Abstract:
According to current regulations, a large number of existing structures show deficits in their shear capacity, which is often limited by the existing shear reinforcement. As the replacement of these structures is not always possible or favorable, effective strengthening methods and an accurate evaluation of their effectiveness are becoming more important.