Influence of Pore Structure Characteristics on the Mechanical and Durability Behavior of Pervious Concrete Material Based on Image Analysis

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Pore Structure Characteristics on the Mechanical and Durability Behavior of Pervious Concrete Material Based on Image Analysis

Author(s): Ruyan Liu, Yin Chi, Shengyun Chen, Qinghui Jiang, Xiaoyu Meng, Kun Wu, Shengjia Li

Publication: IJCSM

Volume: 14

Issue:

Appears on pages(s):

Keywords: pervious concrete, image analysis, pore structure, strength, permeability, durability, numerical simulation

DOI: 10.1186/s40069-020-00404-1

Date: 7/30/2020

Abstract:
Pervious concrete has been widely used in parking lots and other lightweight streets. Performances of pervious concrete are strongly dependent on its pore structure characteristics. This paper investigates the relationship among porosity, permeability, compressive strength, durability and the pore structure characteristics of pervious concrete. The infuences of basalt fber and fne aggregate on the pervious concrete are also discussed. Pervious concrete specimens with diferent pore structures were prepared by combining basalt aggregate with size of 5–10 mm and 10–15 mm at diferent proportion. The pore structure characteristics such as area porosity, pore sizes, and pore distribution of pervious concrete were obtained and analyzed using image analysis method. Experimental results showed that the pore structure characteristics of pervious concrete have efects on its mechanical and durability behaviors. Homogeneous pore distribution and large distances between pores increase the compressive strength and improve freeze–thaw durability of pervious concrete. Due to the diference in the internal pore structure of pervious concretes, specimens with similar volumetric porosities had diferent permeability coefcients. A series of numerical models were regenerated through a MATLAB code using pore structural parameters derived from the image analysis method, then the numerical models were fed to ANSYS for meshing and further simulation. The comparison of the simulation and experimental results showed close accuracy, which verifed the applied simulation analysis method based on image analysis technology.