High-Strength Steel Bars in Earthquake-Resistant Reinforced Concrete T-Shaped Walls

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: High-Strength Steel Bars in Earthquake-Resistant Reinforced Concrete T-Shaped Walls

Author(s): Mohammad Sajedul Huq, Erick A. Burgos, Rémy D. Lequesne, and Andrés Lepage

Publication: Structural Journal

Volume: 118

Issue: 1

Appears on pages(s): 215-226

Keywords: deformation capacity; fracture elongation; high-strength reinforcement; reversed cyclic load; slender walls; tensile-to-yield strength ratio; uniform elongation

DOI: 10.14359/51728091

Date: 1/1/2021

Abstract:
Six large-scale reinforced concrete T-shaped slender walls were tested under reversed cyclic loading to study the effects of reinforcing bar mechanical properties on wall deformation capacity. Effects on lateral stiffness and hysteretic energy dissipation were also quantified. Primary variables included reinforcement yield stress and the ratio of tensile-to-yield strength (ft/fy). An additional aim of the tests was to determine the minimum uniform elongation (strain at peak stress) and fracture elongation required of high-strength reinforcing bars for use in earthquake-resistant structures. The walls were not subjected to axial loads other than the weight of the loading apparatus and self-weight. The T-shaped walls, with a specified concrete compressive strength of 8 ksi (55 MPa), had a 100 in. (2540 mm) long stem joining a single 100 in. (2540 mm) long flange, both 10 in. (254 mm) thick. All walls had a nominal shear span of 300 in. (7620 mm). The control specimen T1 was constructed with conventional Grade 60 (420) reinforcement (where Grade corresponds to the specified yield stress of reinforcement). Walls T2, T3, T4, and T6 were constructed with Grade 100 (690) reinforcement and T5 with Grade 120 (830) reinforcement. Test results showed that regardless of the reinforcement grade, walls designed for similar flexural strength using longitudinal reinforcement with ft/fy between 1.18 and 1.39, uniform elongation not less than 6%, and fracture elongation not less than 10% had similar strengths and drift ratio capacities. The effective initial stiffness and hysteretic energy dissipation index for walls with high-strength reinforcement (T2 through T6) were approximately 70%, on average, of those for the wall with conventional reinforcement (T1).

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

2. Tavallali, H.; Lepage, A.; Rautenberg, J. M.; and Pujol, S., “Concrete Beams Reinforced with High-Strength Steel Subjected to Displacement Reversals,” ACI Structural Journal, V. 111, No. 5, Sept.-Oct. 2014, pp. 1037-1047. doi: 10.14359/51686967

3. Moehle, J. P., and To, D. V., “Performance Characterization of Beams with High-Strength Reinforcement,” RGA #04-14, Charles Pankow Foundation, Vancouver, WA, 2017.

4. Rautenberg, J. M.; Pujol, S.; Tavallali, H.; and Lepage, A., “Drift Capacity of Concrete Columns Reinforced with High-Strength Steel,” ACI Structural Journal, V. 110, No. 2, Mar.-Apr. 2013, pp. 307-317. doi: 10.14359/51684410

5. Sokoli, D., and Ghannoum, W. M., “High-Strength Reinforcement in Columns under High Shear Stresses,” ACI Structural Journal, V. 113, No. 3, May-June 2016, pp. 605-614. doi: 10.14359/51688203

6. FEMA 461, “Interim Testing Protocols for Determining the Seismic Performance Characteristics of Structural and Nonstructural Components,” Federal Emergency Management Agency, Washington, DC, 2007.

7. ASTM A370-17, “Standard Test Methods and Definitions for Mechanical Testing of Steel Products,” ASTM International, West Conshohocken, PA, 2017.

8. ASTM E8/E8M-16, “Standard Test Methods for Tension Testing of Metallic Materials,” ASTM International, West Conshohocken, PA, 2016.

9. Huq, M. S.; Weber‐Kamin, A.; Ameen, S.; Lequesne, R.; and Lepage, A., “High‐Strength Steel Bars in Earthquake‐Resistant T‐Shaped Concrete Walls,” SM Report No. 128, The University of Kansas Center for Research, Inc., Lawrence, KS, 2018.

10. Burgos, E. A.; Lequesne, R. D.; and Lepage, A., “Earthquake-Resistant T-Shaped Concrete Walls with High-Strength Steel Bars,” SM Report No. 142, The University of Kansas Center for Research, Inc., Lawrence, KS, 2020.

11. ATC 115, “Roadmap for the Use of High-Strength Reinforcement in Reinforced Concrete Design,” Applied Technology Council, Redwood City, CA, 2014.

12. ACI Committee 408, “Bond and Development of Straight Reinforcing Bars in Tension (ACI 408R-03),” American Concrete Institute, Farmington Hills, MI, 2003, 49 pp.

13. ASTM A706/A706M-16, “Standard Specification for Deformed and Plain Low-Alloy Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2016.

14. ASTM A615/A615M-16, “Standard Specification for Deformed and Plain Carbon-Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2016.

15. ASTM A1035/A1035M-16, “Standard Specification for Deformed and Plain, Low-Carbon, Chromium, Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2016.

16. ASTM C39/C39M-17, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2017.

17. ASTM C496/C496M-11, “Standard Test Method for Splitting Tensile Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2011.

18. ASCE/SEI 41-17, “Seismic Evaluation and Retrofit of Existing Buildings,” American Society of Civil Engineers, Reston, VA, 2017.

19. Otani, S., “Hysteresis Models of Reinforced Concrete for Earthquake Response Analysis,” Journal of the Faculty of Engineering, The University of Tokyo, V. 36, No. 2, 1981, pp. 125-159.

20. Moehle, J., Seismic Design of Reinforced Concrete Buildings, McGraw-Hill Education, 2015.

21. Fenwick, R., and Bull, D., “What is the Stiffness of Reinforced Concrete Walls?” SESOC Journal, V. 13, No. 2, 2000, pp. 23-32.

22. Sozen, M. A., and Moehle, J. P., “Stiffness of Reinforced Concrete Walls Resisting In-Plane Shear (EPRI TR-102731),” Tier 1 Electric Power Research Institute, Palo Alto, CA, 1993.

23. ATC 72, “Modeling and Acceptance Criteria for Seismic Design and Analysis of Tall Buildings,” Applied Technology Council, Redwood City, CA, 2010.


ALSO AVAILABLE IN:

Electronic Structural Journal