Title: Incorporating Recycled and Crushed-Concrete Aggregates in Structural Concrete

Author(s): Kenneth C. Hover, Terence C. Holland, and Colin L. Lobo

Publication: Concrete International

Volume: 42

Issue: 7

Appears on pages(s): 26-31

Keywords: properties, durability, requirements, performance

DOI: 10.14359/51727002

Date: 7/1/2020

Abstract:
For economic and environmental reasons, it is increasingly desirable to augment the supply of natural aggregates for concrete production with recycled aggregates derived from crushed hardened concrete or from returned concrete. This article introduces new provisions in ACI 318-19 that set requirements for the use of recycled aggregates in concrete.

Related References:

1. ACI Committee 221, “Guide for Use of Normal Weight and Heavyweight Aggregates in Concrete (ACI 221R-96) (Reapproved 2001),” American Concrete Institute, Farmington Hills, MI, 1996, 29 pp.

2. ACI Committee E-701, “Aggregates for Concrete (ACI E1-16),” American Concrete Institute, Farmington Hills, MI, 2016, 26 pp.

3. Bezerra Cabral, A.E.; Schalch, V.; Coitinho Dal Molin, D.C.; and Duarte Ribeiro, J.L., “Mechanical Properties Modeling of Recycled Aggregate Concrete,” Construction and Building Materials, V. 24, No. 4, Apr. 2010, pp. 421-430.

4. ASTM C33/C33M-18, “Standard Specification for Concrete Aggregates,” ASTM International, West Conshohocken, PA, 2018, 8 pp.

5. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 623 pp.

6. “Concrete Terminology (ACI CT-18),” American Concrete Institute, Farmington Hills, MI, 2018, 76 pp.

7. ASTM C33/C33M-16, “Standard Specification for Concrete Aggregates,” ASTM International, West Conshohocken, PA, 2016, 11 pp.

8. “Sand and Sustainability: Finding New Solutions for Environmental Governance of Global Sand Resources,” United Nations Environment Programme (UNEP), Geneva, Switzerland, 2019, 35 pp.

9. “Sand, Rarer Than One Thinks,” UNEP Global Environmental Alert Service (GEAS), Geneva, Switzerland, Mar. 2014, 15 pp.

10. Peduzzi, P., “Sand, Rarer Than One Thinks,” Environmental Development, V. 11, 2014, pp. 208-218.

11. “Mineral Commodity Summaries 2020,” U.S. Geological Survey, 2020, 200 pp., https://doi.org/10.3133/mcs2020.

12. Dumiak, M., “Sand Shortage May Slow Growth in Developing Regions,” Engineering News-Record, July 24, 2019, www.enr.com/articles/47249-sand-shortage-may-slow-growth-in-developing-regions.

13. ACI Committee 555, “Removal and Reuse of Hardened Concrete (ACI 555R-01),” American Concrete Institute, Farmington Hills, MI, 2001, 26 pp.

14. Obla, K.; Kim, H.; and Lobo, C., “Crushed Returned Concrete as Aggregates for New Concrete,” RMC Research & Education Foundation, National Ready Mixed Concrete Association, Silver Spring, MD, 2007, 4 pp.

15. “Recycling Concrete Pavements,” EB043P, American Concrete Pavement Association (ACPA), Washington, DC, 2009, 84 pp.

16. “Technical Advisory T 5040.37 Use of Recycled Concrete Pavement as Aggregate in Hydraulic-Cement Concrete Pavement,” Federal Highway Administration, Washington, DC, www.fhwa.dot.gov/pavement/t504037.cfm. Accessed Feb. 28, 2020.

17. Snyder, M.B.; Cavalline, T.L.; Fick, G.; Taylor, P.; and Gross, J., “Recycling Concrete Pavement Materials: A Practitioner’s Reference Guide,” National Concrete Pavement Technology Center, Ames, IA, 2018, 88 pp.

18. ASTM C666/C666M-15, “Standard Test Method for Resistance of Concrete to Rapid Freezing and Thawing,” ASTM International, West Conshohocken, PA, 2015, 7 pp.

19. ASTM C672/C672M-12, “Standard Test Method for Scaling Resistance of Concrete Surfaces Exposed to Deicing Chemicals,” ASTM International, West Conshohocken, PA, 2012, 3 pp.