Empirical Equations for Shear Strength of Conventional Reinforced Concrete Shear Walls

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Empirical Equations for Shear Strength of Conventional Reinforced Concrete Shear Walls

Author(s): Zeynep Tuna Deger and Cagri Basdogan

Publication: Structural Journal

Volume: 118

Issue: 2

Appears on pages(s): 61-71

Keywords: empirical equations; machine learning; reinforced concrete shear wall; shear strength; wall test database

DOI: 10.14359/51728177

Date: 3/1/2021

Abstract:
The majority of shear wall buildings constructed prior to the introduction of modern seismic codes includes inadequate reinforcement and detailing. To achieve an effective evaluation of such buildings, wall behavior should be well-understood and analytical models should be able to capture expected responses as accurately as possible. This study assesses a prominent shear wall characteristic, shear strength, for different dominant wall behaviors. Major seismic code equations and existing empirical expressions are assessed and alternative relations are proposed for conventional reinforced concrete shear walls. Wall shear strength equations provided by ACI 318 and JSC-2001 reveal the closest-to-accurate results for most wall types, although some discrepancies are observed for nonrectangular shear-controlled walls. The proposed empirical equations are derived using regression analyses with a machine learning approach and are valuable in that they are easy to use, interpretable, compatible with physical behavior, and are able to estimate shear strength reasonably close to accurate.

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

2. CSA A23.3-19, “Design of Concrete Structures,” CSA Group, Toronto, ON, Canada, 2019.

3. Disaster and Emergency Management Presidency, “Turkish Seismic Building Codes (TSC 2018),” TSC, Afet ve Acil Durum Yonetimi Baskanligi, Ankara, Turkey, 2018.

4. European Committee for Standardization, “Eurocode 8: Design of Structures for Earthquake Resistance—Part 3: Assessment and Retrofitting of Buildings (BS EN 1998-3),” CEN, Brussels, Belgium, 2005.

5. Japanese Seismic Code, “Japanese Standard for Seismic Evaluation of Existing Reinforced Concrete Buildings (JSC 2001),” Architectural Institute of Japan, Tokyo, Japan, 2001.

6. Wood, S. L., “Shear Strength of Low-Rise Reinforced Concrete Walls,” ACI Structural Journal, V. 87, No. 1, Jan.-Feb. 1990, pp. 99-107.

7. Wallace, J. W., “Behavior and Design of High-Strength RC Walls,” High-Strength Concrete in Seismic Region, SP-176, C. W. French and M. E. Kreger, eds., American Concrete Institute, Farmington Hills, MI, 1998, pp. 259-279.

8. Su, R. K. L., and Wong, S. M., “Seismic Behaviour of Slender Reinforced Concrete Shear Walls under High Axial Load Ratio,” Engineering Structures, V. 29, No. 8, 2007, pp. 1957-1965. doi: 10.1016/j.engstruct.2006.10.020

9. Orakcal, K.; Massone, L. M.; and Wallace, J. W., “Shear Strength of Lightly Reinforced Wall Piers and Spandrels,” ACI Structural Journal, V. 106, No. 4, July-Aug. 2009, pp. 455-465.

10. Alarcon, C.; Hube, M. A.; and de la Llera, J. C., “Effect of Axial Loads in the Seismic Behavior of Reinforced Concrete Walls with Unconfined Wall Boundaries,” Engineering Structures, V. 73, Aug. 2014, pp. 13-23. doi: 10.1016/j.engstruct.2014.04.047

11. Barda, F.; Hanson, J. M.; and Corley, W. G., “Shear Strength of Low-Rise Walls with Boundary Elements,” Reinforced Concrete Structures in Seismic Zones, SP-53, N. M. Hawkins and D. Mitchell, eds., American Concrete Institute, Farmington Hills, MI, 1977, pp. 149-202.

12. Oesterle, R. G.; Aristizabal-Ochoa, J. D.; Fiorato, A. E.; Russell, H. G.; and Corley, W. G., “Earthquake Resistant Structural Walls: Tests of Isolated Walls, Phase II,” Construction Technology Laboratories, A Division of Portland Cement Association, Skokie, IL, 1979.

13. Collins, M. P.; Mitchell, D.; Adebar, P.; and Vecchio, F. J., “A General Shear Design Method,” ACI Structural Journal, V. 93, No. 1, Jan.-Feb. 1996, pp. 36-45.

14. Hwang, S. J.; Fang, W. H.; Lee, H. J.; and Yu, H. W., “Analytical Model for Predicting Shear Strength of Squat Walls,” Journal of Structural Engineering, ASCE, V. 127, No. 1, 2001, pp. 43-50. doi: 10.1061/(ASCE)0733-9445(2001)127:1(43)

15. Gulec, C. K., and Whittaker, A. S., “Empirical Equations for Peak Shear Strength of Low Aspect Ratio Reinforced Concrete Walls,” ACI Structural Journal, V. 108, No. 1, Jan.-Feb. 2011, pp. 80-89.

16. Gupta, A., and Rangan, B. V., “High-Strength Concrete (HSC) Structural Walls,” ACI Structural Journal, V. 95, No. 2, Mar.-Apr. 1998, pp. 194-205.

17. Kassem, W., and Elsheikh, A., “Estimation of Shear Strength of Structural Shear Walls,” Journal of Structural Engineering, ASCE, V. 136, No. 10, 2010, pp. 1215-1224. doi: 10.1061/(ASCE)ST.1943-541X.0000218

18. Biskinis, D.; Roupakias, G.; and Fardis, M. N., “Degradation of Shear Strength of Reinforced Concrete Members with Inelastic Cyclic Displacements,” ACI Structural Journal, V. 101, No. 6, Nov.-Dec. 2004, pp. 773-783.

19. Grammatikou, S.; Biskinis, D.; and Fardis, M. N., “Strength, Deformation Capacity and Failure Modes of RC Walls under Cyclic Loading,” Bulletin of Earthquake Engineering, V. 13, No. 11, 2015, pp. 3277-3300. doi: 10.1007/s10518-015-9762-x

20. Massone, L. M., and Melo, F., “General Closed-Form Solution for Shear Strength Estimate of RC Elements Based on Panel Response,” Engineering Structures, V. 172, June 2018, pp. 239-252. doi: 10.1016/j.engstruct.2018.06.038

21. Ma, J.; Ning, C. L.; and Li, B., “Peak Shear Strength of Flanged Reinforced Concrete Squat Walls,” Journal of Structural Engineering, ASCE, V. 146, No. 4, 2020, p. 04020037 doi: 10.1061/(ASCE)ST.1943-541X.0002575

22. Jiang, Y.; Luo, J.; Liao, G.; Zhao, Y.; and Zhang, J., “An Efficient Method for Generation of Uniform Support Vector and Its Application in Structural Failure Function Fitting,” Structural Safety, V. 54, May 2015, pp. 1-9. doi: 10.1016/j.strusafe.2014.12.004

23. Mangalathu, S., and Jeon, J. S., “Classification of Failure Mode and Prediction of Shear Strength for Reinforced Concrete Beam-Column Joints Using Machine Learning Techniques,” Engineering Structures, V. 160, Apr. 2018, pp. 85-94. doi: 10.1016/j.engstruct.2018.01.008

24. Sengupta, P., and Li, B., “Hysteresis Behavior of Reinforced Concrete Walls,” Journal of Structural Engineering, ASCE, V. 140, No. 7, 2014, p. 04014030 doi: 10.1061/(ASCE)ST.1943-541X.0000927

25. Gulec, C. K.; Whittaker, A. S.; and Stojadinovic, B., “Shear Strength of Squat Rectangular Reinforced Concrete Walls,” ACI Structural Journal, V. 105, No. 4, July-Aug. 2008, pp. 488-497.

26. Farvashany, F. E.; Foster, S. J.; and Rangan, B. V., “Strength and Deformation of High-Strength Concrete Shear Walls,” ACI Structural Journal, V. 105, No. 1, Jan.-Feb. 2008, pp. 21-29.

27. Weng, P. W.; Li, Y. A.; Tu, Y. S.; and Hwang, S. J., “Prediction of the Lateral Load-Displacement Curves for Reinforced Concrete Squat Walls Failing in Shear,” Journal of Structural Engineering, ASCE, V. 143, No. 10, 2017, p. 04017141 doi: 10.1061/(ASCE)ST.1943-541X.0001872

28. Basdogan, C., “Investigation of Reinforced Concrete Wall Deformation Capacity (In Turkish),” master’s thesis, Istanbul Technical University, Istanbul, Turkey, 2017.

29. Deger, Z. T., and Basdogan, C., “Empirical Expressions for Deformation Capacity of Reinforced Concrete Structural Walls,” ACI Structural Journal, V. 116, No. 6, Nov. 2019, pp. 53-61. doi: 10.14359/51716806

30. Oh, Y. H.; Han, S. W.; and Choi, Y. S., “Evaluation and Improvement of Deformation Capacities of Shear Walls Using Displacement-Based Seismic Design,” International Journal of Concrete Structures and Materials, V. 18, 2006, pp. 55-61. doi: 10.4334/IJCSM.2006.18.1E.055

31. Paterson, J., and Mitchell, D., “Seismic Retrofit of Shear Walls with Headed Bars and Carbon Fiber Wrap,” Journal of Structural Engineering, ASCE, V. 129, No. 5, 2003, pp. 606-614. doi: 10.1061/(ASCE)0733-9445(2003)129:5(606)

32. Tokunaga, R., and Nakachi, T., “Experimental Study on Edge Confinement of Reinforced Concrete Core Walls,” Proceedings, Fifteenth World Conference on Earthquake Engineering (15WCEE), Lisboa, Portugal, 2012.

33. Belmouden, Y., and Lestuzzi, P., “Analytical Model for Predicting Nonlinear Reversed Cyclic Behaviour of Reinforced Concrete Structural Walls,” Engineering Structures, V. 29, No. 7, 2007, pp. 1263-1276. doi: 10.1016/j.engstruct.2006.08.014

34. Luna, B.; Rivera, J.; and Whittaker, A. S., “Seismic Behavior of Low-Aspect-Ratio Reinforced Concrete Shear Walls,” ACI Structural Journal, V. 112, No. 5, Sept.-Oct. 2015, pp. 593-604. doi: 10.14359/51687709

35. Lu, X.; Wang, L.; Wang, D.; and Jiang, H., “An Innovative Joint Connecting Beam for Precast Concrete Shear Wall Structures,” Structural Concrete, V. 17, No. 6, 2016, pp. 972-986. doi: 10.1002/suco.201500193

36. Cortes-Puentes, W. L., and Palermo, D., “Performance of pre-1970s Squat Reinforced Concrete Shear Walls,” Canadian Journal of Civil Engineering, V. 45, No. 11, 2018, pp. 922-959. doi: 10.1139/cjce-2017-0595

37. Jiang, H.; Wang, B.; and Lu, X., “Experimental Study on Damage Behavior of Reinforced Concrete Shear Walls Subjected to Cyclic Loads,” Journal of Earthquake Engineering, V. 17, No. 7, 2013, pp. 958-971. doi: 10.1080/13632469.2013.791895

38. Li, B.; Pan, Z.; and Xiang, W., “Experimental Evaluation of Seismic Performance of Squat RC Structural Walls with Limited Ductility Reinforcing Details,” Journal of Earthquake Engineering, V. 19, No. 2, 2015, pp. 313-331. doi: 10.1080/13632469.2014.962669

39. Villalobos, E.; Escolano-Margarit, D.; Ramirez-Marquez, A.; and Pujol, S., “Seismic Response of Reinforced Concrete Walls with Lap Splices,” Bulletin of Earthquake Engineering, V. 15, No. 5, 2017, pp. 2079-2100. doi: 10.1007/s10518-016-0051-0

40. Han, X.; Chen, B.; Cui, J.; Pan, Z.; Ji, J.; and Sun, D., “Experimental Study on Deformation Performance Indexes of RC Shear Walls,” Journal of Building Structures, V. 36, No. 6, 2018, pp. 1-9.

41. Massone, L. M.; Orakcal, K.; and Wallace, J. W., “Flexural and Shear Responses in Slender RC Walls,” Proceedings, Thirteenth World Conference on Earthquake Engineering (13WCEE), Vancouver, BC, Canada, 2004.

42. Salonikios, T. N.; Kappos, A. J.; Tegos, I. A.; and Penelis, G. G., “Cyclic Load Behavior of Low-Slenderness Reinforced Concrete Walls: Design Basis and Test Results,” ACI Structural Journal, V. 96, No. 4, July-Aug. 1999, pp. 649-660.

43. Sittipunt, C.; Wood, S. L.; Lukkunaprasit, P.; and Pattararattanakul, P., “Cyclic Behavior of Reinforced Concrete Structural Walls with Diagonal Web Reinforcement,” ACI Structural Journal, V. 98, No. 4, July-Aug. 2001, pp. 554-562.

44. Massone, L. M., “RC Wall Shear—Flexure Interaction: Analytical and Experimental Responses,” PhD dissertation, University of California, Los Angeles, Los Angeles, CA, 2006.

45. Tran, T. A., “Experimental and Analytical Studies of Moderate Aspect Ratio Reinforced Concrete Structural Walls,” PhD dissertation, University of California, Los Angeles, Los Angeles, CA, 2012.

46. Dazio, A.; Beyer, K.; and Bachmann, H., “Quasi-Static Cyclic Tests and Plastic Hinge Analysis of RC Structural Walls,” Engineering Structures, V. 31, No. 7, 2009, pp. 1556-1571. doi: 10.1016/j.engstruct.2009.02.018

47. ASCE/SEI 41-17, “Seismic Evaluation and Retrofit of Existing Buildings,” American Society of Civil Engineers, Reston, VA, 2017.

48. Tuna, Z., “Seismic Performance, Modeling, and Failure Assessment of Reinforced Concrete Shear Wall Buildings,” PhD dissertation, University of California, Los Angeles, Los Angeles, CA, 2012.

49. Mohamed, N.; Farghaly, A. S.; Benmokrane, B.; and Neale, K. W., “Experimental Investigation of Concrete Shear Walls Reinforced with Glass Fiber-Reinforced Bars under Lateral Cyclic Loading,” Journal of Composites for Construction, ASCE, V. 18, No. 3, 2014, p. A4014001. doi: 10.1061/(ASCE)CC.1943-5614.0000393

50. Aaleti, S.; Brueggen, B. L.; Johnson, B.; French, C. E.; and Sritharan, S., “Cyclic Response of Reinforced Concrete Walls with Different Anchorage Details: Experimental Investigation,” Journal of Structural Engineering, ASCE, V. 139, No. 7, 2013, pp. 1181-1191. doi: 10.1061/(ASCE)ST.1943-541X.0000732

51. Vapnik, V., The Nature of Statistical Learning Theory, Springer, New York, 1995.

52. Rasmussen, C. E., and Williams, C. K., Gaussian Process for Machine Learning, MIT Press, Cambridge, MA, 2006.


ALSO AVAILABLE IN:

Electronic Structural Journal