Proposed Data Sheet for Alternative Cementitious Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Data Sheet for Alternative Cementitious Materials

Author(s): Terence C. Holland and Kenneth C. Hover

Publication: Concrete International

Volume: 42

Issue: 8

Appears on pages(s): 43-47

Keywords: cement, code, requirements, supplier

DOI: 10.14359/51728106

Date: 8/1/2020

Abstract:
Based on research data, new materials are being proposed for use as alternative cements or alternative supplementary cementitious materials. However, bringing new materials to market is difficult, time-consuming, and expensive. The product data sheet proposed in this article will guide potential suppliers through the testing and documentation that will be required to market alternative cementitious materials.

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 623 pp.

2. ACI Innovation Task Group 10, “Practitioner’s Guide for Alternative Cements (ACI ITG-10R-18),” American Concrete Institute, Farmington Hills, MI, 2018, 14 pp.

3. ASTM C1709-18, “Standard Guide for Evaluation of Alternative Supplementary Cementitious Materials (ASCM) for Use in Concrete,” ASTM International, West Conshohocken, PA, 2018, 4 pp.

4. Becker, R.J.; Holland, T.C.; and Malits, F.S., “Structural Concrete Using Alternative Cements,” Concrete International, V. 41, No. 6, June 2019, pp. 39-44.




  

Edit Module Settings to define Page Content Reviewer