunnel segmental linings. Polypropylene macrofibers could be used in precast tunnel segments as shear reinforcement and for withstanding splitting and spalling tensile stresses which occur under and between Tunnel Boring Machine (TBM) rams, respectively. Fibers could also simplify and speed up the tunnel element production process. In this context, the present study investigates the possibility of using polypropylene macrofiber reinforcement in precast tunnel segments for both hydraulic and metro tunnel linings. Four full-scale segments (two counter-key segments of a hydraulic tunnel and two trapezoidal shaped segments of a metro tunnel) were experimentally evaluated under point load test. The latter simulate the TBM actions on segments during the excavation process (TBM thrust jack phase), which is generally the most critical temporary loading condition for segments. Two reinforcement solutions were studied: a typical conventional reinforcement (reference samples) and a combination of polypropylene macrofibers and conventional reinforcement (hybrid solution). Polypropylene macrofibers were observed to be very effective in combination with conventional reinforcement, underlining the fibers ability in controlling both splitting and spalling phenomena.