Shear Strength of Reinforced Concrete Wall with 700 MPa Shear Reinforcement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength of Reinforced Concrete Wall with 700 MPa Shear Reinforcement

Author(s): Sung-Hyun Kim and Hong-Gun Park

Publication: Structural Journal

Volume: 118

Issue: 2

Appears on pages(s): 167-181

Keywords: cyclic loading; Grade 700 MPa (101.5 ksi) bar; shear strength; shear wall

DOI: 10.14359/51728191

Date: 3/1/2021

Abstract:
In the present study, to investigate shear strength of concrete walls with 700 MPa (101.5 ksi) shear reinforcement, eight wall specimens were tested under cyclic lateral loading. The test parameters were failure modes, bar yield strength, aspect ratio, and axial load ratio. The test results showed that the shear strength of walls with 700 MPa (101.5 ksi) reinforcing bars was equivalent to or slightly less than those of walls with 400 MPa (58 ksi) reinforcing bars. In both walls, the tested shear strength was greater than the nominal strength of current design code. Further, regardless of the bar grade, the failure modes were similar, and shear reinforcement reached its yield strength. To investigate the effect of 700 MPa (101.5 ksi) reinforcing bars on the peak strength and deformation capacity of RC walls, parametric study was performed using an existing strain-based model.

Related References:

1. Horton, J. W.; Chapman, M. C.; and Green, R. A., “The 2011 Mineral, Virginia, Earthquake, And Its Significance for Seismic Hazards in Eastern North America—Overview And Synthesis,” Geological Society of America Special Papers, 509, 2015, pp. 1-25.

2. Mimura, N.; Yasuhara, K.; Kawagoe, S.; Yokoki, H.; and Kazama, S., “Damage from The Great East Japan Earthquake and Tsunami-A Quick Report,” Mitigation and Adaptation Strategies for Global Change, V. 16, No. 7, 2011, pp. 803-818. doi: 10.1007/s11027-011-9297-7

3. Eem, S. H.; Yang, B.; and Jeon, H., “Earthquake Damage Assessment of Buildings Using Opendata In the Pohang And The Gyeongju Earthquakes,” Journal of the Earthquake Engineering Society of Korea, V. 22, No. 3, 2018, pp. 121-128. doi: 10.5000/EESK.2018.22.3.121

4. Eem, S. H., and Choi, I. K., “Seismic Response Analysis of Nuclear Power Plant Structures and Equipment due to the Pohang Earthquake,” Journal of the Earthquake Engineering Society of Korea, V. 22, No. 3, 2018, pp. 113-119. doi: 10.5000/EESK.2018.22.3.113

5. ASCE, “Minimum Design Loads and Associated Criteria for Buildings and Other Structures,” ASCE/SEI 7-16, Reston, VA, 2016.

6. Chock, G. Y.; Ghosh, S. K.; O’Rourke, M.; and Stafford, T. E., “Significant Changes to the Minimum Design Load Provisions of ASCE 7-16,” American Society of Civil Engineers, Reston, VA, 2018.

7. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2019.

8. Sao, S.; Ogata, Y.; Yoshizaki, S.; Kanata, K.; Yamaguchi, T.; Nakayama, T.; Inada, Y.; and Kadoriku, J., “Behavior of Shear Wall Using Various Yield Strength of Reinforcing bar Part 1: An Experimental Study,” SMiRT-10, Anaheim, CA, Aug. 22-27, 1989.

9. Lefas, I. D.; Kotsovos, M. D.; and Ambraseys, N. N., “Behavior of Reinforced Concrete Structural Walls: Strength, Deformation Characteristics, and Failure Mechanism,” ACI Structural Journal, V. 87, No. 1, Jan.-Feb. 1990, pp. 23-31.

10. Park, H.-G.; Baek, J.-W.; Lee, J.-H.; and Shin, H.-M., “Cyclic Loading Tests for Shear Strength of Low-Rise Reinforced Concrete Walls with Grade 550 MPa Bars,” ACI Structural Journal, V. 112, No. 3, May-June 2015, pp. 299-310. doi: 10.14359/51687406

11. Baek, J.-W.; Park, H.-G.; Shin, H.-M.; and Yim, S.-J., “Cyclic Loading Tests for Reinforced Concrete Walls (Aspect Ratio 2.0) with Grade 550 MPa (80 ksi) Shear Reinforcing Bars,” ACI Structural Journal, V. 114, No. 3, May-June 2017, pp. 673-686. doi: 10.14359/51689437

12. Baek, J.-W.; Park, H.-G.; Lee, J.-H.; and Bang, C.-J., “Cyclic Loading Test for Walls of Aspect Ratio 1.0 and 0.5 with Grade 550 MPa Shear Reinforcing Bars,” ACI Structural Journal, V. 114, No. 4, July-Aug. 2017, pp. 969-982. doi: 10.14359/51689680

13. Chen, X. L.; Fu, J. P.; Hao, X.; Yang, H.; and Zhang, D. Y., “Seismic Behavior of Reinforced Concrete Squat Walls with High-Strength Reinforcements: An Experimental Study,” Structural Concrete, V. 20, No. 3, 2019, pp. 911-931. doi: 10.1002/suco.201800181

14. Kabeyasawa, T., and Hiraishi, H., “Tests And Analyses of High-Strength Reinforced Concrete Shear Walls in Japan,” High-Strength Concrete in Seismic Regions, SP-176, American Concrete Institute, Farmington Hills, MI, 1998, pp. 281-310.

15. Cheng, M.-Y.; Hung, S.-C.; Lequesne, R. D.; and Lepage, A., “Earthquake-Resistant Squat Walls Reinforced With High-Strength Steel,” ACI Structural Journal, V. 113, No. 5, Sept.-Oct. 2016, pp. 1065-1076. doi: 10.14359/51688825

16. Huq, M. S., “High-Strength Steel Bars in Earthquake-Resistant T-Shaped Concrete Walls,” University of Kansas, Lawrence, KS, 2018.

17. Korea Concrete Institute, “Concrete Design Code and Commentary,” Kimoondang Publishing Company, Seoul, Korea, 2017.

18. British Standards Institution, “ Eurocode 8:Design of Structures for Earthquake Resistance,” European Committee for Standardization, Bruxells, Belgium, 2003.

19. International Federation for Structural Concrete, (fib), fib Model Code for Concrete Structures 2010, John Wiley & Sons, Berlin, Germany, 2013.

20. Hawkins, N. M., and Ghosh, S., “Acceptance Criteria for Special Precast Concrete Structural Walls Based on Validation Testing,” PCI Journal, V. 49, No. 5, 2004, pp. 78-92. doi: 10.15554/pcij.09012004.78.92

21. Looi, D.; Su, R.; Cheng, B.; and Tsang, H., “Effects of Axial Load on Seismic Performance of Reinforced Concrete Walls with Short Shear Span,” Engineering Structures, V. 151, 2017, pp. 312-326. doi: 10.1016/j.engstruct.2017.08.030

22. Pilakoutas, K., and Elnashiai, A., “Cyclic Behavior of Reinforced Concrete Cantilever Walls, Part 1: Experimental Results,” ACI Structural Journal, V. 92, No. 3, May-June 1995, pp. 271-281.

23. Hidalgo, P. A.; Ledezma, C. A.; and Jordan, R. M., “Seismic Behavior of Squat Reinforced Concrete Shear Walls,” Earthquake Spectra, V. 18, No. 2, 2002, pp. 287-308. doi: 10.1193/1.1490353

24. Massone, L. M., and Wallace, J. W., “Load-deformation Response of Slender Reinforced Concrete Walls,” ACI Structural Journal, V. 101, No. 1, Jan.-Feb. 2004, pp. 103-113.

25. Orakcal, K.; Massone, L. M.; and Wallace, J. W., “Shear Strength Of Lightly Reinforced Wall Piers and Spandrels,” ACI Structural Journal, V. 106, No. 4, July-Aug. 2009, pp. 455-465.

26. Carrillo, J., and Alcocer, S. M., “Shear Strength of Reinforced Concrete Walls for Seismic Design of Low-Rise Housing,” ACI Structural Journal, V. 110, No. 3, May-June 2013, pp. 415-526.

27. Luna, B. N.; Rivera, J. P.; and Whittaker, A. S., “Seismic Behavior of Low-Aspect-Ratio Reinforced Concrete Shear Walls,” ACI Structural Journal, V. 112, No. 5, Sept.-Oct. 2015, pp. 593-603. doi: 10.14359/51687709

28. Gulec, C. K., and Whittaker, A. S., “Empirical Equations for Peak Shear Strength of Low Aspect Ratio Reinforced Concrete Walls,” ACI Structural Journal, V. 108, No. 1, Jan.-Feb. 2011, pp. 80-89.

29. Park, H.-G.; Yu, E.-J.; and Choi, K.-K., “Shear-Strength Degradation Model for RC Columns Subjected to Cyclic Loading,” Engineering Structures, V. 34, 2012, pp. 187-197. doi: 10.1016/j.engstruct.2011.08.041

30. Lee, J.-Y., and Watanabe, F., “Shear Deterioration Of Reinforced Concrete Beams Subjected to Reversed Cyclic Loading,” ACI Structural Journal, V. 100, No. 4, July-Aug. 2003, pp. 480-489.

31. Elwood, K. J., and Eberhard, M. O., “Effective Stiffness of Reinforced Concrete Columns,” ACI Structural Journal, V. 106, No. 4, July-Aug. 2009, pp. 476-484.


ALSO AVAILABLE IN:

Electronic Structural Journal