Concrete Edge Failure of Anchor Groups Placed Parallel to an Edge

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Edge Failure of Anchor Groups Placed Parallel to an Edge

Author(s): Boglárka Bokor, Akanshu Sharma, and Jan Hofmann

Publication: Structural Journal

Volume: 118

Issue: 2

Appears on pages(s): 237-248

Keywords: anchor group; anchorage; concrete edge failure; experimental investigation; parallel arrangement; shear loading; test database

DOI: 10.14359/51728193

Date: 3/1/2021

Abstract:
The behavior of anchor groups arranged parallel to the concrete edge in one single anchor row and loaded in shear perpendicular to the concrete edge is experimentally investigated. A comprehensive test program was performed to obtain information on the group behavior, the influence of the displacement behavior of single anchors, influence of load eccentricity, and influence of crack pattern. A special configuration with unequal edge distance was also tested. The results showed that the anchorage behavior is highly dependent on the load-displacement behavior and on the stiffness conditions of the individual anchors within the group. It would be reasonable to consider the volume of activated concrete to consider different concrete geometries. The test results are aimed to generate a test database and are used to develop a new analytical model for the concrete edge failure mode of shear loaded anchor groups that will be presented in a future paper.

Related References:

ACI Committee 318, 2014, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary,” American Concrete Institute, Farmington Hills, MI, 520 pp.

Anderson, N. S., and Meinheit, D. F., 2006 “Design Criteria of Headed Stud Groups in Shear: Final Report,” Report No. WJE 1996.0002, Wiss, Janney, Elstner Associates, Inc., Northbrook, IL.

Bede, N.; Grosser, P.; and Ožbolt, J., 2017, “Shear Breakout Capacity of Various Fastening Systems in Concrete Elements,” Gradevinar, V. 69, pp. 1093-1100. doi: 10.14256/JCE.2168.2017

Bokor, B.; Sharma, A.; and Hofmann, J., 2017, “On the Limitations of the Current Design Provisions prEN 1992-4 for Design of Anchor Groups Subjected to Tension Loads,” Proceedings: Connections between Steel and Concrete, Sept. 27-29, Stuttgart, Germany.

Bokor, B.; Sharma, A.; and Hofmann, J., 2019, “Experimental and Numerical Investigations on the Concrete Edge Failure of Anchor Groups of Arbitrary Configurations,” Proceedings: 7th International Conference of Euro Asia Civil Engineering Forum, Sept. 30-Oct. 2, Stuttgart, Germany.

Bokor, B.; Sharma, A.; and Hofmann, J., 2020, “Experimental Investigations on the Concrete Edge Failure of Shear Loaded Anchor Groups of Rectangular and Non-Rectangular Configurations,” Engineering Structures, V. 222, No. 1, Nov., p. 111153 doi: 10.1016/j.engstruct.2020.111153

Cannon, R.W.; Burdette, E.G.; Funk, R.R., 1975, “Anchorage to Concrete,” Knoxville: Tennessee Valley Authority, Report No. CEB 75-32.

Cruz, R. D., 1987, “Effect of Edge Distance on Stud Groups Loaded in Shear and Torsion,” master’s thesis, School of Civil and Environmental Engineering, Oklahoma State University, Stillwater, OK.

Di Nunzio, G., and Muciaccia, G., 2019, “Safety Reduction in Anchor Groups Due to Uneven Crack Distribution,” IOP Conf. Series: Materials Science and Engineering 615, 7th International Conference on Euro Asia Civil Engineering Forum, Stuttgart, Germany.

Eligehausen, R., and Fuchs, W., 1988, “Load Bearing Behavior of Anchor Fastenings under Shear, Combined Tension and Shear or Flexural Loading,” Betonwerk und Fertigteiltecnik, V. 2, pp. 48-56.

Eligehausen, R., Mallée, R., Silva J.F., 2006, “Anchorage in Concrete Construction,” Berlin: Ernst & Sohn, 2006, ISBN-13: 978-3-433-01143-0

EN 1992-4, 2018, “Eurocode 2: Design of concrete structures - Part 4 Design of fastenings for use in concrete”, European Committee for Standardization, Brussels, Belgium.

ETA-17/0979, 2018, “ European Technical Assessment Fischer Injection System FIS EM Plus,” Deutsches Institut für Bautechnik.

fib Bulletin 58, 2011, “Design of Anchorages in Concrete: Part I-V,” International Federation for Structural Concrete, Lausanne, Switzerland.

Fuchs, W., 1990, “Tragverhalten von Befestigungen unter Querlast in ungerissenem Beton,” dissertation, University of Stuttgart, Stuttgart, Germany. (in German)

Fuchs, W.; Eligehausen, R.; and Breen, J. E., 1995, “Concrete Capacity Design (CCD) Approach for Fastening to Concrete,” ACI Structural Journal, V. 92, No. 1, Jan.-Feb., pp. 73-94.

Grosser, P., 2012, “Load-bearing Behavior and Design of Anchorages Subjected to Shear and Torsion Loading in Uncracked Concrete,”, PhD Thesis, University of Stuttgart, Stuttgart, Germany.

Hofmann, J., 2005, “Tragverhalten und Bemessung von Befestigungen unter beliebiger Querbelastung in ungerissenem Beton,” dissertation, University of Stuttgart, Stuttgart, Germany. (in German)

Klingner, R. E.; Mendonca, J. A.; and Malik, J. B., 1982, “Effect of Reinforcing Details on the Shear Resistance of Anchor Bolts under Reversed Cyclic Loading,” ACI Journal Proceedings, V. 79, No. 1, Jan.-Feb., pp. 3-11.

Kreismer, K., 1999, “Forschungsbericht über Versuche an randnahen Ankerbolzen im un-gerissenen Beton: Bericht II” (Shear Tests with Single Anchors close to the Edge in Uncracked Concrete), Stuttgart, Germany: Institute of Construction Materials, University of Stuttgart, 1999. Test Report, not published (in German).

Kummerow, A., 1996, “Tragverhalten von unter Querzug beanspruchten Verbundankern mit geringem Randabstand,” diploma thesis, University of Stuttgart, Stuttgart, Germany. (in German)

Mahrenholtz, C., and Sharma, A., 2017, “Testing of Anchors and Reinforcing Bars in Concrete under Cyclic Crack Movements,” Journal of Testing and Evaluation, V. 45, No. 4, pp. 1326-1337. doi: 10.1520/JTE20160082

Mahrenholtz, P., 2012, “Experimental Performance and Recommendations for Qualification of Post-installed Anchors for Seismic Applications,” PhD thesis, University of Stuttgart, Stuttgart, Germany.

Mallée, R., 2002, “Dübelgruppen am Bauteilrand unter Torsionsbeanspruchung,” Beton- und Stahlbetonbau, V. 97, No. 2, pp. 69-77. doi: (in German)10.1002/best.200200300

Schmid, K., 2010, “Tragverhalten und Bemessung von Befestigungen am Bauteilrand mit Rückhängebewehrung unter Querlasten rechtwenklig zum Rand,” dissertation, University of Stuttgart, Stuttgart, Germany. (in German)

Sharma, A., 2013, “Seismic Behavior and Retrofitting of RC Frame Structures with Emphasis on Beam-Column Joints – Experiments and Numerical Modeling,” PhD thesis, University of Stuttgart, Stuttgart, Germany.

Sharma, A.; Eligehausen, R.; and Asmus, J., 2017, “Experimental Investigation of Concrete Edge Failure of Multiple-Row Anchorages with Supplementary Reinforcement,” Structural Concrete, V. 18, No. 1, pp. 153-163. doi: 10.1002/suco.201600015

Stichting Bouwresearch, 1971 “Uit Beton Stekende Ankers,” Rapport A. Brüssel: Samson Uitg., Stichting Bouwresearch, 29. (in Dutch)

Swirsky, R. A.; Dusel, J. P.; Crozier, W. F.; Stoker, J. R.; and Nordlin, E. F., 1977, “Lateral Resistance of Anchor Bolts Installed in Concrete,” Report No. CA-DOT-TL-6680-1-77-07, Office of Transportation Laboratory, California Department of Transportation, Sacramento, CA.

Tian, K.; Ozbolt, J.; Sharma, A.; and Hofmann, J., 2018, “Experimental Study on Concrete Edge Failure of Single Headed Stud Anchors after Fire Exposure,” Fire Safety Journal, V. 96, pp. 176-188. doi: 10.1016/j.firesaf.2018.01.005

Tóth, M.; Bokor, B.; and Sharma, A., 2019, “Anchorage in Steel Fiber Reinforced Concrete – Concept, Experimental Evidence and Design Recommendations for Concrete Cone and Concrete Edge Breakout Failure Modes,” Engineering Structures, V. 181, pp. 60-75. doi: 10.1016/j.engstruct.2018.12.007

Unterweger, A., 2008, “Randnahe Anker unter Querlast: mechanische Modellierung und Bemessung,” dissertation, Austria Universität für Bodenkultur, Vienna, Austria. (in German)

Unterweger, A.; Spyridis, P.; Mihala, R.; and Bergmeister, K., 2008, “Shear Loaded Quadruple Fastenings Close to Edge—Experimental and Numerical Analysis,” Beton- und Stahlbetonbau, V. 1013, pp. 741-747. doi: 10.1002/best.200800644

Wong, T.L.; Donahey, R.C.; Lloyd, J.P., 1988, “Stud Groups Loaded in Shear Near a Free Edge,” Stillwater: Oklahoma State University, Draft Paper, to be submitted to PCI in 1998

Zhao, G.; Fuchs, W.; and Dieterle, H., 1988, “Einfluss der Bauteildicke auf das Tragverhalten von Dübelbefestigungen im ungerissenen Beton unter Querzugbeanspruchung,” Test Report No. 10/11-88/17, University of Stuttgart, Stuttgart, Germany. (in German)


ALSO AVAILABLE IN: