Sustainability and Durability of Solidia Cement Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Sustainability and Durability of Solidia Cement Concrete

Author(s): Sada Sahu and Richard C. Meininger

Publication: Concrete International

Volume: 42

Issue: 8

Appears on pages(s): 29-34

Keywords: emission, test, mixture, clinker

DOI: 10.14359/51728105

Date: 8/1/2020

Abstract:
World cement production is estimated to contribute about 8% of total anthropogenic carbon dioxide (CO2) emissions worldwide. Solidia Cement™ (SC) is a new type of binder with a chemistry and functionality that allows it to have a significantly reduced CO2 footprint. The article describes the CO2 savings in the production of SC and CO2 used for curing of SC concrete.

Related References:

1. “Mineral Commodity Summaries 2020,” U.S. Geological Survey, 2020, p. 43, www.usgs.gov/centers/nmic/mineral-commodity-summaries.

2. Timperly, J., “Q&A: Why Cement Emissions Matter for Climate Change,” CarbonBrief, Sept. 13, 2018, www.carbonbrief.org/qa-why-cement-emissions-matter-for-climate-change.

3. “The Paris Agreement,” United Nations Framework Convention on Climate Change, www.unfccc.int/process-and-meetings/the-paris-agreement/the-paris-agreement. Accessed Apr. 22, 2020.

4. “Technology Roadmap: Low-Carbon Transition in the Cement Industry,” International Energy Agency, Paris, France, 2018, 61 pp., www.wbcsd.org/Sector-Projects/Cement-Sustainability-Initiative/Resources/Technology-Roadmap-Low-Carbon-Transition-in-the-Cement-Industry.

5. Barcelo, L.; Kline, J.; Walenta, G.; and Gartner, E.M., “Cement and Carbon Emissions,” Materials and Structures, V. 47, No. 6, June 2014, pp. 1055-1065.

6. DeCristofaro, N., and Sahu, S., “CO2 Reducing Cement,” World Cement, Jan. 2014, www.worldcement.com/the-americas/09012014/co2_reducing_cement_part_one_solidia_cement_chemistry_and_synthesis_571/.

7. Atakan, V.; Sahu, S.; Quinn, S.; Hu, X.; and DeCristofaro, N., “Why CO2 Matters—Advances in a New Class of Cement,” ZKG International, V. 67, No. 3, Jan. 2014, pp. 60-63.

8. DeCristofaro, N.; Meyer, V.; Sahu, S.; Bryant, J.; and Moro, F., “Environmental Impact of Carbonated Calcium Silicate Cement-Based Concrete,” Proceedings of the 1st International Conference on Construction Materials for Sustainable Future, A. Baricevic, ed., Zadar, Croatia, Apr. 19-21, 2017, pp. 65-70.

9. Sahu, S.; Quinn, S.; Atakan, V.; DeCristofaro, N.; and Walenta, G., “CO2-Reducing Cement Based on Calcium Silicate,” 14th International Congress on the Chemistry of Cement (ICCC), Beijing, China, Oct. 13-16, 2015.

10. Villani, C.; Spragg, R.; Tokpatayeva, R.; Olek, J.; and Weiss, W.J., “Characterizing the Pore Structure of Carbonated Natural Wollastonite,” Proceedings of the 4th International Conference on the Durability of Concrete Structures (ICDCS), West Lafayette, IN, July 24-26, 2014, pp. 262-269.

11. Diamond, S., “A Review of Alkali-Silica Reaction and Expansion Mechanisms 1. Alkalies in Cements and in Concrete Pore Solutions,” Cement and Concrete Research, V. 5, No. 4, July 1975, pp. 329-345.

12. Müllauer, W.; Beddoe, R.E.; and Heinz, D., “Sulfate Attack Expansion Mechanisms,” Cement and Concrete Research, V. 52, Oct. 2013, pp. 208-215.

13. Tian, B., and Cohen, M.D., “Does Gypsum Formation during Sulfate Attack on Concrete Lead to Expansion?,” Cement and Concrete Research, V. 30, No. 1, Jan. 2000, pp. 117-123.