Bond Strength Model of Strand in Corrosion-Induced Cracking Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Bond Strength Model of Strand in Corrosion-Induced Cracking Concrete

Author(s): Ju Yi, Lei Wang, and Royce W. Floyd

Publication: Structural Journal

Volume: 117

Issue: 6

Appears on pages(s): 119-132

Keywords: bond strength; confining stress; corrosion pressure; cracking concrete; strand

DOI: 10.14359/51728060

Date: 11/1/2020

Abstract:
This paper presents an analytical model to predict the evolution of strand bond strength with the propagation of concrete corrosion cracking, in which the transition of bond failure modes from pullout failure with strand rotation to concrete splitting failure is considered. For both failure modes, the ultimate bond strength is determined from the contributions of adhesion, corrosion pressure, and maximum confinement by considering the helical characteristics of seven-wire steel strand. The corrosion pressure in the uncracked, partly cracked, and completely cracked stages is estimated based on the relationship between radial displacement and pressure at the strand-concrete interface. For the contribution from maximum confinement, a critical confining stress is applied for the pullout failure type to consider the effect of strand rotation. The predicted results are shown to reasonably reproduce the variation tendency of strand bond strength and experimental results for specimens with and without stirrups. For the pullout failure type with strand rotation, introduction of the critical confining stress limits overestimation of contributions of confinement to the ultimate bond strength, especially for the corroded specimens with stirrups after complete cover cracking.

Related References:

1. Darmawan, M. S., and Stewart, M. G., “Spatial Time-Dependent Reliability Analysis of Corroding Pretensioned Prestressed Concrete Bridge Girders,” Structural Safety, V. 29, No. 1, 2007, pp. 16-31. doi: 10.1016/j.strusafe.2005.11.002

2. Naito, C. J.; Cetisli, F.; and Tate, T., “A Method for Quality Assurance of Seven-Wire Strand Bond in Portland Cement Concrete,” PCI Journal, V. 60, No. 4, 2015, pp. 69-84. doi: 10.15554/pcij.07012015.69.84

3. Wang, L.; Yi, J.; Zhang, J. R.; Jiang, Y. B.; and Zhang, X. H., “Effect of Corrosion-Induced Crack on the Bond Between Strand and Concrete,” Construction & Building Materials, V. 153, 2017, pp. 598-606. doi: 10.1016/j.conbuildmat.2017.07.113

4. Wang, L.; Zhang, X. H.; Zhang, J. R.; Yi, J.; and Liu, Y. M., “Simplified Model for Corrosion-Induced Bond Degradation between Steel Strand and Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 29, No. 4, 2017, p. 04016257 doi: 10.1061/(ASCE)MT.1943-5533.0001784

5. Li, F. M.; Qu, Y. X.; and Wang, J. H., “Bond Life Degradation of Steel Strand and Concrete under Combined Corrosion and Fatigue,” Engineering Failure Analysis, V. 80, 2017, pp. 186-196. doi: 10.1016/j.engfailanal.2017.06.036

6. Li, F. M., and Yuan, Y. S., “Effects of Corrosion on Bond Behavior between Steel Strand and Concrete,” Construction & Building Materials, V. 38, No. 2, 2013, pp. 413-422. doi: 10.1016/j.conbuildmat.2012.08.008

7. Murray, C. D.; Cranor, B. N.; Floyd, R. W.; and Pei, J. S., “Experimental Testing of Older AASHTO Type II Bridge Girders with Corrosion Damage at the Ends,” PCI Journal, V. 64, No. 1, 2019, pp. 49-64. doi: 10.15554/pcij64.1-02

8. Cairns, J., and Abdullah, R. B., “Bond Strength of Black and Epoxy-Coated Reinforcement—A Theoretical Approach,” ACI Materials Journal, V. 93, No. 4, July-Aug. 1996, pp. 362-369.

9. Laldji, S., and Young, A. G., “Bond between Steel Strand and Cement Grout in Ground Anchorages,” Magazine of Concrete Research, V. 40, No. 143, 1988, pp. 90-98. doi: 10.1680/macr.1988.40.143.90

10. Chao, S. H.; Naaman, A. E.; and Parra-Montesinos, G. J., “Bond Behavior of Strand Embedded in fiber Reinforced Cementitious Composites,” PCI Journal, V. 51, No. 6, 2006, pp. 56-71. doi: 10.15554/pcij.11012006.56.71

11. Aryanto, A., and Shinohara, Y., “Influence of Bond-Slip Relationship and Tensile Strength on Bond Behavior between Corroded Steel Bar and Concrete,” Journal of Structural and Construction Engineering, V. 78, No. 685, 2013, pp. 559-567. doi: 10.3130/aijs.78.559

12. Bhargava, K.; Ghosh, A. K.; Mori, Y.; and Ramanujam, S., “Models for Corrosion-Induced Bond Strength Degradation in Reinforced Concrete,” ACI Materials Journal, V. 104, No. 6, Nov.-Dec. 2007, pp. 594-603.

13. Chen, H., and Nepal, J., “Analytical Model for Residual Bond Strength of Corroded Reinforcement in Concrete Structures,” Journal of Engineering Mechanics, ASCE, V. 142, No. 2, 2016, p. 04015079 doi: 10.1061/(ASCE)EM.1943-7889.0000997

14. Coronelli, D., “Corrosion Cracking and Bond Strength Modeling for Corroded Bars in Reinforced Concrete,” ACI Structural Journal, V. 99, No. 3, May-June 2002, pp. 267-276.

15. Wang, X., and Liu, X., “Bond Strength Modeling for Corroded Reinforcements,” Construction and Building Materials, V. 20, No. 3, 2006, pp. 177-186. doi: 10.1016/j.conbuildmat.2005.01.015

16. Martí-Vargas, J. R.; García-Taengua, E.; and Serna, P., “Influence of Concrete Composition on Anchorage Bond Behavior of Prestressing Reinforcement,” Construction and Building Materials, V. 48, No. 19, 2013, pp. 1156-1164. doi: 10.1016/j.conbuildmat.2013.07.102

17. ASTM A416/A416M-10, “Standard Specification for Steel Strand, Uncoated Seven-Wire for Prestressed Concrete,” ASTM International, West Conshohocken, PA, 2010, 5 pp.

18. Wang, L.; Dai, L. Z.; Zhang, X. H.; and Zhang, J. R., “Concrete Cracking Prediction Including the Filling Proportion of Strand Corrosion Products,” Materials (Basel), V. 10, No. 6, 2016, pp. 1-20. doi: 10.3390/ma10010001

19. Vélez, W.; Matta, F.; and Ziehl, P., “Electrochemical Characterization of Early Corrosion in Prestressed Concrete Exposed to Salt Water,” Materials and Structures, V. 49, No. 1-2, 2016, pp. 507-520. doi: 10.1617/s11527-014-0514-1

20. Yu, L.; François, R.; Dang, V. H.; L’Hostis, V.; and Gagné, R., “Distribution of Corrosion and Pitting Factor of Steel in Corroded RC Beams,” Construction and Building Materials, V. 95, 2015, pp. 384-392. doi: 10.1016/j.conbuildmat.2015.07.119

21. den Uijl, J., and Bigaj, A., “A Bond Model for Ribbed Bars Based on Concrete Confinement,” HERON, V. 41, No. 3, 1996, pp. 201-226.

22. Moser, R. D.; Singh, P. M.; Kahn, L. F.; and Kurtis, K. E., “Chloride-Induced Corrosion of Prestressing Steels Considering Crevice Effects and Surface Imperfections,” Corrosion, V. 67, No. 6, 2011, p. 065001 doi: 10.5006/1.3595096

23. Pantazopoulou, S. J., and Papoulia, K. D., “Modeling Cover-Cracking Due to Reinforcement Corrosion in RC Structures,” Journal of Engineering Mechanics, ASCE, V. 127, No. 4, 2001, pp. 342-351. doi: 10.1061/(ASCE)0733-9399(2001)127:4(342)

24. Roelfstra, P. E., and Wittmann, F. H., “Numerical Method to Link Strain Softening with Failure of Concrete,” Fracture Toughness and Fracture Energy of Concrete, Elsevier Science Publishers, Amsterdam, the Netherlands, 1986, pp. 163-175.

25. Hillerborg, A., “Analysis of One Single Crack,” Fracture Mechanics on Concrete, Development in Civil Engineering, F. H. Wittmann, ed., Elsevier Science Publishers, Amsterdam, the Netherlands, 1983, pp. 223-249.

26. Giuriani, E.; Plizzari, G.; and Schumm, C., “Role of Stirrups and Residual Tensile Strength of Cracked Concrete on Bond,” Journal of Structural Engineering, ASCE, V. 117, No. 1, 1991, pp. 1-18. doi: 10.1061/(ASCE)0733-9445(1991)117:1(1)

27. ACI Committee 318, “Building Code Requirements for structural Concrete (ACI 318-14) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

28. Liu, Y., “Modeling the Time-to-Corrosion Cracking of the Cover Concrete in Chloride Contaminated Reinforced Concrete Structures,” ACI Materials Journal, V. 95, No. 6, Nov.-Dec. 1998, pp. 675-681.

29. Li, F. M., and Yuan, Y. S., “Effects of Corrosion on Bond Behavior between Steel Strand and Concrete,” Construction and Building Materials, V. 38, 2013, pp. 413-422. doi: 10.1016/j.conbuildmat.2012.08.008


ALSO AVAILABLE IN:

Electronic Structural Journal