Proposed Flexural Stiffness of Slender Concrete Columns Reinforced with Glass Fiber-Reinforced Polymer Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Flexural Stiffness of Slender Concrete Columns Reinforced with Glass Fiber-Reinforced Polymer Bars

Author(s): Waseem Abdelazim, Hamdy M. Mohamed, and Brahim Benmokrane

Publication: Structural Journal

Volume: 118

Issue: 1

Appears on pages(s): 227-240

Keywords: design codes; flexural stiffness; glass fiber-reinforced polymer (GFRP) reinforcing bars; reinforced concrete; second-order analysis; slender columns; stability; statistical analysis

DOI: 10.14359/51728183

Date: 1/1/2021

Abstract:
The well-established moment magnification procedure in ACI 318 for the structural analysis of slender steel-reinforced concrete (steel-RC) columns was reexamined to accommodate concrete columns reinforced with glass fiber-reinforced polymer (GFRP) bars. This could encourage North American codes and guidelines (ACI 440.1R; CSA S806) to include detailed sections dealing with the design and analysis of RC columns entirely reinforced with GFRP bars. Consequently, a second-order analytical model was derived to assess the structural performance of more than 9500 slender GFRP-RC columns with a wide range of design parameters. The developed analytical model correlated well with the experimental data of 72 large-scale FRP-RC columns assembled from this study and the literature. The investigated parameters were the applied eccentricity ratio, slenderness ratio, longitudinal GFRP-reinforcement ratio, elastic modulus of GFRP bars, concrete compressive strength, column cross section geometry, and GFRP bar arrangement. Then, a multiple linear regression analysis of the simulated theoretical data was conducted to propose a simple and practical design equation for the effective flexural stiffness of slender GFRP-RC columns. Lastly, the stiffness reduction factor used to reduce the critical buckling load of a single isolated slender GFRP-RC column was recommended as 0.6 based on the performed one-percentile statistical analysis.

Related References:

Abdelazim, W.; Mohamed, H. M.; Afifi, M. Z.; and Benmokrane, B., 2020a, “Proposed Slenderness Limit for Glass Fiber-Reinforced Polymer-Reinforced Concrete Columns Based on Experiments and Buckling Analysis,” ACI Structural Journal, V. 117, No. 1, Jan. doi: 10.14359/51718073

Abdelazim, W.; Mohamed, H. M.; and Benmokrane, B., 2020b, “Inelastic Second-Order Analysis for ‎Slender GFRP-Reinforced Concrete Columns: Experimental Investigations and Theoretical Study‎,” Journal of Composites for Construction, ASCE, V. 24, No. 3, p. 04020016 doi: 10.1061/(ASCE)CC.1943-5614.0001019

Abdelazim, W.; Mohamed, H. M.; Benmokrane, B.; and Afifi, M. Z., 2020c, “Effect of Critical Test Parameters on Behavior of Glass Fiber-Reinforced Polymer-Reinforced Concrete Slender Columns under Eccentric Load,” ACI Structural Journal, ‎V. 117, No. 4, July.

ACI Committee 440, 2015, “Guide for the Design and Construction of Structural Concrete Reinforced with FRP-Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI.

ACI Committee 318, 2019, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 624 pp.

ASTM D2584, 2008, “Standard Test Method for Ignition Loss of Cured Reinforced Resins,” ASTM International, West Conshohocken, PA.

Chen, W. F., and Atsuta, T., 1976, Theory of Beam-Columns, Volume 1: In-Plane Behavior and Design, J. Ross Publishing.

CAN/CSA S806-12, 2012, “Design and Construction of Building Structures with Fibre-Reinforced Polymers,” Canadian Standards Association, Rexdale, ON, Canada.

CAN/CSA A23.3-14, 2014, “Design of Concrete Sructures,” Canadian Standards Association, Rexdale, ON, Canada.

Guérin, M.; Mohamed, H. M.; Benmokrane, B.; Shield, C. K.; and Nanni, A., 2018, “Effect of Glass Fiber-Reinforced Polymer Reinforcement Ratio on Axial-Flexural Strength of Reinforced Concrete Columns,” ACI Structural Journal, V. 115, No. 4, July, pp. 1049-1061. doi: 10.14359/51701279

Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2018, “Flexural Stiffness of GFRP- and CFRP-RC circular Members under Eccentric Loads Based on Experimental and Curvature Analysis,” ACI Structural Journal, V. 115, No. 4, July. doi: 10.14359/51702235

Hadhood, A.; Mohamed, H. M.; Benmokrane, B.; Nanni, A.; and Shield, C. K., 2019, “Assessment of Design Guidelines of Concrete Columns Reinforced with Glass Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 116, No. 4, July. doi: 10.14359/51715663

Hasan, H. A.; Karim, H.; Sheikh, M. N.; and Hadi, M. N. S., 2019, “Moment-Curvature Behavior of Glass Fiber-Reinforced Polymer Bar-Reinforced Normal-Strength Concrete and High-Strength Concrete Columns,” ACI Structural Journal, V. 116, No. 4, July. doi: 10.14359/51715573

Zadeh, H. J., and Nanni, A., 2017, “Flexural Stiffness and Second-Order Effects in Fiber-Reinforced Polymer-Reinforced Concrete Frames,” ACI Structural Journal, V. 114, No. 2, Mar.-Apr.

Khuntia, M., and Ghosh, S. K., 2004, “Flexural Stiffness of Reinforced Concrete Columns and Beams: Analytical Approach,” ACI Structural Journal, V. 101, No. 3, May-June.

MacGregor, J. G., 1976, “Safety and Limit States Design for Reinforced Concrete,” Canadian Journal of Civil Engineering, V. 3, No. 4, pp. 484-513. doi: 10.1139/l76-055

MacGregor, J. G.; Breen, J. E.; and Pfrang, E. O., Jan. 1970, “Design of Slender Concrete Columns,” ACI Journal Proceedings, V. 67, No. 1, Jan.

MacGregor, J. G.; Oelhafen, U. H.; and Hage, S. E., 1975, “A Re-Examination of the EI Value for Slender Columns,” Reinforced Concrete Columns, SP-50, American Concrete Institute, Farmington Hills, MI, pp. 1-40.

Martin, I.; MacGregor, J. G.; Pfrang, E. O.; and Breen, J. E., 1966, “A Critical Review of the Design of Reinforced Concrete Columns.” Symposium on Reinforced Concrete Columns, SP-13, American Concrete Institute, Farmington Hills, MI, pp. 13-53.

Mirmiran, A.; Yuan, W.; and Chen, X., Feb. 2001, “Design for Slenderness in Concrete Columns Internally Reinforced with Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 98, No. 1, Jan.-Feb.

Mirza, S. A., July-Aug. 1990, “Flexural Stiffness of Rectangular Reinforced Concrete Columns,” ACI Structural Journal, V. 87, No. 4, July-Aug.

Mirza, S. A., and MacGregor, J. G., 1982, “Probabilistic Study of Strength of Reinforced Concrete Members,” Canadian Journal of Civil Engineering, V. 9, No. 3, p. 1982 doi: 10.1139/l82-053

Popovics, S., 1973, “A Numerical Approach to the Complete Stress-Strain Curve of Concrete,” Cement and Concrete Research, V. 3, No. 5, Sept. 2001.

Thorenfeldt, E.; Tomaszewicz, A.; and Jensen, J. J., 1987, “Mechanical Properties of High Strength Concrete and Application to Design,” Proceedings of the Symposium on Utilization of High-Strength Concrete, Trondheim, Norway, pp. 149-159.

Tikka, T. K., and Mirza, S. A., 2005, “Nonlinear EI Equation for Slender Reinforced Concrete Columns,” ACI Structural Journal, V. 102, No. 6, Nov.-Dec.

Timoshenko, S. P., and Gere, J. M., 1963, Theory of Elastic Stability, second edition, McGraw-Hill, New York, 1963.

Xue, W.; Peng, F.; and Fang, Z., 2018, “Behavior and Design of Slender Rectangular Concrete Columns Longitudinally Reinforced with Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 115, No. 2, Mar., pp. 311-322. doi: 10.14359/51701131

Zadeh, H. J., and Nanni, A., 2013, “Design of RC Columns Using Glass FRP Reinforcement,” Journal of Composites for Construction, ASCE, V. 17, No. 3, pp. 294-304. doi: 10.1061/(ASCE)CC.1943-5614.0000354


ALSO AVAILABLE IN:

Electronic Structural Journal