Cyclic Flexural Performance of Fire-Damaged Reinforced Concrete Beams Strengthened with Carbon Fiber-Reinforced Polymer Plates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cyclic Flexural Performance of Fire-Damaged Reinforced Concrete Beams Strengthened with Carbon Fiber-Reinforced Polymer Plates

Author(s): Akhrawat Lenwari, Chanachai Thongchom, and Riyad S. Aboutaha

Publication: Structural Journal

Volume: 117

Issue: 6

Appears on pages(s): 133-146

Keywords: carbon fiber-reinforced polymers; cyclic loading test; fire damage; flexural strengthening; nondestructive testing; reinforced concrete beams; sustained loading

DOI: 10.14359/51728064

Date: 11/1/2020

Abstract:
This paper presents the cyclic flexural performance of reinforced concrete (RC) beams after being exposed to a fire for 3 hours, air-cooled, and then strengthened with partial-length, adhesive-bonded carbon fiber-reinforced polymer (CFRP) plates. A total of 15 T-beams were tested under static four-point bending with periodic unloading and reloading at regular intervals until failure. Test variables included the level of exposure temperature (700 or 900°C [1292 or 1652°F]), sustained service loading (in addition to the beam self-weight) at the elevated temperature, and the CFRP plate length. The investigated flexural responses included the cyclic load-deflection relationship, CFRP strain-deflection relationship, and failure mode. No repair was conducted on beams exposed to 700°C (1292°F) before installation of the externally bonded CFRP plates. However, repair was necessary for beams exposed to 900°C (1652°F) due to excessive spalling of the concrete. For these beams, the concrete substrate was removed to a depth of 60 mm and replaced with the repair mortar before FRP strengthening. The externally bonded CFRP plates were found to reinstate the fire-damaged beams in terms of their flexural strength and stiffness at load levels beyond the cracking load of an undamaged beam. The level of strength enhancement was higher for the fire-damaged beams subjected to the simulated service loading than the counterpart beams exposed to fire with no load and the undamaged beams. Using mechanical end anchorages, the level of strength enhancement increased when the CFRP plate was extended closer to the supports. However, the addition of CFRP plates decreased the ductility of most strengthened beams. All CFRP-strengthened RC beams exhibited an intermediate crack-induced debonding failure. A comparison between the effective strain limits predicted with the ACI 440.2R-17 equation and the measured tensile strains in CFRP plates showed that the equation could be unconservative for the CFRP-strengthened RC beams under cyclic loading.

Related References:

1. Neves, I.; Rodrigues, J. P. C.; and Loureiro, A. D. P., “Mechanical Properties of Reinforcing and Prestressing Steels after Heating,” Journal of Materials in Civil Engineering, ASCE, V. 8, No. 4, 1996, pp. 189-194. doi: 10.1061/(ASCE)0899-1561(1996)8:4(189)

2. Naus, D. J., “The Effect of Elevated Temperature on Concrete Materials and Structures—A Literature Review,” Report No. ORNL/TM-2005/553, Oak Ridge National Laboratory, Oak Ridge, TN, 2005.

3. Chang, Y. F.; Chen, Y. H.; Sheu, M. S.; and Yao, G. C., “Residual Stress–Strain Relationship for Concrete after Exposure to High Temperatures,” Cement and Concrete Research, V. 36, No. 10, 2006, pp. 1999-2005. doi: 10.1016/j.cemconres.2006.05.029

4. Sharma, U. K.; Zaidi, K. A.; and Bhandari, N. M., “Residual Compressive Stress-Strain Relationship for Concrete Subjected to Elevated Temperatures,” Journal of Structural Fire Engineering, V. 3, No. 4, 2012, pp. 327-350. doi: 10.1260/2040-2317.3.4.327

5. Tao, Z.; Wang, X.; and Uy, B., “Stress-Strain Curves of Structural and Reinforcing Steels after Exposure to Elevated Temperatures,” Journal of Materials in Civil Engineering, ASCE, V. 25, No. 9, 2013, pp. 1306-1316. doi: 10.1061/(ASCE)MT.1943-5533.0000676

6. Haddad, R. H., and Shannis, L. G., “Post-Fire Behavior of Bond between High Strength Pozzolanic Concrete and Reinforcing Steel,” Construction and Building Materials, V. 18, No. 6, 2004, pp. 425-435. doi: 10.1016/j.conbuildmat.2004.03.006

7. Bingöl, A. F., and Gul, R., “Residual Bond Strength between Steel Bars and Concrete after Elevated Temperatures,” Fire Safety Journal, V. 44, No. 6, 2009, pp. 854-859. doi: 10.1016/j.firesaf.2009.04.001

8. El-Hawary, M. M.; Ragab, A. M.; El-Azim, A. A.; and Elibiari, S., “Effect of Fire on Flexural Behaviour of RC Beams,” Construction and Building Materials, V. 10, No. 2, 1996, pp. 147-150. doi: 10.1016/0950-0618(95)00041-0

9. Hansanti, S., “Behaviors of Reinforced Concrete Beams after Fire,” MEng thesis, Chulalongkorn University, Bangkok, Thailand, 2001. (in Thai)

10. Kumar, A., and Kumar, V., “Behaviour of RCC Beams after Exposure to Elevated Temperatures,” Journal of the Institution of Engineers (India), V. 84, No. 3, 2003, pp. 165-170.

11. Kodur, V. K. R.; Dwaikat, M. B.; and Fike, R. S., “An Approach for Evaluating the Residual Strength of Fire-Exposed RC Beams,” Magazine of Concrete Research, V. 62, No. 7, 2010, pp. 479-488. doi: 10.1680/macr.2010.62.7.479

12. Xu, Y. Y.; Wu, B.; Jiang, M.; and Huang, X., “Experimental Study on Residual Flexural Behavior of Reinforced Concrete Beams after Exposure to Fire,” Advanced Materials Research, V. 457-458, 2012, pp. 183-187. doi: 10.4028/www.scientific.net/AMR.457-458.183

13. Thongchom, C.; Jitsumroeng, S.; Lenwari, A.; and Aboutaha, R. S., “Experimental Study on Reinforced Concrete T-Beams at Elevated Temperatures,” The Fifteenth East Asia-Pacific Conference on Structural Engineering and Construction (EASEC15), Oct. 11-13, 2017, Xi’an, China, 2017, pp. 1406-1413.

14. Thongchom, C.; Lenwari, A.; and Aboutaha, R. S., “Effect of Sustained Service Loading on Post-Fire Flexural Response of Reinforced Concrete T-Beams,” ACI Structural Journal, V. 116, No. 3, May 2019, pp. 243-254. doi: 10.14359/51714477

15. Haddad, R. H.; Shannag, M. J.; and Moh’d, A., “Repair of Heat-Damaged RC Shallow Beams Using Advanced Composites,” Materials and Structures, V. 41, No. 2, 2008, pp. 287-299. doi: 10.1617/s11527-007-9238-9

16. Danie Roy, A. B.; Sharma, U. K.; and Bhargava, P., “Strengthening Heat Damaged Reinforced Concrete Beams Using Glass Fiber-Reinforced Polymer (GFRP) Laminates,” Applications of Structural Fire Engineering, Dubrovnik, Croatia, 2015.

17. Irshidat, M. R., and Al-Saleh, M. H., “Flexural Strength Recovery of Heat-Damaged RC Beams Using Carbon Nanotubes Modified CFRP,” Construction and Building Materials, V. 145, 2017, pp. 474-482. doi: 10.1016/j.conbuildmat.2017.04.047

18. Haddad, R. H., and Almomani, O. A., “Recovering Flexural Performance of Thermally Damaged Concrete Beams Using NSM CFRP Strips,” Construction and Building Materials, V. 154, 2017, pp. 632-643. doi: 10.1016/j.conbuildmat.2017.07.211

19. Thongchom, C.; Lenwari, A.; and Aboutaha, R. S., “Bond Properties between Carbon Fibre-Reinforced Polymer Plate and Fire-Damaged Concrete,” International Journal of Adhesion and Adhesives, V. 97, 2020, p. 102485 doi: 10.1016/j.ijadhadh.2019.102485

20. ACI Committee 440, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-17),” American Concrete Institute, Farmington Hills, MI, 2017, 112 pp.

21. Lenwari, A., and Thepchatri, T., “Experimental Study on RC Beams Strengthened with Carbon and Glass Fiber Sheets,” Engineering Journal, V. 13, No. 2, 2009, pp. 9-18. doi: 10.4186/ej.2009.13.2.9

22. ICC, “International Building Code,” International Code Council, Falls Church, VA, 2015.

23. ASTM A370-19, “Standard Test Methods and Definitions for Mechanical Testing of Steel Products,” ASTM International, West Conshohocken, PA, 2019, 50 pp.

24. ASTM D3039/D3039M-17, “Standard Test Method for Tensile Properties of Polymer Matrix Composite Materials,” ASTM International, West Conshohocken, PA, 2017, 13 pp.

25. SIKA, “Sikadur®-30. Thixotropic Epoxy Adhesive for Bonding Reinforcement,” Product Data Sheet, Version Jan. 2017.

26. ISO 834-1, “Fire Resistance Tests-Elements of Building Construction. Part 1: General Requirement,” International Standards Organization, Geneva, Switzerland, 1999.

27. ASTM E119-08a, “Standard Methods for Fire Tests of Building Construction and Materials,” ASTM International, West Conshohocken, PA, 2008, 31 pp.

28. BS 476-20, “Fire Tests on Building Materials and Structures – Part 20: Method for Determination of the Fire Resistance of Elements of Construction (General Principles),” British Standards Institute, London, UK, 1987.

29. ASTM C805/C805M-13, “Standard Test Method for Rebound Number of Hardened Concrete,” ASTM International, West Conshohocken, PA, 2013, 4 pp.

30. ASTM C1583/C1583M-13, “Standard Test Method for Tensile Strength of Concrete Surfaces and the Bond Strength or Tensile Strength of Concrete Repair and Overlay Materials by Direct Tension (Pull-off Method)”, ASTM International, West Conshohocken, PA, 2013, 4 pp.

31. SIKA, “Sika MonoTop®-614T. High Performance Repair Mortar,” Product Data Sheet, Version Feb. 2008.

32. fib Bulletin 14, “Externally Bonded FRP Reinforcement for RC Structures: Technical Report on the Design and Use of Externally Bonded Fibre Reinforced Polymer Reinforcement (FRP EBR) for Reinforced Concrete Structures,” International Federation for Structural Concrete (fib), Lausanne, Switzerland, 2001.

33. Teng, J. G.; Smith, S. T.; Yao, J.; and Chen, J. F., “Intermediate Crack–Induced Debonding in RC Beams and Slabs,” Construction and Building Materials, V. 17, No. 6-7, 2003, pp. 447-462. doi: 10.1016/S0950-0618(03)00043-6

34. Teng, J. G.; Lu, X. Z.; Ye, L. P.; and Jiang, J. J., “Recent Research on Intermediate Crack–Induced Debonding in FRP–Strengthened Beams,” Proceedings of the 4th International Conference on Advanced Composite Materials for Bridges and Structures, Calgary, AB, Canada, 2004.

35. Lee, J. H.; Chacko, R. M.; and Lopez, M. M., “Use of Mixed–Mode Fracture Interfaces for the Modeling of Large–Scale FRP–Strengthened Beams,” Journal of Composites for Construction, ASCE, V. 14, No. 6, 2010, pp. 845-855. doi: 10.1061/(ASCE)CC.1943-5614.0000143

36. Orton, S. L.; Jirsa, J. O.; and Bayrak, O., “Design Considerations of Carbon Fiber Anchors,” Journal of Composites for Construction, ASCE, V. 12, No. 6, 2008, pp. 608-616. doi: 10.1061/(ASCE)1090-0268(2008)12:6(608)


ALSO AVAILABLE IN:

Electronic Structural Journal