Numerical Simulation of Internal Relative Humidity of Concrete Exposed to Drying

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Numerical Simulation of Internal Relative Humidity of Concrete Exposed to Drying

Author(s): Sarah De Carufel, Andrew Fahim, Pouria Ghods, and Rouhollah Aalizadeh

Publication: Materials Journal

Volume: 117

Issue: 6

Appears on pages(s): 101-110

Keywords: ASTM F2170; concrete drying; concrete relative humidity; finite element modeling; moisture transport; permeability; pore size distribution; resilient flooring

DOI: 10.14359/51728146

Date: 11/1/2020

Abstract:
This paper presents a model developed to predict the internal relative humidity (RH) of concrete during drying. The model makes use of simplified inputs, including the concrete mixture design and the cement Bogue composition, thus making it accessible to engineers and practitioners. These inputs are used to separately determine the permeability of both liquid and vapor phases, hence solving for moisture transport through an empirical derivation of the (de) sorption isotherm, total porosity, and pore tortuosity. The model is validated using previously published literature data as well as experiments designed specifically for model validation. The model was found successful in predicting RH profiles for the validation data with the simple inputs required. However, it was found that in cases where the standardized ASTM F2170 method is used to measure RH, the agreement between the model and experimental data decreases. This was found to be related to errors associated with performing humidity measurements within cavities drilled in concrete. Such errors are discussed, and room for improvement in in-place humidity measurements is proposed. Finally, the model is used to validate the use of RH measurements at a specific concrete depth to evaluate the susceptibility of moisture-sensitive flooring to failures.

Related References:

1. Barrick, J., and Krokosky, E., “The Effects of Temperature and Relative Humidity on Static Strength of Hydrated Portland Cement,” Journal of Testing and Evaluation, V. 4, No. 1, 1976, pp. 61-73. doi: 10.1520/JTE10509J

2. Choi, S., and Won, M. C., “Thermal Strain and Drying Shrinkage of Concrete Structures in the Field,” ACI Materials Journal, V. 107, No. 5, Sept.-Oct. 2010, pp. 498-507.

3. Nielsen, E. P., and Geiker, M. R., “Chloride Diffusion in Partially Saturated Cementitious Material,” Cement and Concrete Research, V. 33, No. 1, 2003, pp. 133-138. doi: 10.1016/S0008-8846(02)00939-0

4. ACI Committee 302, “Guide for Concrete Slabs That Receive Moisture-Sensitive Flooring Materials (ACI 302.2R-06),” American Concrete Institute, Farmington Hills, MI, 2006, 42 pp..

5. ASTM F2170-19, “Standard Test Method for Determining Relative Humidity in Concrete Floor Slabs Using in situ Probes,” ASTM International, West Conshohocken, PA, 2019, 7 pp.

6. Bažant, Z. P., and Najjar, L. J., “Nonlinear Water Diffusion in Nonsaturated Concrete,” Materiales de Construcción, V. 5, No. 1, 1972, pp. 3-20.

7. Xi, Y.; Bažant, Z. P.; and Jennings, H. M., “Moisture Diffusion in Cementitious Materials Adsorption Isotherms,” Advanced Cement Based Materials, V. 1, No. 6, 1994, pp. 248-257. doi: 10.1016/1065-7355(94)90033-7

8. Xi, Y.; Bažant, Z. P.; Molina, L.; and Jennings, H. M., “Moisture Diffusion in Cementitious Materials Moisture Capacity and Diffusivity,” Advanced Cement Based Materials, V. 1, No. 6, 1994, pp. 258-266. doi: 10.1016/1065-7355(94)90034-5

9. Ishida, T.; Maekawa, K.; and Kishi, T., “Enhanced Modeling of Moisture Equilibrium and Transport in Cementitious Materials under Arbitrary Temperature and Relative Humidity History,” Cement and Concrete Research, V. 37, No. 4, 2007, pp. 565-578. doi: 10.1016/j.cemconres.2006.11.015

10. Zhang, Z.; Thiery, M.; and Baroghel-Bouny, V., “Numerical Modelling of Moisture Transfers with Hysteresis within Cementitious Materials: Verification and Investigation of the Effects of Repeated Wetting-Drying Boundary Conditions,” Cement and Concrete Research, V. 68, Feb. 2015, pp. 10-23. doi: 10.1016/j.cemconres.2014.10.012

11. Quenard, D., and Sallee, H., “Water Vapour Adsorption and Transfer in Cement-Based Materials: A Network Simulation,” Materials and Structures, V. 25, Nov, 1992, pp. 515-522. doi: 10.1007/BF02472447

12. Ye, G.; Lura, P.; and Breugel, K., “Modelling of Water Permeability in Cementitious Materials,” Materials and Structures, V. 39, No. 9, 2006, pp. 877-885. doi: 10.1617/s11527-006-9138-4

13. International Federation for Structural Concrete, (fib), “fib Model Code for Concrete 513 Structures,” Ernst & Sohn, Berlin, Germany, 2007.

14. Huang, Q.; Jiang, Z.; Gu, X.; Zhang, W.; and Guo, B., “Numerical Simulation of Moisture Transport in Concrete Based on a Pore Size Distribution Model,” Cement and Concrete Research, V. 67, 2015, pp. 31-43. doi: 10.1016/j.cemconres.2014.08.003

15. Fahim, A.; De Carufel, S.; Ghods, P.; Alizadeh, A. R.; and Salehi, M., “Practical Model for Predicting Internal Relative Humidity of Concrete Exposed to Drying,” Journal of Materials in Civil Engineering, ASCE, V. 31, No. 8, 2019, p. 04019143. doi: 10.1061/(ASCE)MT.1943-5533.0002785

16. Gong, F.; Zhang, D.; Sicat, E.; and Ueda, T., “Empirical Estimation of Pore Size Distribution in Cement, Mortar, and Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 26, No. 7, 2014, p. 04014023 doi: 10.1061/(ASCE)MT.1943-5533.0000945

17. Papadakis, V. G.; Vayenas, C. G.; and Fardis, M. N., “Physical and Chemical Characteristics Affecting the Durability of Concrete,” ACI Materials Journal, V. 8, No. 2, Mar.-Apr. 1991, pp. 186-196.

18. Dunlap, P., and Faris, S., “Surface Tension of Aqueous Solutions of Potassium Hydroxide,” Nature, V. 196, No. 4861, 1962, pp. 1312-1313. doi: 10.1038/1961312a0

19. Hagymassy, J. J. R. Jr.; Brunauer, S.; and Mikhail, R. S. H., “Pore Structure Analysis by Water Vapor Adsorption,” Journal of Colloid and Interface Science, V. 29, No. 3, 1969, pp. 485-491. doi: 10.1016/0021-9797(69)90132-5

20. Brunauer, S.; Emmett, P. H.; and Teller, E., “Adsorption of Gases in Multimolecular Layers,” Journal of the American Chemical Society, V. 60, No. 2, 1938, pp. 309-319. doi: 10.1021/ja01269a023

21. Valckenborg, R. M. E.; Pel, L.; Hazrati, K.; Kopinga, K.; and Marchand, J., “Pore Water Distribution in Mortar during Drying as Determined by NMR,” Materials and Structures, V. 34, No. 10, 2001, pp. 599-604. doi: 10.1007/BF02482126

22. Muller, A. C. A.; Scrivener, K. L.; Gajewicz, A. M.; and McDonald, P. J., “Use of Bench-Top NMR to Measure the Density, Composition and Desorption Isotherm of C-S-H in Cement Paste,” Microporous and Mesoporous Materials, V. 178, Sept, 2013, pp. 99-103. doi: 10.1016/j.micromeso.2013.01.032

23. Parrott, L. J.; Killoh, D. C.; and Patel, R. G., “Cement Hydration under Partially Saturated Conditions,” Proceedings, Eighth International Congress on the Chemistry of Cement, Abla Grafica e Editora, Rio De Janeiro, Brazil, V. 3, 1986, pp. 46-50.

24. Ho, D.; Cui, Q.; and Ritchie, D., “The Influence of Humidity and Curing Time on the Quality of Concrete,” Cement and Concrete Research, V. 19, No. 3, 1989, pp. 457-464. doi: 10.1016/0008-8846(89)90034-3

25. Sun, G.; Zhang, Y.; Sun, W.; Liu, Z.; and Wang, C., “Multi-Scale Prediction of the Effective Chloride Diffusion Coefficient of Concrete,” Construction and Building Materials, V. 31, No. 10, 2012, pp. 151-156.

26. Nakarai, K.; Ishida, T.; and Maekawa, K., “Multi-Scale Physicochemical Modeling of Soil-Cementitious Material Interaction,” Soil and Foundation, V. 46, No. 5, 2006, pp. 653-663. doi: 10.3208/sandf.46.653

27. Rangelov, M., and Nassiri, S., “Empirical Time-Dependent Tortuosity Relations for Hydrating Mortar Mixtures Based on Modified Archie’s Law,” Construction and Building Materials, V. 171, May, 2018, pp. 825-838. doi: 10.1016/j.conbuildmat.2018.03.173

28. Vinkler, M., and Vítek, J. L., “Drying Concrete: Experimental and Numerical Modeling,” Journal of Materials in Civil Engineering, ASCE, V. 28, No. 9, 2016, p. 04016070. doi: 10.1061/(ASCE)MT.1943-5533.0001577

29. Kim, J. K., and Lee, C. S., “Moisture Diffusion of Concrete Considering Self-Desiccation at Early Ages,” Cement and Concrete Research, V. 29, No. 12, 1999, pp. 1921-1927. doi: 10.1016/S0008-8846(99)00192-1

30. Hedenblad, G., “Drying on Construction Water in Concrete,” The Swedeish Council for Building Research, Stockholm, Sweden, 1997, p. 31.


ALSO AVAILABLE IN:

Electronic Materials Journal